Assessment of carbonation and corrosion in a 50-year-old reinforced concrete building

被引:0
|
作者
Dudi, Lupesh [1 ]
Bishnoi, Shashank [1 ]
机构
[1] Indian Inst Technol Delhi, Dept Civil Engn, New Delhi 110016, India
关键词
Non-destructive testing; Long-term natural carbonation; Accelerated carbonation; Mineralogy; Corrosion assessment; PORE SOLUTION; ACCELERATED CARBONATION; CEMENT PASTE; CALCIUM-CARBONATE; TRANSFORMATION; DURABILITY; RETENTION; MECHANISM; KINETICS; POROSITY;
D O I
10.1617/s11527-024-02487-8
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
This paper presents an investigation conducted on a 50-year-old structure in a composite climactic zone of India. The study comprises two parts, one covering the comparison of long-term natural and short-term accelerated carbonation while another revealing insight into the structure's durability and potential concerns. Mineralogy, pore solution, and transport properties comparison of natural and accelerated carbonated concrete samples highlight similar modifications, demonstrating the representative nature of accelerated carbonation at 3% carbon dioxide concentration. However, accelerated carbonation led to the preferred precipitation of calcite and a higher degree of C-S-H carbonation. Core strength and carbonation depth measurements indicate that the carbonation coefficient shows a high variation within the structure due to micro-climatic conditions, and there is a need to consider carbon dioxide concentration greater than 400 ppm for residential buildings. Additional investigations based on half-cell potential, surface resistivity, and corrosion rate measurement highlighted that moisture availability is the main deterioration-controlling factor during the propagation phase. Also, it was realized that during an inspection, if different non-destructive measurements fall in the middle range, it becomes inconclusive to ascertain the severity of corrosion. In such situations, visual inspection of the reinforcement is imperative. Finally, the authors recommend collecting data on carbon dioxide concentration and the moisture state of different locations in the structure during structural inspection.
引用
收藏
页数:18
相关论文
共 50 条
  • [21] Exertional dyspnea in a 50-year-old man
    Singh, Amita
    Kala, Jaya
    Sahay, Sandeep
    Shah, Ashok
    SAUDI MEDICAL JOURNAL, 2006, 27 (09) : 1439 - 1440
  • [22] 50-Year-Old Man With Hematochezia and Fatigue
    Busebee, Bradley T.
    Zhong, Qiaonan
    Murray, Joseph A.
    MAYO CLINIC PROCEEDINGS, 2023, 98 (02) : 332 - 336
  • [23] Nasal discharge in a 50-year-old woman
    Chamberlain, W
    White, MD
    Wians, FH
    Willis, MS
    LABORATORY MEDICINE, 2004, 35 (05) : 279 - 283
  • [24] 50-year-old woman with pulmonary infiltrates
    Diaz, Marta
    Martin, Natalia
    Maria Fraile, Jose
    Xavier Zamora, Francisco
    MEDICINA CLINICA, 2009, 133 (08): : 321 - 321
  • [25] Palatal ulcer in a 50-year-old patient
    Voigtlaender, C.
    Schuler, G.
    Simon, M., Jr.
    HAUTARZT, 2007, 58 (02): : 161 - 162
  • [26] 50-YEAR-OLD MAN WITH FEVER AND RHINORRHEA
    STEPANEK, J
    UTZ, JP
    MAYO CLINIC PROCEEDINGS, 1995, 70 (05) : 489 - 492
  • [27] Mathematicians crack 50-year-old problem
    Whyte, Chelsea
    NEW SCIENTIST, 2019, 243 (3248) : 13 - 13
  • [28] A 50-Year-Old Male With A Hypothalamic Mass
    Podgorski, Andrzej
    Zielinski, Grzegorz
    Grala, Bartlomiej
    Koziarski, Andrzej
    BRAIN PATHOLOGY, 2019, 29 (03) : 455 - 456
  • [29] A 50-year-old woman with spinal stenosis
    Mazanec, D
    Drucker, Y
    JAMA-JOURNAL OF THE AMERICAN MEDICAL ASSOCIATION, 1996, 275 (18): : 1401 - 1401
  • [30] The Search for the Missing 50-Year-Old Gold
    Violette, David B., Jr.
    ADVANCES IN SKIN & WOUND CARE, 2014, 27 (10) : 444 - 446