OPTICAL PROPERTIES OF IRIDIUM AT 77 AND 295 degree K.

被引:0
|
作者
Kirillova, M.M.
Nomerovannaya, L.V.
Noskov, M.M.
机构
来源
Physics of Metals and Metallography | 1972年 / 34卷 / 02期
关键词
D O I
暂无
中图分类号
学科分类号
摘要
The refractive and absorptive indices, n and k, of iridium were measured in the spectral range 15-0. 302 mu (0. 08-4. 08 eV) at 77 and 295 K. The optical properties in the infrared range are discussed in the model of two-band conductivity. It is established that the band transitions of electrons in iridium begin at greater than 0. 4 eV and cause appreciable spikes on the curve of light conductivity sigma ( omega ) at h omega similar 0. 44, 1. 0, 1. 6 and 2. 8 eV.
引用
收藏
页码:61 / 66
相关论文
共 50 条
  • [1] OPTICAL PROPERTIES OF IRIDIUM AT 77 AND 295 DEGREES K
    KIRILLOV.MM
    NOMEROVA.LV
    NOSKOV, MM
    PHYSICS OF METALS AND METALLOGRAPHY, 1973, 34 (02): : 61 - 66
  • [2] OPTICAL PROPERTIES OF IRIDIUM AT 77 DEGREES AND 295 DEGREES K
    KIRILLOV.MM
    NOSKOV, MM
    NOMEROVA.LV
    FIZIKA METALLOV I METALLOVEDENIE, 1972, 34 (02): : 291 - &
  • [3] FORMATION OF THE FINE STRUCTURE OF PURE IRON AND NICKEL IN THE PROCESS OF CREEP AT 295 AND 77 degree K.
    Demchuk, I.S.
    Krakhmalev, V.I.
    Metal Science and Heat Treatment (English translation of Metallovedenie i Termicheskaya Obrabotka Metallov), 1979, 21 (3-4): : 291 - 293
  • [4] CRYOTHERMOSTAT FOR OPTICAL USE IN THE RANGE 77-400 degree K.
    Askarov, P.A.
    Evstropov, V.V.
    Malkin, A.S.
    Shernyakov, Yu.M.
    Instruments and experimental techniques New York, 1981, 24 (5 pt 2): : 1329 - 1330
  • [5] EFFECT OF DEFORMATION AND ANNEALING ON THE PROPERTIES OF ELINVARS AT 77-650 degree K.
    Deryabin, A.V.
    Shvetsov, B.N.
    Chomova, N.G.
    Chirkov, Yu.A.
    Metal Science and Heat Treatment (English Translation of Metallovedenie i Termicheskaya Obrabotka, 1983, 25 (11-12): : 908 - 912
  • [6] SOME INVESTIGATIONS OF THE ACOUSTOELECTRIC INSTABILITY IN GaAs AT 77 degree K.
    Kurova, I.A.
    Ormont, N.N.
    Soviet Physics, Semiconductors (English translation of Fizika i Tekhnika Poluprovodnikov), 1974, 7 (10): : 1373 - 1374
  • [7] INVESTIGATION OF THE 300 degree K ANNEALING STAGE OF GERMANIUM IRRADIATED WITH FAST ELECTRONS AT 77 degree K.
    Gerasimov, A.B.
    Gogotishvili, M.K.
    Dolidze, N.D.
    Konovalenko, B.M.
    Magradze, M.V.
    1978, 12 (08): : 878 - 880
  • [8] Mechanical properties of zylon/epoxy composite at 295K and 77 K
    Walsh, Robert P.
    Swenson, Charles A.
    IEEE TRANSACTIONS ON APPLIED SUPERCONDUCTIVITY, 2006, 16 (02) : 1761 - 1764
  • [9] CREEP AND RUPTURE OF ALUMINIUM IN THE RANGE 77-273 degree K.
    Demikhovskaya, N.N.
    Kurov, I.Ye.
    Physics of Metals and Metallography, 1979, 47 (01): : 136 - 141
  • [10] MAXIMUM DRIFT VELOCITY OF ELECTRONS IN INDIUM ANTIMONIDE AT 77 degree K.
    Asauskas, R.
    Dobrovol'skis, Z.
    Krotkus, A.
    Soviet physics. Semiconductors, 1980, 14 (12): : 1377 - 1380