Dephosphorization study on hydrogen reduction-melting separation of high-phosphorus oolitic hematite

被引:0
|
作者
Zhao, Yijiang [1 ]
Ma, Jianghua [1 ]
Yang, Chaoxin [1 ]
Huang, Jipeng [1 ]
Liu, Yu [2 ]
He, Zhu [1 ]
Li, Guangqiang [1 ,2 ,3 ]
机构
[1] Wuhan Univ Sci & Technol, Key Lab Ferrous Met & Resources Utilizat, Minist Educ, Wuhan 430081, Hubei, Peoples R China
[2] Wuhan Univ Sci & Technol, State Key Lab Refractories & Met, Wuhan 430081, Hubei, Peoples R China
[3] Wuhan Univ Sci & Technol, Hubei Prov Key Lab New Proc Ironmaking & Steelmaki, Wuhan 430081, Hubei, Peoples R China
关键词
High-phosphorus oolitic hematite; DRI; Melting separation; Slag; Dephosphorization; MOLTEN STEEL; IRON-ORES; SLAGS;
D O I
10.1016/j.jmrt.2024.11.025
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In order to clarify the dephosphorization mechanism of DRI (Direct Reduced Iron) derived from hydrogen reduced high-phosphorus iron ore during the electric arc furnace melting process, slag was prepared using reagent-grade powder based on the gangue mineral composition of high-phosphorus oolitic hematite. By incorporating varying amounts of CaO, FeOx, and reduced iron powder, experiments simulating the dephosphorization of melting separation slag from DRI with different basicity and metallization rates were conducted at 1873 K. The results show that phosphorus in the iron primarily exists in the form of Fe-P-O spherical slag inclusions and FexP, while in the slag, phosphorus mainly resides within the silicate phases. As the amount of CaO added increases, there is a significant decrease in the phosphorus content within the slag inclusions, and the Pcontaining compounds in the iron gradually shift from FexP and Fe3(PO4)2 to FeO. As the dephosphorization capacity of the slag increases, the distribution of phosphorus-rich phases in the rapidly cooled slag becomes more extensive. When the basicity increases to 3, the phosphorus-rich phases in the slag transition to 2CaO & sdot;SiO2 and 3CaO & sdot;SiO2. When the basicity is fixed at 2.5, regulating the metallization rate can control the FeOx content in the molten slag, thereby enhancing the dephosphorization ability of slag. The results show that under conditions of a DRI basicity of 2.5 and a metallization rate of 85%, slag/metal separation can produce low-phosphorus iron with 0.022 wt% P, achieving a dephosphorization rate exceeding 95%.
引用
收藏
页码:6756 / 6766
页数:11
相关论文
共 50 条
  • [21] Direct Reduction of High-phosphorus Oolitic Hematite Ore Based on Biomass Pyrolysis
    Huang, Dong-bo
    Zong, Yan-bing
    Wei, Ru-fei
    Gao, Wei
    Liu, Xiao-ming
    JOURNAL OF IRON AND STEEL RESEARCH INTERNATIONAL, 2016, 23 (09) : 874 - 883
  • [22] Effects of sodium salts on reduction roasting and Fe-P separation of high-phosphorus oolitic hematite ore
    Li, Guanghui
    Zhang, Shuhui
    Rao, Mingjun
    Zhang, Yuanbo
    Jiang, Tao
    INTERNATIONAL JOURNAL OF MINERAL PROCESSING, 2013, 124 : 26 - 34
  • [23] Effect of Na2CO3 and CaCO3 on deep dephosphorization by the direct reduction of high-phosphorus oolitic hematite
    Xu, Hongda
    Li, Rui
    Kou, Jue
    Wen, Xiaojin
    Zhang, Jun
    Geng, Chao
    Sun, Tichang
    PHYSICOCHEMICAL PROBLEMS OF MINERAL PROCESSING, 2024, 60 (06):
  • [24] The function of blast furnace dust as reductant on simultaneous reduction of high-phosphorus oolitic hematite
    Cao, Yun-ye
    Duan, Dong-ping
    Zhou, E.
    Sun, Ti-chang
    IRONMAKING & STEELMAKING, 2020, 47 (05) : 520 - 530
  • [25] Phosphorus Removal and Iron Recovery from High-Phosphorus Hematite Using Direct Reduction Followed by Melting Separation
    Tang, Huiqing
    Qin, Yanqi
    Qi, Tengfei
    MINERAL PROCESSING AND EXTRACTIVE METALLURGY REVIEW, 2016, 37 (04): : 236 - 245
  • [26] Dephosphorisation of high phosphorus oolitic hematite by carbon composite pre-reduction and fast melting separation
    Wang, G.
    Liu, J.
    Wang, J. S.
    Xue, Q. G.
    IRONMAKING & STEELMAKING, 2015, 42 (09) : 689 - 697
  • [27] Dephosphorization of high phosphorus oolitic hematite by acid leaching and the leaching kinetics
    Wang, H. H.
    Li, G. Q.
    Zhao, D.
    Ma, J. H.
    Yang, J.
    HYDROMETALLURGY, 2017, 171 : 61 - 68
  • [28] Application of Wood Char in Processing Oolitic High-phosphorus Hematite for Phosphorus Removal
    Tang, Hui-qing
    Qin, Yan-qi
    Qi, Teng-fei
    Dong, Zhi-lei
    Xue, Qing-guo
    JOURNAL OF IRON AND STEEL RESEARCH INTERNATIONAL, 2016, 23 (02) : 109 - 115
  • [29] Application of Wood Char in Processing Oolitic High-phosphorus Hematite for Phosphorus Removal
    Hui-qing Tang
    Yan-qi Qin
    Teng-fei Qi
    Zhi-lei Dong
    Qing-guo Xue
    Journal of Iron and Steel Research International, 2016, 23 : 109 - 115
  • [30] Red mud as a green dephosphorization agent: Co-reduction with high phosphorus oolitic hematite for iron extraction and dephosphorization
    Wang, Xiaoping
    Lu, Wenda
    Rong, Lingkun
    Wu, Shichao
    Ma, Zhenyuan
    Luo, Na
    Shi, Jingyang
    PROCESS SAFETY AND ENVIRONMENTAL PROTECTION, 2025, 193 : 990 - 1001