Joining of alumina to Tetragonal Zirconia Polycrystal (TZP) using a Bi2O3-Y2O3 filler

被引:0
|
作者
Nejabat, M. [1 ]
Hadian, A. M. [1 ]
Zamani, C. [1 ]
机构
[1] Univ Tehran, Coll Engn, Sch Met & Mat Engn, POB 11155-4563, Tehran, Iran
关键词
Joining; Wetting; ZrO2; STAINLESS-STEEL; TEMPERATURE; AL2O3; MICROSTRUCTURE; CERAMICS; AG; CU;
D O I
10.1016/j.ceramint.2024.07.391
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
In this study, joining of alumina to zirconia was conducted using a Bi2O3-Y2O3 filler under a normal atmosphere. In order to prevent the possible diffusion of yttrium from zirconia substrate into the interface, yttria was added to the filler. The wettability of 97Bi(2)O(3)-3Y(2)O(3) (wt%) filler was examined, and it was found that this filler has good wettability on alumina and zirconia. The bonded samples that were brazed at 975 degrees C for 10, 15, and 20 min were determined to be acceptable, while the samples that underwent various process temperatures showed defects such as voids, incomplete fusion, and cracks. Three new phases were observed formed at the interface using SEM images, and the content of these phases increased with increasing holding time. The effectiveness of adding yttria to the filler was confirmed by EDS analysis, as the yttrium of the zirconia substrate did not diffuse into the interface. The fracture surfaces were studied, and XRD analysis was taken from them. Brittle fracture has occurred in all samples, and BiAlO3, Y3Al5O12, and (Bi1.85Zr0.15) O-3.75 phases were identified at the interface. According to measurements of the shear strength of the joints, the sample brazed for 15 min at a temperature of 975 degrees C had the maximum strength of 31 MPa.
引用
收藏
页码:40880 / 40888
页数:9
相关论文
共 50 条
  • [31] RAPID OMNIDIRECTIONAL COMPACTION OF Y2O3 STABILIZED TETRAGONAL ZIRCONIA
    PECHENIK, A
    PYZIK, AJ
    BEAMAN, DR
    PROCESSING SCIENCE OF ADVANCED CERAMICS, 1989, 155 : 283 - 291
  • [32] Creep deformation in a 3mol%Y2O3-stabilized tetragonal zirconia
    Morita, K
    Hiraga, K
    Sakka, Y
    SUPERPLASTICITY-CURRENT STATUS AND FUTURE POTENTIAL, 2000, 601 : 93 - 98
  • [33] Low-temperature phase stability and mechanical properties of Y2O3- and Nb2O5-co-doped tetragonal zirconia polycrystal ceramics
    Lee, DY
    Kim, DJ
    Cho, DH
    JOURNAL OF MATERIALS SCIENCE LETTERS, 1998, 17 (03) : 185 - 187
  • [34] DETERMINATION OF ENTHALPIES OF MIXING THE SOLID-SOLUTIONS IN THE BI2O3-Y2O3 BY THE HIGH-TEMPERATURE SOLVING CALORIMETRY TECHNIQUE
    BEREZOVSKAYA, YM
    SEMENOV, YV
    VASILEVA, IA
    KHODAKOVSKII, IL
    ZHURNAL FIZICHESKOI KHIMII, 1989, 63 (05): : 1368 - 1370
  • [35] CONDUCTION IN BI2O3-BASED OXIDE ION CONDUCTORS UNDER LOW OXYGEN-PRESSURE .1. CURRENT BLACKENING OF BI2O3-Y2O3 ELECTROLYTE
    TAKAHASHI, T
    ESAKA, T
    IWAHARA, H
    JOURNAL OF APPLIED ELECTROCHEMISTRY, 1977, 7 (04) : 299 - 302
  • [36] INTERNAL FRICTION, DIELECTRIC LOSS, AND IONIC CONDUCTIVITY OF TETRAGONAL ZrO2-3% Y2O3 (Y-TZP).
    Weller, M.
    Schubert, H.
    1600, (69):
  • [37] FATIGUE BEHAVIOR OF 2-MOL-PERCENT AND 4-MOL-PERCENT Y2O3-CONTAINING TETRAGONAL ZIRCONIA POLYCRYSTALS (Y-TZP)
    ASHIZUKA, M
    KIYOHARA, H
    GONDO, M
    KUBOTA, Y
    YOGYO-KYOKAI-SHI, 1987, 95 (04): : 387 - 393
  • [39] FATIGUE BEHAVIOR OF HIPED Y2O3 CONTAINING TETRAGONAL ZIRCONIA POLYCRYSTALS
    ASHIZUKA, M
    SASAKI, T
    FURUKAWA, M
    JOURNAL OF THE JAPAN INSTITUTE OF METALS, 1988, 52 (06) : 616 - 621
  • [40] Joining ZTA ceramic by using Dy2O3-Al2O3-SiO2 glass ceramic filler
    Guo, Chaohui
    Zhu, Weiwei
    Shen, Yuanxun
    Sui, Qi
    Liu, Yaodong
    Ran, Xu
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2020, 40 (15) : 5819 - 5828