Experimental study on spheroidal morphology of palladium coated copper wire with different palladium layer thickness

被引:0
|
作者
An, Bin [1 ]
Zhou, Hongliang [1 ,2 ]
Cao, Jun [1 ,2 ]
Ming, Pingmei [1 ,2 ]
Xia, Jie [1 ]
Yao, Jingguang [1 ]
Persic, John [1 ,3 ]
Zhang, Yuemin [1 ,2 ]
机构
[1] Henan Polytech Univ, Sch Mech & Power Engn, Jiaozuo 454003, Peoples R China
[2] Henan Polytech Univ, Henan Int Joint Lab Adv Elect Packaging Mat Precis, Jiaozuo 454003, Peoples R China
[3] Microbonds Inc, 7495 Birchmount Rd, Markham, ON L3R 5G2, Canada
来源
APL MATERIALS | 2024年 / 12卷 / 10期
基金
中国国家自然科学基金;
关键词
CORROSION BEHAVIOR; CU; RELIABILITY; MECHANISM; AL;
D O I
10.1063/5.0232025
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Palladium (Pd) coated copper (PCC) wire is an emerging bonding wire that has been widely researched. In this paper, the effects of electronic flame-off (EFO) current and EFO time on the free air ball (FAB) morphology of four PCC wires with Pd layer thicknesses of 60, 80, 100, and 120 nm, respectively, are first investigated. The larger the EFO current or the longer the EFO time, the larger the FAB diameter. The EFO time or EFO current setting is either too high or too low to form a FAB with good morphology. Taking the ratio of FAB diameter to wire diameter as 2 as the standard, the EFO current of 48 mA and the EFO time of 700 mu s are selected as the optimal EFO parameter combination. Under this parameter combination, the symmetry, roundness, and surface smoothness of the FAB of the four PCC wires are all at a better level. It is found that the FAB surface Pd coverage of PCC wire with 120 nm Pd layer thickness is higher through the corrosion test. The Pd transfer law on the FAB at different EFO times under optimal EFO current is also studied. The results show that with the prolongation of the EFO time, the Pd on the FAB surface is gradually transferred from the neck to the middle and lower parts. This study can provide technical reference for the selection of Pd layer thickness and EFO parameters of PCC wire. (c) 2024 Author(s).
引用
收藏
页数:13
相关论文
共 50 条
  • [31] Ultra-fine pitch palladium-coated copper wire bonding: Effect of bonding parameters
    Lim, Adeline B. Y.
    Chang, Andrew C. K.
    Yauw, Oranna
    Chylak, Bob
    Gan, Chee Lip
    Chen, Zhong
    MICROELECTRONICS RELIABILITY, 2014, 54 (11) : 2555 - 2563
  • [32] HYDROGEN PERMEATION THROUGH COPPER-COATED PALLADIUM
    ANDREW, PL
    HAASZ, AA
    JOURNAL OF APPLIED PHYSICS, 1991, 70 (07) : 3600 - 3604
  • [33] Mechanism to improve the reliability of copper wire bonding with palladium-coating of the wire
    Qin, Wentao
    Anderson, Tom
    Chang, George
    MICROELECTRONICS RELIABILITY, 2019, 99 : 239 - 244
  • [34] Nickel-palladium bond pads for copper wire bonding
    Clauberg, Horst
    Backus, Petra
    Chylak, Bob
    MICROELECTRONICS RELIABILITY, 2011, 51 (01) : 75 - 80
  • [35] Brief Review on Corrosion of Palladium Coated Copper Wire Bonds under High Temperature Storage Stress Test
    Cha, Chan Lam
    Lau, Kok-Tee
    Zaimi, Muhammad
    PROCEEDINGS OF INNOVATIVE RESEARCH AND INDUSTRIAL DIALOGUE 2018 (IRID'18), 2019, : 33 - 34
  • [36] Investigation of mechanical and microstructural properties of a new, corrosion resistant gold-palladium coated copper bond wire
    Lorenz, Georg
    Naumann, Falk
    Klengel, Robert
    Mengel, Sandy
    Petzold, Matthias
    Eto, Motoki
    Araki, Noritoshi
    Yamada, Takashi
    2019 22ND EUROPEAN MICROELECTRONICS AND PACKAGING CONFERENCE & EXHIBITION (EMPC), 2019,
  • [37] Enhancement of Mechanical Properties of Gold-Coated Silver Composite Bonding Wire with Palladium and Copper Elements Addition
    Kang F.
    Kong J.
    Chen J.
    Zhou W.
    Yang G.
    Pei H.
    Xiyou Jinshu/Chinese Journal of Rare Metals, 2019, 43 (12): : 1302 - 1308
  • [38] STUDY OF THE UNDERPOTENTIAL DEPOSITION OF COPPER ON PALLADIUM
    BAKOS, I
    SZABO, S
    NAGY, F
    MALLAT, T
    MAGYAR KEMIAI FOLYOIRAT, 1990, 96 (07): : 318 - 323
  • [39] High temperature degradation of palladium coated copper bond wires
    Krinke, J. C.
    Dragicevic, D.
    Leinert, S.
    Friess, E.
    Glueck, J.
    MICROELECTRONICS RELIABILITY, 2014, 54 (9-10) : 1995 - 1999
  • [40] Palladium Coated Copper Nanowires as a Hydrogen Oxidation Electrocatalyst in Base
    Alia, Shaun M.
    Yan, Yushan
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2015, 162 (08) : F849 - F853