Improving structure stability of single-crystalline Ni-rich cathode at high voltage by element gradient doping and interfacial modification

被引:5
|
作者
Wang, Ruijuan [1 ]
Zhang, Yixu [1 ]
Li, Zhi [1 ]
Wu, Lei [1 ]
Chen, Jiarui [1 ]
Liu, Xiaolin [1 ]
Hu, Hui [1 ]
Ding, Hao [1 ]
Cao, Shuang [1 ]
Wei, Qiliang [2 ]
Wang, Xianyou [1 ]
机构
[1] Xiangtan Univ, Sch Chem,Natl Base Int Sci & Technol Cooperat New, Natl Local Joint Engn Lab Key Mat New Energy Stora, Hunan Prov Key Lab Electrochem Energy Storage & Co, Xiangtan 411105, Peoples R China
[2] Ningbo Univ Technol, Inst Micro Nano Mat & Devices, Ningbo 315211, Zhejiang, Peoples R China
来源
关键词
Single-crystalline Ni-rich cathode; High cut-off voltage; Material fragmentation; Li4TeO5 coating layer; Te6+doping; DEGRADATION;
D O I
10.1016/j.jechem.2024.10.015
中图分类号
O69 [应用化学];
学科分类号
081704 ;
摘要
Single-crystalline Ni-rich cathodes can provide high energy density and capacity retention rates for lithium-ion batteries (LIBs). However, single-crystalline Ni-rich cathodes experience severe transition metal dissolution, irreversible phase transitions, and reduced structural stability during prolonged cycling at high voltage, which will significantly hinder their practical application. Herein, a Li4TeO5 surface coating along with bulk Te-gradient doping strategy is proposed and developed to solve these issues for single-crystalline Ni-rich LiNi0.90Co0.05Mn0.05O2 cathode (LTeO-1.0). It has been found that the bulk Te6+ gradient doping can lead to the formation of robust Te-O bonds that effectively inhibit H2-H3 phase transformations and reinforce the lattice framework, and the in-situ Li4TeO5 coating layer can act as a protective layer that suppresses the parasitic reactions and grain fragmentation. Besides, the modified material exhibits a higher Young's modulus, which will be conducive to maintaining significant structural and electrochemical stability under high-voltage conditions. Especially, the LTeO-1.0 electrode shows the improved Li+ diffusion kinetics and thermodynamic stability as well as high capacity retention of 95.83% and 82.12% after 200 cycles at the cut-off voltage of 4.3 and 4.5 V. Therefore, the efficacious dualmodification strategy will definitely contribute to enhancing the structural and electrochemical stability of single-crystalline Ni-rich cathodes and developing their application in LIBs. (c) 2024 Science Press and Dalian Institute of Chemical Physics, Chinese Academy of Sciences. Published by Elsevier B.V. and Science Press. All rights are reserved, including those for text and data mining, AI training, and similar technologies.
引用
收藏
页码:630 / 640
页数:11
相关论文
共 50 条
  • [21] Overall structural modification of a layered Ni-rich cathode for enhanced cycling stability and rate capability at high voltage
    Tang, Manjing
    Yang, Jun
    Chen, Nantao
    Zhu, Shengcai
    Wang, Xing
    Wang, Tian
    Zhang, Congcong
    Xia, Yongyao
    JOURNAL OF MATERIALS CHEMISTRY A, 2019, 7 (11) : 6080 - 6089
  • [22] Mechanical densification synthesis of single-crystalline Ni-rich cathode for high-energy lithium-ion batteries
    Nam, Gwonsik
    Hwang, Jaeseong
    Kang, Donghun
    Oh, Sieon
    Chae, Sujong
    Yoon, Moonsu
    Ko, Minseong
    JOURNAL OF ENERGY CHEMISTRY, 2023, 79 : 562 - 568
  • [23] Mechanical densification synthesis of single-crystalline Ni-rich cathode for high-energy lithium-ion batteries
    Gwonsik Nam
    Jaeseong Hwang
    Donghun Kang
    Sieon Oh
    Sujong Chae
    Moonsu Yoon
    Minseong Ko
    Journal of Energy Chemistry, 2023, 79 (04) : 562 - 568
  • [24] Improving electrochemical characteristics of Ni-rich cathode materials by Na doping
    Hwang, Do-Young
    Lee, Seung-Hwan
    JOURNAL OF CERAMIC PROCESSING RESEARCH, 2021, 22 (06): : 615 - 619
  • [25] Challenges and Modification Strategies of Ni-Rich Cathode Materials Operating at High-Voltage
    Liao, Caijian
    Li, Fangkun
    Liu, Jun
    NANOMATERIALS, 2022, 12 (11)
  • [26] A Universal Molten Salt Method for Direct Upcycling of Spent Ni-rich Cathode towards Single-crystalline Li-rich Cathode
    Qin, Zuoyu
    Zhang, Ying
    Luo, Wuqing
    Zhang, Tao
    Wang, Tao
    Ni, Lianshan
    Wang, Haoji
    Zhang, Ning
    Liu, Xiaohe
    Zhou, Jiang
    Chen, Gen
    ANGEWANDTE CHEMIE-INTERNATIONAL EDITION, 2023, 62 (25)
  • [27] Improving interfacial stability of ultrahigh-voltage lithium metal batteries with single-crystal Ni-rich cathode via a multifunctional additive strategy
    Zhang, Zhi
    Liu, Fangyan
    Huang, Zeyu
    Yi, Maoyi
    Fan, Xinming
    Bai, Maohui
    Hong, Bo
    Zhang, Zhian
    Li, Jie
    Lai, Yanqing
    JOURNAL OF COLLOID AND INTERFACE SCIENCE, 2022, 608 : 1471 - 1480
  • [28] Upcycling spent cathodes into single-crystalline Ni-rich cathode materials through selective lithium extraction
    Kim, Kyoung Sun
    Jeon, Min Ku
    Song, Seok Hyun
    Hong, Seokjae
    Kim, Hwa Soo
    Kim, Sung-Wook
    Kim, Jinsoo
    Oh, Pilgun
    Hwang, Junhyeok
    Song, Jinju
    Ma, Jiyoung
    Woo, Jung-Je
    Yu, Seung-Ho
    Kim, Hyungsub
    JOURNAL OF MATERIALS CHEMISTRY A, 2023, 11 (39) : 21222 - 21230
  • [29] Surface Reduction Stabilizes the Single-Crystalline Ni-Rich Layered Cathode for Li-Ion Batteries
    Fan, Qinglu
    Zuba, Mateusz Jan
    Zong, Yanxu
    Menon, Ashok S.
    Pacileo, Anthony T.
    Piper, Louis F. J.
    Zhou, Guangwen
    Liu, Hao
    ACS APPLIED MATERIALS & INTERFACES, 2022, 14 (34) : 38795 - 38806
  • [30] Single-Crystalline Ni-Rich LiNixMnyCo1-x-yO2 Cathode Materials: A Perspective
    Zhang, Hao
    He, Xinzi
    Chen, Zonghai
    Yang, Yang
    Xu, Hong
    Wang, Li
    He, Xiangming
    ADVANCED ENERGY MATERIALS, 2022, 12 (45)