Microstructural evolution, crystallographic texture, grain morphology, and mechanical integrity of wire arc additively manufactured Inconel 625 alloy

被引:5
|
作者
Kishor, Gaurav [1 ]
Mugada, Krishna Kishore [1 ]
Mahto, Raju Prasad [1 ]
Sivanandam, Aravindan [2 ]
Digavalli, Ravi Kumar [2 ]
Amirthalingam, Murugaiyan [3 ]
机构
[1] Sardar Vallabhbhai Natl Inst Technol Surat, Dept Mech Engn, Surat, India
[2] Indian Inst Technol, Dept Mech Engn, Delhi, India
[3] Indian Inst Technol Madras, Dept Met & Mat Engn, Chennai, India
关键词
Inconel; 625; Microstructure; Crystallographic texture; Recrystallization; Anisotropy; DEPOSITION; SINGLE;
D O I
10.1016/j.matchar.2024.114525
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The material in wire arc additive manufacturing (WAAM) undergoes complex material flow and multiple thermal heating and cooling cycles, forming highly heterogeneous microstructures in terms of size, crystallographic orientations, and mechanical properties. The inhomogeneity also depends on the dislocation density and phases, which are influenced by the thermal history of the process. In this study, the Cold Metal Transfer (CMT) process was used to deposit a 60-layer build of Inconel 625 alloy. Detailed variations in the microstructural size, orientations, and phases along the building direction were studied using optical microscopy, electron backscatter diffraction (EBSD), and X-ray diffraction (XRD). Microstructural observations reveal dendrites, equiaxed crystals, cellular, and columnar structures with primary and secondary dendrites. Dynamic recrystallization (DRX) followed by abnormal grain growth was found in the build. The average grain size varies with deposited height, with a grain size of around 13 f 1 mu m near the substrate, 45 f 1 mu m in the middle region, and 18 f 1 mu m at the top. The top region exhibited a strong intensity of recrystallized Cube, Cube-ND, and Cube-RD textures, with weaker intensities of copper and brass textures. The middle and bottom regions show strong intensities of Goss, copper, F, S, and E textures, respectively. The highest dislocation density of 5.122 x 10-4 nm- 2 was found in the top region, while the lowest (4.14 x 10-4 nm- 2) was observed in the bottom region. The ultimate tensile strength of the build ranged from 603 f 05 MPa to 699 f 10 MPa, while the yield strength varied from 313 f 07 MPa to 365 f 08 MPa along different orientations. Vickers hardness results showed a slight variation, from 240 f 5 to 260 f 2 HV, from bottom to the top of the deposited build. The findings from this study provide valuable insights into the microstructural evolution mechanism and mechanical behavior of WAAM-fabricated Inconel 625, which can guide other researchers in optimizing process parameters, enhancing material properties, and understanding the effects of thermal history on additive manufacturing of high-performance alloys.
引用
收藏
页数:19
相关论文
共 50 条
  • [31] Investigation of Microstructural Properties and Mechanical Behavior of Wire Arc Additively Manufactured Incoloy 825
    Chigilipalli, Bharat Kumar
    Veeramani, Anandakrishnan
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2024, 33 (06) : 2837 - 2852
  • [32] Effect of robotic weaving motion on mechanical and microstructural characteristics of wire arc additively manufactured NiTi shape memory alloy
    Gonela, Karuna Kumar
    Vijayavarman, Chakkravarthy
    Palanivel, Manojkumar
    Mariappan, Lakshmanan
    Ramasubramanian, Lakshmi Narayan
    Kannan, Arasappan Rajesh
    INTERNATIONAL JOURNAL OF MATERIALS RESEARCH, 2023, 114 (10-11) : 947 - 954
  • [33] Comprehensive and Comparative Heat Treatment of Additively Manufactured Inconel 625 Alloy and Corresponding Microstructures and Mechanical Properties
    Luna, Victoria
    Trujillo, Leslie
    Gamon, Ariel
    Arrieta, Edel
    Murr, Lawrence E.
    Wicker, Ryan B.
    Katsarelis, Colton
    Gradl, Paul R.
    Medina, Francisco
    JOURNAL OF MANUFACTURING AND MATERIALS PROCESSING, 2022, 6 (05):
  • [34] Improvement in corrosion resistance of wire arc additive manufactured Inconel 625 alloy through heat treatment
    Zhao, Xipeng
    Di, Xinjie
    Zhang, Xi
    Li, Chengning
    MATERIALS RESEARCH EXPRESS, 2021, 8 (06)
  • [35] Influence of Shielding Gas Composition on Structure and Mechanical Properties of Wire and Arc Additive Manufactured Inconel 625
    Ivan Jurić
    Ivica Garašić
    Matija Bušić
    Zoran Kožuh
    JOM, 2019, 71 : 703 - 708
  • [36] Influence of Shielding Gas Composition on Structure and Mechanical Properties of Wire and Arc Additive Manufactured Inconel 625
    Juric, Ivan
    Garasic, Ivica
    Busic, Matija
    Kozuh, Zoran
    JOM, 2019, 71 (02) : 703 - 708
  • [37] Effects of wire-EDM parameters on the surface integrity and mechanical characteristics of additively manufactured Inconel 939
    Ozaner, Ozan Can
    Dursun, Gokhan
    Akbulut, Guray
    MATERIALS TODAY-PROCEEDINGS, 2021, 38 : 1861 - 1865
  • [38] Mechanical and microstructural features of wire-and-arc additively manufactured carbon steel thick plates
    Laghi, Vittoria
    Arre, Lidiana
    Tonelli, Lavinia
    Di Egidio, Gianluca
    Ceschini, Lorella
    Monzon, Ivan
    Laguia, Alberto
    Dieste, Jose Antonio
    Palermo, Michele
    INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2023, 127 (3-4): : 1391 - 1405
  • [39] Microstructural heterogeneity and exceptional mechanical properties in a wire-arc additively manufactured stainless steel
    Jafarzad-Shayan, M. M.
    Zarei-Hanzaki, A.
    Moshiri, A.
    Kim, H. Seop
    Haftlang, F.
    Tahaghoghi, M.
    Mahmoudi, M.
    Momeni, M.
    Abedi, H. R.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2023, 882
  • [40] Effects of the grain shape and crystallographic texture on the grain-scale mechanical behavior of additively manufactured aluminum alloys
    Romanova, V
    Zinovieva, O.
    Balokhonov, R.
    Dymnich, E.
    Moskvichev, E.
    Filippov, A.
    Lychagin, D.
    ADDITIVE MANUFACTURING, 2021, 48