Experimental study on seismic behavior of steel reinforced concrete column-reinforced concrete beam joint after fire

被引:0
|
作者
Li J. [1 ,2 ]
Zhang X. [2 ]
Zhou C. [2 ]
Wu H. [2 ]
Che J. [1 ]
机构
[1] School of Civil Engineering, Quanzhou Institute of Information Engineering, Quanzhou
[2] College of Civil and Environment Engineering, Ningbo University, Ningbo
关键词
After fire; Column-beam joint; Low-cycle reversed loading test; Seismic behavior; Steel reinforced concrete;
D O I
10.14006/j.jzjgxb.2021.S2.0017
中图分类号
学科分类号
摘要
In order to study the seismic behavior of steel reinforced concrete (SRC) column-reinforced concrete (RC) beam joints after fire, four joints after fire and two comparative joints without exposure to fire were tested under low-cycle reversed loading. The hysteretic characteristics, ductility, energy dissipation performance, bearing capacity and stiffness degradation of this kind of joints after fire were studied, and the effects of fire duration and axial compression ratio on the seismic performance of this kind of joints after fire were analyzed. The test results show that after fire damage, the hysteretic curve of the SRC column-RC beam joint is still plump, but the bearing capacity decreases significantly. When subjected to fire for 75 min, the capacity decreases by 13.2%-15.8%, and when subjected to fire for 120 min, it decreases by 33.1%-34.9%. The ductility of joints after fire is affected by fire duration. When the fire duration is 75 min, the displacement ductility coefficient of the joint is 10.5%-10.7% lower than that of the joint without fire under the same conditions. When the fire duration is increased to 120 min, the ductility coefficient is 6.9%-7.4% higher than that of the joint at room temperature. Compared with the joints at room temperature, the stiffness of the joints at the initial stage of loading after fire decreases and the equivalent damping ratio increases. The longer the fire duration, the higher the degree of stiffness reduction and equivalent damping ratio increase. With the process of loading, the stiffness of the joints after fire is consistent with that of the original joints at room temperature, but the equivalent damping ratio decreases compared with the original joints at room temperature, the longer the fire duration, the higher the reduction degree. The axial compression ratio has a certain influence on the seismic performance of joints after fire. With the increase of axial compression ratio, the strength, initial stiffness and equivalent damping ratio of the specimen increase to a certain extent, but the ductility coefficient does not change significantly. equivalent damping ratio of the specimen are improved to a certain extent, but the ductility coefficient does not change significantly. © 2021, Editorial Office of Journal of Building Structures. All right reserved.
引用
收藏
页码:143 / 151
页数:8
相关论文
共 20 条
  • [11] WANG Guangyong, XIE Fudi, ZHANG Dongming, Test and parametric analysis on post-fire seismic performance of steel reinforced concrete columns, China Civil Engineering Journal, 48, 7, pp. 60-70, (2015)
  • [12] SHI Benlong, WANG Guangyong, MAO Xiaoyong, Experimental research on seismic performance of steel reinforced concrete column after exposure to fire, Journal of Building Structures, 38, 5, pp. 117-127, (2017)
  • [13] LI Junhua, CHEN Jianhua, SUN Bin, Experimental study on the seismic performance of steel reinforced concrete columns after exposure to fire, Journal of Building Structures, 36, 5, pp. 124-132, (2015)
  • [14] SONG T Y, HAN L H, TAO Z., Structural behavior of SRC beam-to-column joints subjected to simulated fire including cooling phase, Journal of Structural Engineering, 141, 9, (2015)
  • [15] LI Junhua, MA Chao, CHEN Jianhua, Et al., Experimental study on seismic behavior of steel reinforced concrete columns-steel beam joint after exposure to fire, Journal of Disaster Prevention and Mitigation Engineering, 35, 1, pp. 51-56, (2015)
  • [16] LI Junhua, ZHANG Zihua, CHI Yuyu, Experimental study on seismic behavior of steel reinforced concrete beam-column joints after exposure to fire, Engineering Mechanics, 34, 7, pp. 156-165, (2017)
  • [17] XIE Fudi, WU Zhixin, LIU Dongdong, Anti-seismic performance finite element analysis of steel reinforced concrete frame after fire, Journal of Beijing University of Civil Engineering and Architecture, 29, 3, pp. 35-39, (2013)
  • [18] WANG Guangyong, ZHANG Chao, LI Yumei, Et al., Post-fire seismic performance of steel reinforced concrete frame structures, Journal of Building Structures, 38, 12, pp. 78-87, (2017)
  • [19] LI Junhua, ZHANG Lei, GU Jufeng, Et al., Experimental study on seismic performance of SRC frame after exposure to fire, Journal of Building Structures, 41, 8, pp. 124-133, (2020)
  • [20] LI Junhua, LI Quanping, ZHANG Lei, Et al., Cyclic loading test on the performance of SRC column-RC beam frame after exposure to fire, Journal of Civil and Environmental Engineering, 43, 1, pp. 107-119, (2021)