- [21] Effects of thickness coating on the electrochemical behaviour of thermal spray Cr3C2-NiCr coatings SURFACE & COATINGS TECHNOLOGY, 2002, 153 (2-3): : 107 - 113
- [26] High temperature erosion of Cr3C2-NiCr thermal spray coatings - The role of phase microstructure SURFACE & COATINGS TECHNOLOGY, 2009, 203 (09): : 1144 - 1153
- [27] Oxidation behavior of FeAl-20WC composite coating obtained by HVOF thermal spray Dongbei Daxue Xuebao/Journal of Northeastern University, 2010, 31 (SUPPL. 1): : 293 - 296
- [29] Microstructural characterization and abrasive wear performance of HVOF sprayed Cr3C2-NiCr coating SURFACE & COATINGS TECHNOLOGY, 2006, 200 (24): : 6749 - 6757
- [30] The effects of post-treatment on the hot corrosion behavior of the HVOF-sprayed Cr3C2-NiCr coating SURFACE & COATINGS TECHNOLOGY, 2012, 206 (19-20): : 4212 - 4224