Evaluation indices of freezing-thawing destruction for airfield runway concrete

被引:0
|
作者
Dun, Xiao [1 ]
Cen, Guo-Ping [1 ]
Huang, Can-Hua [1 ]
Zhou, Qi [1 ]
Jiang, Jian-Wen [2 ]
Yang, Xin [2 ]
机构
[1] School of Engineering, Air Force University of Engineering, Xi'an 710038, Shaanxi, China
[2] Airport and Barracks Department, Air Force Logistics Department, Beijing 100720, China
关键词
Concretes - Thawing - Bending strength - Elastic moduli;
D O I
暂无
中图分类号
学科分类号
摘要
In order to research the evaluation indices of freezing-thawing destruction for airfield runway concrete in north cold area of China, three concrete examples with anti-freezing capability were made, and their freezing-thawing devastating experiment was done by rapid freezing experimental machine. Their dynamic moduli of elasticity were measured by DT-10W, and the changing rules of relative dynamic moduli of elasticity, flexural strength losses, concrete mass losses and surface scale-offs under different freezing-thawing cycles were analyzed. The critical value of freezing-thawing destruction was presented for airfield runway concrete. Experimental result indicates that as freezing-thawing cycles accumulate, the compressive and flexural strengthes decline at different rates for the samples, of which the flexural strengthes lose more faster. The surface scaling areas and depthes of concretes become serious and mass losses have severe influence on the surface smoothnesses of the samples. According to the rules, the evaluation indices are put forward after 300 freezing-thawing cycles, which is that relative dynamic modulus of elasticity is less than 75% (flexural strength loss ratio is not more than 46%) and mass loss ratio is less than 1.0% (moderate surface scale-off).
引用
收藏
页码:13 / 18
相关论文
共 50 条
  • [41] Investigation of Microstructural Damage in Ultrahigh-Performance Concrete under Freezing-Thawing Action
    Gu, Chunping
    Sun, Wei
    Guo, Liping
    Wang, Qiannan
    Liu, Jintao
    Yang, Yang
    Shi, Tao
    ADVANCES IN MATERIALS SCIENCE AND ENGINEERING, 2018, 2018
  • [42] Freezing-thawing processes in glass fiber board
    Hokoi, S.
    Hatano, M.
    Matsumoto, M.
    Kumaran, M.K.
    Journal of Thermal Envelope and Building Science, 2000, 24 (01): : 42 - 60
  • [43] Laboratory Investigation on Preplaced Ballast Aggregate Concrete Deterioration over Freezing-Thawing Cycles
    Esmaeili, Morteza
    Behnajad, Sajad
    Esfahani, Milad Hossein
    INTERNATIONAL JOURNAL OF CONCRETE STRUCTURES AND MATERIALS, 2023, 17 (01)
  • [44] Degradation Mechanism and Numerical Simulation of Pervious Concrete under Salt Freezing-Thawing Cycle
    Xiang, Junzheng
    Liu, Hengrui
    Lu, Hao
    Gui, Faliang
    MATERIALS, 2022, 15 (09)
  • [45] The influence of freezing-thawing cycles on the capillary water absorption and porosity of concrete with mineral admixture
    Tahir Gonen
    Salih Yazicioglu
    Bahar Demirel
    KSCE Journal of Civil Engineering, 2015, 19 : 667 - 671
  • [46] Bond Deterioration Mechanism and Its Modeling for Reinforced Concrete Subjected to Freezing-Thawing Action
    Kanazawa, T.
    Sato, Y.
    CONCREEP 10: MECHANICS AND PHYSICS OF CREEP, SHRINKAGE, AND DURABILITY OF CONCRETE AND CONCRETE STRUCTURES, 2015, : 1245 - 1250
  • [47] Effect of expansive agent, fiber or their combination on freezing-thawing durability of high performance concrete
    College of Aerospace Engineering, Nanjing University of Aeronautics and Astronautics, Nanjing 210016, China
    不详
    Nanjing Hangkong Hangtian Daxue Xuebao, 2006, 2 (245-250):
  • [48] Effect of freezing-thawing and ageing on thermal characteristics and mechanical properties of conductive asphalt concrete
    Pan, Pan
    Wu, Shaopeng
    Hu, Xiaodi
    Wang, Peng
    Liu, Quantao
    CONSTRUCTION AND BUILDING MATERIALS, 2017, 140 : 239 - 247
  • [49] Monitoring the residual strain of concrete in a freezing-thawing environment using white light interferometer
    Lv, Haifeng
    Liao, Kaixing
    Kong, Xianglong
    Zhao, Xuefeng
    Sun, Changsen
    COLD REGIONS SCIENCE AND TECHNOLOGY, 2017, 142 : 132 - 138
  • [50] Meso-Scale Failure of Freezing-Thawing Damage of Concrete under Uniaxial Compression
    Si, Zheng
    Du, Xiaoqi
    Huang, Lingzhi
    Li, Yanlong
    APPLIED SCIENCES-BASEL, 2020, 10 (04):