Effect of Hot Extrusion Processes on the Thermoelectric and Mechanical Properties of Bi2Te2.7Se0.3 Materials

被引:0
|
作者
Li, Quan [1 ,2 ]
Xing, Tong [2 ]
Li, Xiaoya [2 ]
Qiu, Pengfei [2 ]
Shi, Xun [2 ]
机构
[1] School of Materials and Chemistry, University of Shanghai for Science and Technology, Shanghai,200093, China
[2] State Key Laboratory of High Performance Ceramics and Superfine Microstructure, Shanghai Institute of Ceramics, Chinese Academy of Sciences, Shanghai,200050, China
关键词
Bismuth alloys - Bismuth compounds - Continuous casting - Crystal whiskers - Die casting - Disintegration - Extrusion molding - Ingot molds - Ingots - Machinability - Patternmaking - Pressure pouring - Semiconducting tellurium compounds - Shaw process;
D O I
10.14062/j.issn.0454-5648.20240245
中图分类号
学科分类号
摘要
Introduction Bi2Te3-based alloys are the most well-known thermoelectric materials for room-temperature applications. The existing Bi2Te3-based thermoelectric materials produced commercially are prepared by a zone melting method, resulting in highly oriented materials with high thermoelectric properties. However, the ingots produced by the zone melting method are prone to disintegration due to the weak van der Waals forces between the layers of Te atoms, leading to the poor mechanical properties and the proclivity for fracture during processing and practical applications. It is thus important to improve the mechanical properties and machinability of Bi2Te3-based materials with the excellent thermoelectric properties. This work was to prepare a n-type Bi2Te2.7Se0.3 thermoelectric material via spark plasma sintering combined with hot extrusion (SPS+HE). The parameters affacting hot extrusion process and preparation of n-type Bi2Te2.7Se0.3 materials under different process conditions were optimized, and the thermoelectric performance and mechanical properties were investigated. In addition, the machinability of the extruded Bi2Te2.7Se0.3 material was also analyzed. Methods The commercial zone-melting crystal rods were pulverized and sintered via spark plasma sintering (SPS) at 350 ℃ and 20 MPa for 5 min. The ingot was then put into a hot extrusion mold, and treated at 390–550 ℃, extrusion speed of 0.05–0.50 mm/s, extrusion ratio of 9:1, and extrusion angle of 30°. Under the determined hot extrusion parameters, n-type Bi2Te2.7Se0.3 materials were prepared by different processes, i.e., the raw materials were ground for 1 h and then sintered by SPS and subsequent hot extrusion (HE); the raw materials were melted at 700 ℃ for 5 h and then cold-pressed (MT), and sintered by subsequent hot extrusion (HE); the raw materials were melted and cold-pressed, followed by annealing and hot extrusion (MT+AN+HE); and the raw materials were ground for 1.5 h and cold-pressed, followed by hot extrusion (BM+HE). The phase structure was analyzed by X-ray diffraction (XRD, D8 Advance, Bruker Co. Ltd., USA) at room temperature. The microstructure and fracture morphology were determined by scanning electron microscopy (SEM, Supra 55, ZEISS Co., Germany). The electrical conductivity and the Seebeck coefficient were measured by ZEM-3 (ULVAC Co. Ltd., Japan). The thermal diffusivity (λ) was measured by a laser flash method (LFA457, Netzsch Co., Germany). The thermal conductivity was calculated according to κ=λρCp, where Cp was the heat capacity according to the Neumann-Kopp rule, and the density ρ was measured based on the Archimedes prinicple. Results and discussion The results show that n-type Bi2Te2.7Se0.3 thermoelectric materials can be prepared under optimum process conditions (i.e., extrusion temperature of 400 ℃ and extrusion speed of 0.05 mm/s). The XRD patterns of all the hot-extruded samples agree well with a rhombohedral structure (JCPDS 50–0954) of Bi2Te2.7Se0.3. No impurity peaks appear. The SEM images reveal that Bi, Te, and Se are homogeneously distributed in the materials without any impurity phases. The electrical conductivity σ of all the samples decreases with increasing temperature, having a metallic conduction behavior. The σ of the MT+AN+HE sample is the maximum value of 1.4×105 S/m. All the samples have negative Seebeck coefficients S, indicating that electrons are the major charge carriers. The S of the SPS+HE sample is the maximum value of 191.0 μV/K. At 300 K, the SPS+HE sample has the maximum power factor PF of 37.0 μW/(cm·K2). However, the PF of the material gradually decreases with the increase of temperature, which is consistent with the change of electrical conductivity and Seebeck coefficient due to the intrinsic excitation. The lattice thermal conductivity of MT+HE sample is the minimum value (i.e., 0.9 W·m–1·K–1). The maximum zT value reaches 0.83 at 400 K for SPS+HE sample and its Vickers hardness is 602.5 N/mm2, which is twice greater than that of the zone-melting sample. This is mainly due to the dynamic recrystallization process of grain refinement during the hot extrusion process. The machinability of the extruded Bi2Te2.7Se0.3 material are improved. The thermoelectric micron-sized particles with a minimum size of 147 μm can be achieved, providing a promising material for the development of Bi2Te3-based thermoelectric micro-devices. Conclusions The optimal hot extrusion process parameters for n-type Bi2Te2.7Se0.3 thermoelectric materials were obtained (i.e., extrusion ratio 9:1, extrusion angle 30°, extrusion temperature 400 K and extrusion speed 0.05 mm/s). A series of n-type Bi2Te2.7Se0.3 thermoelectric material samples were prepared via hot extrusion under the optimum process conditions. The Bi2Te2.7Se0.3 sample prepared by SPS and sebsequent hot extrusion (SPS+HE) had the maximum zT value 0.83 at 400 K, and its mechanical properties were improved. The Vickers hardness of the SPS+HE sample could reach 602.5 N/mm2, which was twice greater than that of the zone-melting Bi2Te2.7Se0.3 material. In addition, the machining performance was also improved, and the thermoelectric micron-sized particles with the minimum size of 147 μm could be machined for the extruded Bi2Te2.7Se0.3 sample, providing a promising material for the Bi2Te3-based thermoelectric micro-devices. © 2024 Chinese Ceramic Society. All rights reserved.
引用
收藏
页码:3243 / 3251
相关论文
共 50 条
  • [31] Effects of Ni Magnetic Nanoparticles on Thermoelectric Properties of n-Type Bi2Te2.7Se0.3 Materials
    Ma, Shifang
    Li, Cuncheng
    Xing, Lin
    Mu, Xin
    Zhu, Wanting
    Nie, Xiaolei
    Sang, Xiahan
    Wei, Ping
    Zhang, Qingjie
    Zhao, Wenyu
    JOURNAL OF ELECTRONIC MATERIALS, 2020, 49 (05) : 2881 - 2889
  • [32] Comparison of characteristics of Bi2Te3 and Bi2Te2.7Se0.3 thermoelectric materials synthesized by hydrothermal process
    Y. Saberi
    S. A. Sajjadi
    H. Mansouri
    Journal of Materials Science: Materials in Electronics, 2020, 31 : 18988 - 18995
  • [33] Enhanced thermoelectric properties of n-type Bi2Te2.7Se0.3 for power generation
    Chen, Xi
    Cai, Fanggong
    Dong, Rong
    Lei, Xiaobo
    Sui, Runqing
    Qiu, Lanxin
    Zeng, Zhili
    Sun, Wei
    Zheng, Hao
    Zhang, Qinyong
    JOURNAL OF MATERIALS SCIENCE-MATERIALS IN ELECTRONICS, 2020, 31 (06) : 4924 - 4930
  • [34] Enhancement of thermoelectric properties induced by oriented nanolayer in Bi2Te2.7Se0.3 columnar films
    Tan, Ming
    Deng, Yuan
    Hao, Yanming
    MATERIALS CHEMISTRY AND PHYSICS, 2014, 146 (1-2) : 153 - 158
  • [35] EFFECTS OF MILLING DURATION ON THE THERMOELECTRIC PROPERTIES OF N-TYPE Bi2Te2.7Se0.3
    Park, Min-Soo
    Koo, Hye-Young
    Park, Yonh-Ho
    Ha, Gook-Hyun
    ARCHIVES OF METALLURGY AND MATERIALS, 2019, 64 (02) : 591 - 595
  • [36] Enhanced thermoelectric properties of n-type Bi2Te2.7Se0.3 for power generation
    Xi Chen
    Fanggong Cai
    Rong Dong
    Xiaobo Lei
    Runqing Sui
    Lanxin Qiu
    Zhili Zeng
    Wei Sun
    Hao Zheng
    Qinyong Zhang
    Journal of Materials Science: Materials in Electronics, 2020, 31 : 4924 - 4930
  • [37] Lattice distortion and anisotropic thermoelectric properties in hot-deformed CuI-doped Bi2Te2.7Se0.3
    Kim, Jin Hee
    Cho, Hyunyong
    Back, Song Yi
    Yun, Jae Hyun
    Lee, Ho Seong
    Rhyee, Jong-Soo
    JOURNAL OF ALLOYS AND COMPOUNDS, 2020, 815
  • [38] Preparation and Thermoelectric Properties of n-Type Bi2Te2.7Se0.3:D m
    Lee, Go-Eun
    Eum, A-Young
    Song, Kwon-Min
    Kim, Il-Ho
    Lim, Young Soo
    Seo, Won-Seon
    Choi, Byeong-Jun
    Hwang, Chang-Won
    JOURNAL OF ELECTRONIC MATERIALS, 2015, 44 (06) : 1579 - 1584
  • [39] Thermoelectric Properties of Cu2Te Nanoparticle Incorporated N-Type Bi2Te2.7Se0.3
    Jung, Yong-Jae
    Kim, Hyun-Sik
    Won, Jong Ho
    Kim, Minkyung
    Kang, Minji
    Jang, Eun Young
    Nguyen Vu Binh
    Kim, Sang-il
    Moon, Kyoung-Seok
    Roh, Jong Wook
    Nam, Woo Hyun
    Koo, Sang-Mo
    Oh, Jong-Min
    Cho, Jung Young
    Shin, Weon Ho
    MATERIALS, 2022, 15 (06)
  • [40] Effect of dopant on n-type Bi2Te2.7Se0.3 thermoelectric materials fabricated by spark plasma sintering
    Cho, Dong-Choul
    Lee, Jae-Seol
    Lim, Chul-Ho
    Lee, Chi-Hwan
    HIGH-PERFORMANCE CERAMICS V, PTS 1 AND 2, 2008, 368-372 : 544 - +