Rhombohedral Li1-xZr2-xSbx(PO4)3 electrolytes with improved Li+ conductivity for high-performance solid-state Li-metal battery

被引:0
|
作者
Pu, Xingrui [1 ]
Cheng, Xing [1 ]
Yan, Qiaohong [1 ]
Lin, Yueming [1 ]
Yan, Rentai [1 ]
Li, Bo [1 ]
Yang, Ruize [1 ]
Zhu, Xiaohong [1 ]
机构
[1] Sichuan Univ, Coll Mat Sci & Engn, Chengdu 610064, Sichuan, Peoples R China
关键词
NASICON; Ceramic electrolyte; Ionic conductivity; Interfacial resistance; Solid-state Li-metal battery; IONIC-CONDUCTIVITY; LIZR2(PO4)(3); TEMPERATURE; TRANSPORT; PHASE; CONDUCTORS; STABILITY; MOBILITY; GROWTH; ENERGY;
D O I
10.1016/j.est.2024.113959
中图分类号
TE [石油、天然气工业]; TK [能源与动力工程];
学科分类号
0807 ; 0820 ;
摘要
Recent studies on solid electrolytes have promoted the development of solid-state Li-metal batteries (SSLBs). The NASICON-type LiZr2(PO4)(3) (LZP) electrolyte has received less attention due to its low conductivity and the existence of several crystal forms, which have impeded the development of LZP-based materials for SSLBs. Herein, Li1-xZr2-xSbx(PO4)(3) (LZSP) ceramics were synthesized by solid-state method, and the cycle performances of symmetrical cell and Li-metal battery using LZSP electrolyte were characterized for the first time. The Sb5+ doping stabilizes the rhombohedral phase at room temperature and results in distortions in the ZrO6 octahedron and PO4 tetrahedron, which lead to variations of bond length and bond angle. The room temperature total conductivity of Li0.94Zr1.94Sb0.06(PO4)(3) (LZSP-0.06) increased to 6.53 x 10(-5) S<middle dot>cm(-1). This rise can be attributed to a reduction of the Li+ ions transport barrier originated from variations of bond length, bond angle and Raman vibrations mode. The Li/LZSP-0.06/Li symmetrical cell maintains a stable cycle duration of 670 h at a current density of 0.12 mA cm(-2). The specific capacity of Li/LZSP-0.06/LiFePO4 battery reaches 140.1 mAh g(-1) at 0.5C and the coulombic efficiency is 99.8 %. This battery maintains 80 % capacity after 105 cycles. These results provide reference significance for the research on SSLBs using LZP-based electrolytes. In general, the Li0.94Zr1.94Sb0.06(PO4)(3) ceramic appears to be a promising solid electrolyte for SSLBs.
引用
收藏
页数:12
相关论文
共 50 条
  • [21] Revealing cooperative Li-ion migration in Li1+xAlxTi2-x(PO4)3 solid state electrolytes with high Al doping
    Zhang, Bingkai
    Lin, Zhan
    Dong, Huafeng
    Wang, Lin-Wang
    Pan, Feng
    JOURNAL OF MATERIALS CHEMISTRY A, 2020, 8 (01) : 342 - 348
  • [22] Formation and Mobility of Defects in the NASICON-Type Compounds Li1 — xZr2 — xNbx(PO4)3 and Li1 + xZr2 — xScx(PO4)3
    I. A. Stenina
    E. V. Antipov
    A. I. Rebrov
    R. V. Shpanchenko
    A. B. Yaroslavtsev
    Doklady Chemistry, 2002, 382 : 46 - 49
  • [23] Preparation, characterization and conductivity studies of Li3-2xAl2-xSbx (PO4)3
    Anantharamulu, N.
    Prasad, G.
    Vithal, M.
    BULLETIN OF MATERIALS SCIENCE, 2008, 31 (02) : 133 - 138
  • [24] RECHARGEABLE SOLID-STATE BATTERY WITH LITHIUM CONDUCTIVE GLASS, LI3PO4-LI2S-SIS2
    IWAMOTO, K
    AOTANI, N
    TAKADA, K
    KONDO, S
    SOLID STATE IONICS, 1994, 70 : 658 - 661
  • [25] Li-ion conductivity of NASICON-type Li1+2xZr2-xCax(PO4)3 solid electrolyte prepared by spark plasma sintering
    Kotobuki, Masashi
    Yanagiya, Shunichi
    JOURNAL OF ALLOYS AND COMPOUNDS, 2021, 862 (862)
  • [26] HIGH IONIC-CONDUCTIVITY IN THE COMPOUNDS LI3FE2(PO4)3 AND LI3SC2(PO4)3
    GENKINA, EA
    DEMYANETS, LN
    IVANOVSHITS, AK
    MAKSIMOV, BA
    MELNIKOV, OK
    SIMONOV, VI
    JETP LETTERS, 1983, 38 (05) : 305 - 308
  • [27] Migration properties of Li+ in Li1+x AlxTi2-x(PO4)3
    Li Mei
    Zhong Shu-Ying
    Hu Jun-Ping
    Sun Bao-Zhen
    Xu Bo
    ACTA PHYSICA SINICA, 2024, 73 (13)
  • [28] IONIC-CONDUCTIVITY OF THE LITHIUM TITANIUM PHOSPHATE (LI1+XALXTI2-X(PO4)3), (LI1+XSCXTI2-X(PO4)3), (LI1+XYXTI2-X(PO4)3), (LI1+XLAXTI2-X(PO4)3 SYSTEMS
    AONO, H
    SUGIMOTO, E
    SADAOKA, Y
    IMANAKA, N
    ADACHI, GY
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1989, 136 (02) : 590 - 591
  • [29] Y-Doped LiZr2(PO4)3 in a PVDF-HFP Composite Electrolyte for Solid-State Li-Metal Batteries
    Gami, Pratiksha
    Badole, Manish
    Vasavan, Hari Narayanan
    Das, Asish Kumar
    Saxena, Samriddhi
    Kumar, Sunil
    ACS APPLIED ENGINEERING MATERIALS, 2024, 2 (05): : 1278 - 1287
  • [30] NASICON-type Li1+2xZr2-xCax(PO4)3 with high ionic conductivity at room temperature
    Xie, Hui
    Li, Yutao
    Goodenough, John B.
    RSC ADVANCES, 2011, 1 (09) : 1728 - 1731