Effect of Welding Speed on Microstructure and Properties of Laser⁃Welded Joint of TA15 Titanium Alloy

被引:0
|
作者
Liu, Shichao [1 ]
Wang, Shanlin [1 ,2 ]
Zhang, Yuanmin [2 ]
Dai, Zhongkui [2 ]
Tu, Wenbin [2 ]
Chen, Yuhua [2 ]
Xiao, Xi [3 ]
机构
[1] Nanchang Regional Military Representative Office, Wuhan Regional Military Representative Bureau, Chinese People’s Liberation Army Naval Armaments Department, Jiangxi, Nanchang,330200, China
[2] Jiangxi Key Laboratory of Forming, Joining Technology for Aerospace Components, Nanchang Hangkong University, Jiangxi, Nanchang,330063, China
[3] Jiangxi Hongdu Aviation Industry Co., Ltd., Jiangxi, Nanchang,330200, China
来源
关键词
Bending moments - Corrosion fatigue - Corrosion resistance - Corrosion resistant alloys - Creep resistance - Dealloying - Decarburization - Electrolytic polishing - Ferrite - High temperature corrosion - Laser beam machining - Laser beam welding - Laser cooling - Laser safety - Passivation - Pearlite - Shearing - Strain hardening - Strain rate - Superplasticity - Tantalum metallography - Titanium metallography - Weld decay;
D O I
10.3788/CJL231413
中图分类号
学科分类号
摘要
Objective Titanium and its alloys have excellent properties, such as low density, good corrosion resistance, high-temperature performance, high specific strength and stiffness, and good fatigue and creep resistance. Therefore, titanium alloys are used in several structural parts of the aircrafts to lessen their weight and improve their service life. However, an advanced and efficient processing method for these materials has a significant impact on the widespread use of each material. Compared with other welding technologies, laser welding with a fast cooling speed, small overall deformation after welding, and easy control of the laser beam can yield high-quality welds of complex structural parts. The welding and assembly accuracies can also be improved. However, welded joints often have defects such as pores, cracks, inclusions, and incomplete penetration owing to improper selection of welding parameters, which significantly affect the service life and safety of the aircraft. The microstructure of the welded joint determines its mechanical properties, and the microstructural evolution in the welded joint is closely related to the welding process parameters. In the past, the microstructural evolution of welded joints of titanium alloys was mostly studied by traditional metallography and scanning electron microscope, and the elaborate analysis and understanding of the microstructural evolution of welded joints were limited. In this study, TA15-welded joints are prepared at different welding speeds using laserwelding technology. An electron backscatter diffractometer (EBSD) is used to analyze the microstructure characteristics in each area of the joint, and the relationship between the microstructure and mechanical properties of the joint is investigated in detail, providing a theoretical basis for the rapid application of titanium alloys in laser welding. Methods The effect of welding speed (1.25, 1.55, 1.85, 2.15, and 2.45 m/min) on the mechanical microstructure and properties of a TA15 titanium alloy laser-welded joint is studied. The microstructure of the TA15 titanium alloy laser-welded joint is analyzed using a scanning electron microscope and an EBSD probe. The samples for the EBSD tests are prepared through electrolytic polishing. The polishing voltage and current are set to 30 V and 0.65‒0.90 A, respectively, and the calibration step is 0.15 μm. The microhardness values of the joints are measured using an automatic microhardness tester. The applied load is 200 g and the loading time is 10 s. Tensile tests are conducted on the welded joints using a microcomputer-controlled electronic universal testing machine. The tensile rate is 1 mm/min. The sizes of the tensile samples are shown in Fig. 1. Results and Discussions Large β columnar crystals shown in Fig. 2 are distributed in the weld zone of TA15 titanium alloy laserwelded joints at different welding speeds. With an increase in welding speed, the widths of the weld and heat-affected zones of the TA15 titanium alloy laser-welded joint decrease. As the welding speed increases from 1.25 m/min to 2.45 m/min, as shown in Figs. 4 and 5, the grain size of the weld zone decreases from 3.09 μm to 2.66 μm, and the volume fraction of high-angle grain boundary increases from 91.6% to 95.8%. The grain size of the heat-affected zone decreases from 1.16 μm to 0.94 μm, and the volume fraction of high-angle grain boundary initially decreases from 91.1% to 89.7% and then increases to 94.2%. The β-phase volume fraction of the heat-affected zone initially decreases from 1.09% to 0.64% and then increases to 2.34% as the welding speed increases. The β -phase volume fraction in the weld zone decreases from 0.13% to 0.03% as the welding speed increases. As shown in Figs. 7 and 8, as the welding speed increases from 1.25 m/min to 2.45 m/min, the hardness and tensile strength of the welded joint initially increase and then decrease; the tensile strength initially increases from 1090.9 MPa to 1140.1 MPa and then decreases to 1093.9 MPa. The increases in the hardness and strength of the welded joint are attributed to the continuous refinement of the grain size; however, the decrease in hardness and strength caused by the increase in the welding speed is attributed to the increase in the β-phase content in the joint. With an increase in welding speed, the elongation of the welded joint decreases from 4.0% to 3.7% and then increases again to 4.0%. The tensile fracture positions of all the welded joints are located in the heat-affected zone. Conclusions An increase in welding speed results in a decrease in the welding heat input, resulting in a decrease in the grain size of the weld and heat-affected zones. The contents of large angle grain boundaries and β phase of the weld zone continuously increase and decrease, respectively, as the welding speed increases. However, the contents of the high-angle grain boundaries and β phase in the heat affected zone initially decrease and then increase as the welding speed increases. The tensile strength of the TA15-welded joints first increases and then decreases with increasing welding speed; however, the joint elongation first decreases and then increases with increasing welding speed. The tensile fracture locations of the TA15 titanium alloy laser-welded joints at different welding speeds appear in the heat affected zone. The contents of high-angle grain boundaries and β phase in the heat affected zone initially increase and then decrease, causing the joint elongation to initially decrease and then increase. © 2024 Science Press. All rights reserved.
引用
收藏
相关论文
共 50 条
  • [31] Influence of deformation parameters on microstructure and mechanical properties of TA15 titanium alloy
    Zhu Jing-Chuan
    Wang Yang
    Liu Yong
    Lai Zhong-Hong
    Zhan Jia-Jun
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2007, 17 : S490 - S494
  • [32] Influence of deformation parameters on microstructure and mechanical properties of TA15 titanium alloy
    朱景川
    王洋
    刘勇
    来忠红
    占家军
    Transactions of Nonferrous Metals Society of China, 2007, (S1) : 490 - 494
  • [33] Microstructure and Mechanical Properties of TA15 Titanium Alloy Φ8 mm Tube
    Shang Xiuli
    Tong Xuewen
    Wang Lian
    Xu Zhe
    Li Nong
    Feng Hongchao
    Cheng Xiaoli
    TI-2011: PROCEEDINGS OF THE 12TH WORLD CONFERENCE ON TITANIUM, VOL I, 2012, : 831 - 833
  • [34] Effects of microstructure on damage tolerance properties of TA15 ELI titanium alloy
    Li, Shi-Kai
    Hui, Song-Xiao
    Ye, Wen-Jun
    Yu, Yang
    Xiong, Bai-Qing
    Zhongguo Youse Jinshu Xuebao/Chinese Journal of Nonferrous Metals, 2007, 17 (07): : 1119 - 1123
  • [35] Synergistically strengthened TA15 titanium alloy by laser powder bed fusion: Microstructure and mechanical properties
    Xie, Qidong
    Zhang, Yanze
    Yang, Mengjia
    Zhang, Longbo
    Zhen, Chen
    Bingheng, Lu
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2025, 35 : 5537 - 5551
  • [36] Effects of double annealing on microstructure and mechanical properties of laser melting deposition TA15 titanium alloy
    Wang, C.
    Yi, J. Z.
    Qin, L. Y.
    Wang, W. D.
    Wang, X. M.
    Yang, G.
    MATERIALS RESEARCH EXPRESS, 2019, 6 (11):
  • [37] EFFECT OF CYCLIC HEAT TREATMENT ON MICROSTRUCTURE EVOLUTION OF TA15 TITANIUM ALLOY
    Zhang, Dan-Ya
    Nong, Zhi-Sheng
    Wang, Tian-Xing
    ARCHIVES OF METALLURGY AND MATERIALS, 2023, 68 (03) : 869 - 874
  • [38] Effect of annealing temperature on microstructure and mechanical properties of laser deposited TA15 titanium alloys
    Yang G.
    Wang W.
    Qin L.
    Ren Y.
    Li C.
    Wang W.
    1600, Science Press (43):
  • [39] Effect of β heat treatment on mechanical properties of TA15 titanium alloy
    Zhang, WF
    Cao, CX
    Li, XW
    Ma, JM
    Zhu, ZS
    RARE METAL MATERIALS AND ENGINEERING, 2004, 33 (07) : 768 - 770
  • [40] Effect of Heat Treatment on Fatigue Properties of TA15 Titanium Alloy Repaired by Laser Deposition
    Zhou, Song
    Wang, Shuofan
    An, Jinlan
    Wang, Xiangming
    Xie, Liyang
    Xing, Bendong
    Cui, Can
    ADVANCED ENGINEERING MATERIALS, 2024, 26 (05)