Mechanism of low-temperature reduction degradation of iron ore sinters

被引:0
|
作者
Loo, C.E.
Bristow, N.J.
机构
关键词
Crack propagation - Degradation - Deterioration - Fracture - Granular materials - Iron ore reduction - Low temperature operations - Magnetite - Minerals;
D O I
暂无
中图分类号
学科分类号
摘要
The degradation of ferrous materials under conditions of low-temperature reduction is a complex phenomenon. The onset of the process is linked to the gaseous reduction of hematite to a 'porous' form of magnetite, which results in a volume increase and the initiation of cracks. The subsequent propagation of the cracks and further reduction of hematite, which lead to the eventual breakdown of the sinter matrix, are less well understood. It is proposed that reduction degradation can be viewed as consisting of two distinct sub-processes. In the first easily accessible hematite grains are reduced, resulting in the initiation of cracks and their propagation into the surrounding sinter matrix as more of the grain is reduced. The second involves the further growth and branching of these cracks, the reduction of areas of newly exposed hematite grains along the walls of the cracks providing the energy requirements. In experimental work indentation methods were used to determine the vulnerability of sinter phases to crack propagation, and two cases are presented to demonstrate that decreases in the fracture toughness of mineral phases in the sinter result in severe deteriorations in sinter reduction degradation indices. It is considered that the proposed mechanism furthers understanding of the causes of reduction degradation, views on which are many and varied.
引用
收藏
相关论文
共 50 条
  • [31] FORMATION OF BINARY FERRITES IN IRON ORE SINTERS
    MAZANEK, E
    JASIENSK.S
    JOURNAL OF THE IRON AND STEEL INSTITUTE, 1966, 204 : 344 - &
  • [32] Low Temperature Reduction Degradation Characteristics of Sinter, Pellet and Lump Ore
    Wu Sheng-li
    Liu Xiao-qin
    Zhou Qi
    Xu Jian
    Liu Cheng-song
    JOURNAL OF IRON AND STEEL RESEARCH INTERNATIONAL, 2011, 18 (08) : 20 - 24
  • [33] Low temperature reduction degradation characteristics of sinter, pellet and lump ore
    Wu S.-L.
    Liu X.-Q.
    Zhou Q.
    Xu J.
    Liu C.-S.
    Journal of Iron and Steel Research International, 2011, 18 (8) : 20 - 24
  • [35] Fluidized magnetization roasting of refractory siderite-containing iron ore via preoxidation–low-temperature reduction
    Haoyan Sun
    Zheng Zou
    Meiju Zhang
    Dong Yan
    International Journal of Minerals,Metallurgy and Materials, 2023, (06) : 1057 - 1066
  • [36] Fluidized magnetization roasting of refractory siderite-containing iron ore via preoxidation–low-temperature reduction
    Haoyan Sun
    Zheng Zou
    Meiju Zhang
    Dong Yan
    International Journal of Minerals, Metallurgy and Materials, 2023, 30 : 1057 - 1066
  • [37] STRUCTURE AND STRENGTH OF IRON-ORE SINTERS
    EFIMENKO, GG
    SMIRNOV, SV
    KNYAZHANSKII, MM
    GABRINETS, EA
    IGNATOV, NV
    RUSSIAN METALLURGY, 1984, (01): : 1 - 5
  • [38] Non-isothermal reduction as a method of determining the softening-melting temperature of iron-ore pellets and sinters
    Mróz, J
    STEEL RESEARCH, 1998, 69 (12): : 465 - 468
  • [39] MECHANISM OF LOW-TEMPERATURE REDUCTION OF MANGANESE OXIDES WITH HYDROGEN
    PAVLOVAV.AI
    KHOMYAKO.KG
    RUSSIAN JOURNAL OF PHYSICAL CHEMISTRY,USSR, 1966, 40 (08): : 936 - &
  • [40] Experimental Study on Reduction Behavior of Iron Ore Fines at Low Temperature
    Li Qiu-ju
    Yu Xiao
    Wang Dao-jing
    Hong Xin
    JOURNAL OF IRON AND STEEL RESEARCH INTERNATIONAL, 2009, 16 : 1199 - 1203