In situ TEM study on hydrogen-induced cracking of nickel

被引:0
|
作者
Li, J.
Wang, Y.
Qiao, L.
Chu, W.
机构
来源
关键词
D O I
暂无
中图分类号
学科分类号
摘要
引用
收藏
页码:911 / 916
相关论文
共 50 条
  • [41] STUDY ON HYDROGEN-INDUCED CRACKING AND EMBRITTLEMENT OF HIGH STRENGTH STEEL.
    WEN-YUE, ZHANG
    AKIO, HIROSE
    1600,
  • [42] Hydrogen-induced intergranular cracking of pure nickel under various strain rates and temperatures in gaseous hydrogen environment
    Wada, K.
    Shibata, C.
    Enoki, H.
    Iijima, T.
    Yamabe, J.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2023, 873
  • [43] Acoustic Emission Monitoring of Wet H 2 S Cracking of Linepipe Steels: Application to Hydrogen-Induced Cracking and Stress-Oriented Hydrogen-Induced Cracking
    Smanio, V.
    Kittel, J.
    Fregonese, M.
    Cassagne, T.
    Normand, B.
    Ropital, F.
    CORROSION, 2011, 67 (06)
  • [44] Hydrogen-induced cracking by nanovoids in 310 stainless steel
    Department of Material Physics, Univ. of Sci. and Technology Beijing, Beijing 100083, China
    Sci China Ser E Technol Sci, 4 (x5-382):
  • [45] Hydrogen-induced cracking behaviors of Incoloy alloy 825
    Yang, Yong-jin
    Gao, Ke-wei
    Chen, Chang-feng
    INTERNATIONAL JOURNAL OF MINERALS METALLURGY AND MATERIALS, 2010, 17 (01) : 58 - 62
  • [46] Hydrogen-induced cracking behaviors of Incoloy alloy 825
    Yong-jin Yang
    Ke-wei Gao
    Chang-feng Chen
    International Journal of Minerals, Metallurgy, and Materials, 2010, 17 : 58 - 62
  • [47] Effects of microstructure on hydrogen-induced cracking in aluminum alloys
    Ben Ali, N.
    Tanguy, D.
    Estevez, R.
    SCRIPTA MATERIALIA, 2011, 65 (03) : 210 - 213
  • [48] DYNAMIC-MODEL OF HYDROGEN-INDUCED INTERGRANULAR CRACKING
    KAMEDA, J
    JOKL, ML
    SCRIPTA METALLURGICA, 1982, 16 (03): : 325 - 330
  • [49] Hydrogen-induced cracking by nanovoids in 310 stainless steel
    Huang, YZ
    Chen, QZ
    Wang, YB
    Chu, WY
    SCIENCE IN CHINA SERIES E-TECHNOLOGICAL SCIENCES, 1998, 41 (04): : 372 - 382
  • [50] Sour Environmental Severity for Hydrogen-Induced Cracking Susceptibility
    Fujishiro, Taishi
    Hara, Takuya
    Yasuda, Kyono
    Mizuno, Daisuke
    Ishikawa, Nobuyuki
    Tada, Eiji
    Kimura, Mitsuo
    CORROSION, 2022, 78 (02) : 189 - 197