Toroidal Milling of Hardened SAE H13 Steel

被引:0
|
作者
Diniz, A.E. [1 ]
Ferreira, J.R. [2 ]
Silveira, J.F. [2 ]
机构
[1] Dept. of Fabrication Engineering, State University of Campinas, Cd. Univ. Zeferino Vaz Barao Geraldo, Rua Mendeleiev, s/n, 13083-970 Campinas, SP, Brazil
[2] Department of Production, Mechanical Engineering Institute, Fed. University of Itajubá, Av. BPS 1303, 37500-902 Itajubá, MG, Brazil
关键词
Milling of dies and molds - Minimum quantity of lubricants;
D O I
10.1590/S1678-58782004000100003
中图分类号
学科分类号
摘要
引用
收藏
页码:17 / 21
相关论文
共 50 条
  • [31] Influences of TiAlN Coating on Cutting Temperature during Orthogonal Machining H13 Hardened Steel
    Hao, Guangchao
    Liu, Zhanqiang
    Liang, Xiaoliang
    Zhao, Jinfu
    COATINGS, 2019, 9 (06):
  • [32] Superplasticity of Annealed H13 Steel
    Duan, Zhenxin
    Pei, Wen
    Gong, Xuebo
    Chen, Hua
    MATERIALS, 2017, 10 (08):
  • [33] Boriding kinetics of H13 steel
    Genel, K
    VACUUM, 2006, 80 (05) : 451 - 457
  • [34] Optimization of cutting parameters for desirable surface roughness in end-milling hardened AISI H13 steel under a certain metal removal rate
    Ding, T. C.
    Zhang, S.
    Li, Z. M.
    Wang, Y. W.
    HIGH SPEED MACHINING, 2011, 188 : 307 - +
  • [35] Influence of minimum quantity lubrication on surface integrity of ground hardened H13 hot die steel
    Awale, A. S.
    Srivastava, A.
    Vashista, M.
    Yusufzai, M. Z. Khan
    INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2019, 100 (1-4): : 983 - 997
  • [36] On the machining characteristics of H13 tool steel in different hardness states in ball end milling
    J. J. Junz Wang
    M. Y. Zheng
    The International Journal of Advanced Manufacturing Technology, 2003, 22 : 855 - 863
  • [37] On the machining characteristics of H13 tool steel in different hardness states in ball end milling
    Wang, J.J.J. (jjwang@mail.ncku.edu.tw), 1600, Springer-Verlag London Ltd (22): : 11 - 12
  • [38] Influence of minimum quantity lubrication on surface integrity of ground hardened H13 hot die steel
    A. S. Awale
    A. Srivastava
    M. Vashista
    M. Z. Khan Yusufzai
    The International Journal of Advanced Manufacturing Technology, 2019, 100 : 983 - 997
  • [39] MICROSTRUCTURAL ALTERATION AND MICROHARDNESS AT NEAR-SURFACE OF AISI H13 STEEL BY HARD MILLING
    Zhang, S.
    Ding, T. C.
    Li, J. F.
    MACHINING SCIENCE AND TECHNOLOGY, 2012, 16 (03) : 473 - 486
  • [40] Wear and residual stress in high-feed milling of AISI H13 tool steel
    Bakirci, Altug
    Koca, Selim
    Erdogan, Ozlem
    Cakir, Mustafa Cemal
    MATERIALS TESTING, 2023, 65 (12) : 1845 - 1856