共 50 条
- [1] Formation and characteristics of quasi-cleavage crack in hydrogen damaged low strength steel ECF 12: FRACTURE FROM DEFECTS, VOLS. I-III, 1998, : 1121 - 1126
- [4] Quantitative comparison of cleavage and quasi-cleavage fracture surfaces in hydrogen embrittled low-carbon steel LETTERS ON MATERIALS, 2020, 10 (03): : 303 - 308
- [5] Crack Initiation and Propagation Behavior of Hydrogen-induced Quasi-cleavage Fracture in X80 Pipeline Steel with Stress Concentration TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 2020, 106 (09): : 61 - 71
- [9] Quasi-cleavage fracture planes in spheroidized A533B steel JOURNAL OF MICROSCOPY-OXFORD, 2007, 227 (03): : 248 - 253
- [10] Origin of Serrated Markings on the Hydrogen Related Quasi-cleavage Fracture in Low-carbon Steel with Ferrite Microstructure Tetsu-To-Hagane/Journal of the Iron and Steel Institute of Japan, 110 (11): : 890 - 898