Magnetic properties of TbCu7-type Sm-Fe-Co-Cr-Y system nitrided compounds

被引:0
|
作者
School of Science and Technology, Meiji University, 1-1-1 Higashimita, Tama-ku, Kawasaki 214-8571, Japan [1 ]
机构
来源
Funtai Oyobi Fummatsu Yakin | 2006年 / 7卷 / 590-596期
关键词
Density (specific gravity) - Heat treatment - Magnetic properties - Nitriding - Powders - X ray diffraction;
D O I
10.2497/jjspm.53.590
中图分类号
学科分类号
摘要
Experiments were carried out to investigate the effects of composition, heat-treatment and nitrogenation conditions on the magnetic properties of Sm-Fe-Co-Cr-Y-N compounds with the TbCu7-type structure. The optimum preparation conditions of the compounds were as follows: composition: {Sm 10(Fe0.9Co0.1)89.4Cr 0.3Y0.3}86.6N13.4 roller velocity: 50 m/s, heat treatment: 680°C for 60 min in high-purity Ar gas, and nitrogenation condition: 420°C for 10 h in highpurity N2 gas. Typical magnetic properties of the obtained compound powders were as follows: Jr=0.98 T, Hcj= 765.1 kA/m, HcB = 545.4 kA/m, (BH)max = 138.5 kJ/m3 (17.4 MGOe), and T c=523°C. It was found that this sample was an exchange spring magnet from recoil loops of the hysteresis curve, X-ray diffraction patterns and σ-T (Magnetization-Temperature) curve. The value of (BH)max for a compression-molded isotropic bonded magnet prepared by using {Sm 10(Fe0.9Co0.1)89.4Cr 0.3Y0.3}86.6N13.4 powder was 96.2kJ/m3 (12.1 MGOe), when the density of bonded magnet was 6.05 Mg/m 3. And the average reversible temperature coefficient of J r was α(Jr)ave=- 0.05 %/°C, the temperature coefficient of Hcj in the range from 25°C to 125°C obtained by a linear extrapolation was α (Hcj)=- 0.40 %/°C.
引用
收藏
相关论文
共 50 条
  • [21] Structure and magnetic properties of SmCo7-xTix with TbCu7-type structure
    Zhou, J
    Al-Omari, IA
    Liu, JP
    Sellmyer, DJ
    JOURNAL OF APPLIED PHYSICS, 2000, 87 (09) : 5299 - 5301
  • [22] Preparation of TbCu7-type Sm-Fe powders by low-temperature HDDR treatment
    Takagi, Kenta
    Jinno, Miho
    Ozaki, Kimihiro
    JOURNAL OF MAGNETISM AND MAGNETIC MATERIALS, 2018, 454 : 170 - 175
  • [23] Effects of Hf and CNTs on magnetic transformation and thermal stabilities of TbCu7-type Sm-Co matrix ribbon magnets
    Sun, Ji-Bing
    Han, Dan
    Cui, Chun-Xiang
    Yang, Wei
    Zhou, Hao
    Tian, Rui-Ting
    Yang, Li-Guo
    JOURNAL OF ALLOYS AND COMPOUNDS, 2009, 487 (1-2) : 626 - 630
  • [24] Development of TbCu7-type Sm-Fe-N anisotropic magnet powder and its sintered magnets
    Sato, Suguru
    Nishikawa, Kenichi
    Node, Eri
    Okada, Shusuke
    JOURNAL OF ALLOYS AND COMPOUNDS, 2022, 929
  • [25] Effect of niobium substitution on microstructures and thermal stability of TbCu7-type Sm-Fe-N magnets
    Wu, Guiyong
    Li, Hongwei
    Yu, Dunbo
    Li, Kuoshe
    Yan, Wenlong
    Yuan, Chao
    Sun, Liang
    Luo, Yang
    Zhang, Kun
    JOURNAL OF RARE EARTHS, 2018, 36 (03) : 281 - 286
  • [26] Effect of niobium substitution on microstructures and thermal stability of TbCu7-type Sm-Fe-N magnets
    Guiyong Wu
    Hongwei Li
    Dunbo Yu
    Kuoshe Li
    Wenlong Yan
    Chao Yuan
    Liang Sun
    Yang Luo
    Kun Zhang
    Journal of Rare Earths, 2018, 36 (03) : 281 - 286
  • [27] Development of TbCu7-type Sm-Fe-N anisotropic magnet powder and its sintered magnets
    Sato, Suguru
    Nishikawa, Kenichi
    Node, Eri
    Okada, Shusuke
    Journal of Alloys and Compounds, 2022, 929
  • [28] Magnetic properties and magnetization behavior of SmCo-based magnets with TbCu7-type structure
    泮敏翔
    张朋越
    葛洪良
    吴琼
    俞能君
    Journal of Rare Earths, 2013, 31 (03) : 262 - 266
  • [29] Magnetic behavior of rapidly solidified Pr-Co alloys with the TbCu7-type structure
    Kostogorova, J.
    Shield, J. E.
    JOURNAL OF APPLIED PHYSICS, 2006, 99 (08)
  • [30] Effect of Ti Addition on Magnetic Properties of TbCu7-lype Sm-Fe-Co-Mn System Nitrides
    Yamamoto, Hiroshi
    Osanai, Kenta
    ELECTRONICS AND COMMUNICATIONS IN JAPAN, 2008, 91 (07) : 25 - 31