Oxidation Behavior of Ta-Ti-Al-W Alloy at 1000℃

被引:0
|
作者
Li, Jiaxin [1 ,2 ]
Chen, Yuhong [1 ,2 ]
Bai, Zhangjun [4 ]
Li, Ning [1 ,3 ]
Cheng, Yuewei [4 ]
机构
[1] School of Materials Science & Engineering, North Minzu University, Yinchuan,750021, China
[2] Key Lab of Powder Material & Advanced Ceramics, School of Materials Science & Engineering, North Minzu University, Yinchuan,750021, China
[3] International Scientific & Technological Cooperation Base of Industrial Waste Recycling and Advanced Materials, Yinchuan,750021, China
[4] CNMC Ningxia Orient Group Co., Ltd, Shizuishan,753000, China
关键词
D O I
暂无
中图分类号
学科分类号
摘要
The Ta-25Ti-18Al-6.5W alloy was prepared by vacuum suspension melting method to investigate the oxidation behavior of Ta-Ti-Al-W alloy at 1000℃. The phase composition and microstructure of as-sintered and oxidized specimens were characterized by XRD, SEM, and EDS. Results show that the oxidation kinetics of the alloy follows the parabolic law at first, and then changes into the linear law. During the oxidation process, Ta can be oxidized preferentially, and the enrichment areas of TiO2 and Al2O3 are observed in the surface of oxide scale, because of the higher diffusion rates of Ti and Al. In the initial stage, the oxidation is controlled by external diffusion of alloying elements. The oxidation layer is mainly composed of the TiO2 and solid solution of Ta2O5, WO3, TiO2, Al2O3. With increasing the oxidation duration, the oxides scale which controls the oxidation process shows different layer structures: an outer layer mainly composed of TiO2 and Al2O3, a Ta2O5ss solid solution inner layer and a transition layer with less oxygen content. © 2021, Science Press. All right reserved.
引用
收藏
页码:195 / 200
相关论文
共 50 条
  • [41] Oxidation behavior of Ti-22Al-26Nb alloy at high temperatures
    Shenyang Institute of Chemical Technology, Shenyang 110142, China
    Xiyou Jinshu Cailiao Yu Gongcheng, 2009, 12 (2183-2186):
  • [42] Effect of Cr on the oxidation behavior of Ti46Al-2V alloy
    Pilone, Daniela
    Felli, Ferdinando
    TMS 2008 ANNUAL MEETING SUPPLEMENTAL PROCEEDINGS, VOL 3: GENERAL PAPER SELECTIONS, 2008, : 413 - 418
  • [43] Development and oxidation behavior of Al-Cu-Fe quasicrystalline coating on Ti alloy
    Cai, F
    Zhou, CG
    Xu, HB
    Gong, SK
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2004, 20 (06) : 713 - 715
  • [44] Oxidation behavior of Al-W alloy films deposited on Cu as a passivation layer
    Takeyama, M
    Ichikawa, T
    Noya, A
    THIN SOLID FILMS, 1996, 272 (01) : 18 - 20
  • [46] High-Temperature Oxidation Behavior of a Ni-Cr-W-Al Alloy
    Ma, Y. C.
    Zhao, X. J.
    Gao, M.
    Liu, K.
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2011, 27 (09) : 841 - 845
  • [47] Research on Oxidation Behavior of Novel Co-Al-W Alloy at High Temperature
    Xu Yangtao
    Xia Tiandong
    Yan Jianqiang
    Zhao Wenjun
    RARE METAL MATERIALS AND ENGINEERING, 2011, 40 (10) : 1742 - 1747
  • [48] Insights into the role of W/B alloying on high-temperature oxidation behavior of Ti42Al5Mn alloy
    Zhao, Pengxiang
    Ma, Hui
    Li, Xiaobing
    Gao, Ming
    Ma, Yingche
    Liu, Kui
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2024, 178 : 188 - 200
  • [49] Tribological behavior of Ti-Al-Nb alloy with different Ta additions for high temperature applications
    Guo, Runping
    Xiong, Guifang
    Liu, JunRu
    Wang, Yunsheng
    Davoodi, Danial
    Miri, Reza
    Tayebi, Morteza
    MATERIALS LETTERS, 2023, 330
  • [50] Deformation behavior and fracture mechanism of Ti-22Al-20Nb-7Ta alloy
    Zhou, Xuan
    Fu, Li
    Ge, Hualong
    Mao, Yong
    MATERIALS CHARACTERIZATION, 2022, 194