Mirror grinding process for aluminum alloy using elastic grinding wheel

被引:0
|
作者
Yuan, Wei-Jie [1 ]
Deng, Ri-Tao [1 ]
Yang, Zhen-Tao [2 ]
Yin, Shao-Hui [1 ]
机构
[1] School of Mechanical and Vehicle Engineering, Hunan University, Changsha,410082, China
[2] Hunan Changbudao Optical Technology Co., Ltd., Changsha,410202, China
来源
Surface Technology | 2018年 / 47卷 / 07期
基金
中国国家自然科学基金;
关键词
Abrasives - Aluminum alloys - Efficiency - Grinding (machining) - Grinding wheels - Particle size - Polishing - Polyurethanes;
D O I
10.16490/j.cnki.issn.1001-3660.2018.07.004
中图分类号
学科分类号
摘要
The work aims to solve the problem of low polishing efficiency in traditional polishing process for aluminum alloy mobile phone shell. Grinding process for 6061 aluminum alloy was studied by using polyurethane elastic grinding wheel. Orthogonal test was performed to study the influences of abrasive particle size, feed speed, cutting depth and grinding wheel linear speed on surface roughness and material removal rate. Turning line approach was used for processing in the test, which could reduce the influence of uneven abrasive distribution. Roughness of machined surface was measured with a white light interferometer, and removal rate was obtained by calculating mass change of the workpiece in unit time. Optimal process parameters were obtained based upon comprehensive optimization of the results. In the selected 16 grinding parameters, the minimum obtainable surface roughness Ra was 44.87 nm, and the maximum removal rate was 0.329 g/min. The most important factor affecting surface roughness was abrasive particle size, and the minimum factor was feed rate. As for the material removal rate, the most important factor was cutting depth, the least was feed rate. After comprehensive optimization, the optimal combination of process parameters was: grinding wheel as 600# speed as 2000 r/min, cutting depth as 0.04 mm, and feed rate as 20 mm/min. The application of polyurethane elastic grinding wheel to aluminum alloy grinding can improve surface quality, simplify technological process, save material preparation, installation & adjustment time, and further improve efficiency. © 2018 Chongqing Wujiu Periodicals Press. All rights reserved.
引用
收藏
页码:21 / 27
相关论文
共 50 条
  • [41] The determination of redressing timing for grinding wheel by using statistical process control
    Kang, Yuan (yk@cycu.edu.tw), 1600, National Taiwan University of Science and Technology (31):
  • [42] Mirror Grinding Process Parameter Selection and Design
    Hua, Li
    Wang, Xiangjun
    Zhou, Rui
    APPLIED MECHANICS, MATERIALS AND MANUFACTURING IV, 2014, 670-671 : 526 - 528
  • [43] GRINDING WHEEL PROFILE FOR HOB RELIEF GRINDING
    SIMON, V
    JOURNAL OF MECHANICAL DESIGN-TRANSACTIONS OF THE ASME, 1982, 104 (04): : 731 - 742
  • [44] The effect of integrating the structural modifications of the grinding wheel upon the internal cylindrical grinding process
    Nadolny, K.
    ARCHIVES OF CIVIL AND MECHANICAL ENGINEERING, 2012, 12 (01) : 60 - 67
  • [45] The influence of grinding process on forced vibration damping in headstock of grinding wheel of cylindrical grinder
    Orynski, F
    Pawlowski, W
    INTERNATIONAL JOURNAL OF MACHINE TOOLS & MANUFACTURE, 1999, 39 (02): : 229 - 235
  • [46] Influence of grinding process on forced vibration damping in headstock of grinding wheel of cylindrical grinder
    Technical Univ of Lodz, Lodz, Poland
    Int J Mach Tools Manuf, 2 (229-235):
  • [47] Deep grinding of titanium alloy with continuous wheel correction
    Nosenko V.A.
    Nosenko S.V.
    Russian Engineering Research, 2010, 30 (11) : 1124 - 1128
  • [48] Study on Grinding Mechanism of BCB Grinding Wheel
    Li, Wei
    Hong, Yang
    Jin, Liangsheng
    ADVANCED MANUFACTURING TECHNOLOGY, PTS 1-4, 2012, 472-475 : 2914 - 2917
  • [49] GRINDING MECHANISM OF SEGMENTAL GRINDING WHEEL.
    Matsui, Seiki
    Technology Reports of the Tohoku University, 1986, 51 (02): : 143 - 157
  • [50] SELECTING A WHEEL MATERIAL FOR GRINDING TITANIUM-ALLOY
    SAYUTIN, GI
    TATARINOV, AP
    SOVIET ENGINEERING RESEARCH, 1985, 5 (07): : 75 - 76