FRICTION REDUCTION AND DEGRADATION IN TURBULENT FLOW OF DILUTE POLYMER SOLUTIONS.

被引:0
|
作者
van der Meulen, J.H.J.
机构
来源
关键词
D O I
暂无
中图分类号
O3 [力学];
学科分类号
08 ; 0801 ;
摘要
An experimental study of friction reduction and polymer degradation in turbulent pipe flow is described for dilute water solutions of guar gum, CMC, Separan NP-10 and Polyox WSR-301. The tests are made in a turbulent-flow rheometer with a 2 mm I. D. pipe over a Reynolds number range from 8,000 to 25,000. The maximum attainable friction reduction for guar gum, Separan NP-10 and Polyox WSR-301 is found to be almost equal, but large differences in effectiveness occur. It was found that contrary to published data for guar gum, this material is not very stable.