Achieving high strength-ductility of AZ91 magnesium alloy via wire-arc directed energy deposition assisted by interlayer friction stir processing

被引:1
|
作者
Wei, Jingxun [1 ,2 ]
He, Changshu [1 ,2 ,3 ]
Qie, Mofan [1 ,2 ]
Liu, Yunan [1 ,2 ]
Zhou, Hao [1 ,2 ]
Kang, Chenxi [1 ,2 ]
Qin, Gaowu [1 ,2 ,3 ]
机构
[1] Northeastern Univ, Sch Mat Sci & Engn, Shenyang 110819, Peoples R China
[2] Northeastern Univ, Key Lab Anisotropy & Texture Mat, Shenyang 110819, Peoples R China
[3] Northeastern Univ, Res Ctr Met Wires, Shenyang 110819, Peoples R China
关键词
Wire-arc directed energy deposition; Friction stir processing; AZ91 magnesium alloy; Microstructure evolution; Mechanical properties; MECHANICAL-PROPERTIES; MICROSTRUCTURE EVOLUTION; PERFORMANCE; DEPENDENCE; BEHAVIOR; TEXTURE;
D O I
10.1016/j.addma.2024.104453
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The coarse grain size and poor mechanical properties of wire-arc directed energy deposition (DED) magnesium (Mg) alloys have hindered their wider application. In this study, the AZ91 Mg alloy component was fabricated by wire-arc DED assisted by interlayer friction stir processing (IFSP), and the highest strength and elongation were obtained in wire-arc DED AZ91 Mg alloy, which was mainly attributed to grain refinement, fragmentation/ dispersion/dissolution of beta-Mg17Al12 phase and heterogeneous microstructure in the IFSP stir zone (SZ). The formation of heterogeneous structure is caused by the fact that the refined grains in the SZ of the previous layer are affected by the thermal cycling of the subsequent additive manufacturing process, which led to different degrees of grain growth in different micro-zones within a SZ, and ultimately formed the microstructure characteristics with alternating distribution of coarse and fine grains. Compared with the wire-arc DED samples, the ultimate tensile strength of the wire-arc DED + IFSP samples in the perpendicular and parallel to the building directions increased from 284 and 264 MPa to 315 and 324 MPa, respectively. These values are comparable to those of their wrought counterparts, and the elongation increased by over 50 %. This study thus provides new insights into microstructure modification and performance enhancement of wire-arc DED fabricated Mg-alloys via a novel IFSP technique.
引用
收藏
页数:13
相关论文
共 50 条
  • [41] Superplastic tensile behavior of a fine-grained AZ91 magnesium alloy prepared by friction stir processing
    Zhang, Datong
    Wang, Saixiang
    Qiu, Chen
    Zhang, Wen
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2012, 556 : 100 - 106
  • [42] Achieving exceptional strength-ductility synergy of laser direct energy deposited AA7075 alloy by subsequent friction stir processing
    Lv, Jiming
    Lu, Haifei
    Zhang, Hongmei
    Sun, Zhonggang
    Luo, Kaiyu
    Lu, Jinzhong
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2025, 923
  • [43] Enhanced Strength–Ductility Synergy in Submerged Friction Stir Processing ER2319 Alloy Manufactured by Wire-Arc Additive Manufacturing via Creating Ultrafine Microstructure
    Jinpeng Hu
    Tao Sun
    Fujun Cao
    Yifu Shen
    Zhiyuan Yang
    Chan Guo
    Acta Metallurgica Sinica (English Letters), 2024, 37 : 793 - 807
  • [44] Superplastic behaviour of friction stir processed AZ91 magnesium alloy produced by high pressure die cast
    Cavaliere, P.
    De Marco, P. P.
    JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2007, 184 (1-3) : 77 - 83
  • [45] Fatigue behaviour of friction stir processed AZ91 magnesium alloy produced by high pressure die casting
    Cavaliere, P.
    De Marco, P. P.
    MATERIALS CHARACTERIZATION, 2007, 58 (03) : 226 - 232
  • [46] Microstructure, hardness, and wear resistance of AZ91 magnesium alloy produced by friction stir processing with air-cooling
    Iwaszko, Jozef
    Kudla, Krzysztof
    INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2021, 116 (3-4): : 1309 - 1323
  • [47] Enhanced corrosion resistance of AZ91 magnesium alloy through refinement and homogenization of surface microstructure by friction stir processing
    Liu, Qu
    Ma, Qing-xian
    Chen, Gao-qiang
    Cao, Xiong
    Zhang, Shuai
    Pan, Ji-luan
    Zhang, Gong
    Shi, Qing-yu
    CORROSION SCIENCE, 2018, 138 : 284 - 296
  • [48] EFFECT OF PROCESSING PARAMETERS ON THERMO-MECHANICALLY AFFECTED ZONE OF FRICTION STIR PROCESSED AZ91 MAGNESIUM ALLOY
    Taherishargh, M.
    Parvin, N.
    Asadi, P.
    PROCEEDINGS OF THE ASME 10TH BIENNIAL CONFERENCE ON ENGINEERING SYSTEMS DESIGN AND ANALYSIS, 2010, VOL 1, 2010, : 627 - 631
  • [49] Microstructure, hardness, and wear resistance of AZ91 magnesium alloy produced by friction stir processing with air-cooling
    Józef Iwaszko
    Krzysztof Kudła
    The International Journal of Advanced Manufacturing Technology, 2021, 116 : 1309 - 1323
  • [50] Pre-weld friction stir processing enabling strong and ductile fusion welds on AZ91 magnesium alloy
    Sharahi, Hasan Jiryaei
    Pouranvari, Majid
    Movahedi, Mojtaba
    SCIENCE AND TECHNOLOGY OF WELDING AND JOINING, 2023, 28 (02) : 162 - 171