Uniaxial compaction and sintering of ZrO2-3 mol% Y2O3 using rubber and PEG solutions as binders

被引:0
|
作者
Dvornik, M. I. [1 ]
Shichalin, O. O. [2 ,3 ]
Mikhailenko, E. A. [1 ]
Burkov, A. A. [1 ]
Nikolenko, S. V. [1 ]
Vlasova, N. M. [1 ]
Chernyakov, E. V. [1 ]
Gnidenko, A. A. [1 ]
Chigrin, P. G. [1 ]
Buravlev, I. Yu [2 ]
Konovalova, N. S. [4 ]
机构
[1] Russian Acad Sci, Khabarovsk Fed Res Ctr, Far Eastern Branch, 153 Tikhookeanskaya St, Khabarovsk 680042, Russia
[2] Far Eastern Fed Univ, 10 Ajax Bay, Vladivostok 690922, Russia
[3] Sakhalin State Univ, 33 Kommunistichesky Ave, Yuzhno Sakhalinsk 693000, Russia
[4] Russian Acad Sci, Yu A Kosygin Inst Tecton & Geophys, Far Eastern Branch, 65 Kim Y Chen Str, Khabarovsk 680000, Russia
关键词
MECHANICAL-PROPERTIES; IMPACT; CERAMICS; POROSITY; POWDERS;
D O I
10.1016/j.matchemphys.2024.129981
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In the study, investigations were conducted on the uniaxial compaction of samples made from ultrafine ZrO2-3 mol% Y2O3 powder with varying concentrations of binders. Butadiene rubber solution in petrol and aqueous solutions of polyethylene glycols (PEG-400, PEG-1500 and PEG-4000) at concentrations of 6, 12 and 18 % were employed as binders. An exponential increase in the density of all obtained compacts followed a logarithmic trend, reaching 100 % as the compaction pressure increased from 50 to 400 MPa. The density of all green bodies after binder removal, as a function of pressure and initial binder concentration, can be satisfactorily described by a single equation. According to this equation, the binder fills the pores in the green body while having a minimal impact on the volumetric concentration of the solid phase (Zirconia Oxide). The utilization of the PEG-1500 solution as a binder enabled the attainment of the maximum density, which was 4 % higher than the presented averaged trend. The phase composition of the sintered samples consisted solely of tetragonal zirconia. It was determined that increasing the sintered sample density by augmenting the compaction pressure and reducing the binder concentration led to an increase in the green body density from 96.9 to 99.6 %, hardness from 1100 to 1350 HV, fracture toughness from 4.5 to 5.9 MPa*m1/2 and strength from 123 to 960 MPa. The use of powders with a binder mass fraction of 6-12 % enabled the fabrication of cups with a diameter of 5 mm, which could not be compacted at lower binder concentrations or without a binder due to cracking.
引用
收藏
页数:10
相关论文
共 50 条
  • [1] Rapid rate sintering of nanocrystalline ZrO2-3 mol% Y2O3
    Pennsylvania State Univ, University Park, United States
    J Am Ceram Soc, 4 (906-912):
  • [2] Synthesis and sintering behavior of nanocrystalline ZrO2-3 mol% Y2O3 powders
    Srdic, Vladimir V.
    Radonjic, Ljiljana
    Key Engineering Materials, 1997, 132-136 (Pt 1): : 45 - 48
  • [3] Electric response of ZrO2-3 mol% Y2O3 nanocrystals
    Cachadiña, I
    Solier, JD
    Sánchez-Bajo, F
    Domínguez-Rodríguez, YA
    BOLETIN DE LA SOCIEDAD ESPANOLA DE CERAMICA Y VIDRIO, 1999, 38 (06): : 611 - 614
  • [4] Characterization of heterogeneous microstructure evolution in ZrO2-3 mol%Y2O3 during isothermal sintering
    Nettleship, Ian
    Chen, Tiandan
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2007, 90 (12) : 3793 - 3799
  • [5] The ceramic ZrO2-3 mol.% Y2O3 formed by sintering and its behavior at fracture
    Konstantinova, TE
    Danilenko, IA
    Gorokh, AV
    Volkova, GK
    REFRACTORIES AND INDUSTRIAL CERAMICS, 2001, 42 (3-4) : 102 - 105
  • [6] Influences of powder preparation routes on the sintering behaviour of doped ZrO2-3 mol%Y2O3
    Chiou, YH
    Lin, ST
    CERAMICS INTERNATIONAL, 1997, 23 (02) : 171 - 177
  • [7] Sintering properties of ZrO2-3 Mol % Y2O3 obtained from mixture of nano and microcrystalline powders
    Mineiro, S. L.
    Nono, M. C. A.
    Kuranaga, C.
    ADVANCED POWDER TECHNOLOGY V, 2006, 530-531 : 456 - +
  • [8] Influence of CoO and Al2O3 on the phase partitioning of ZrO2-3 mol% Y2O3
    Chiou, YH
    Lin, ST
    CERAMICS INTERNATIONAL, 1996, 22 (03) : 249 - 256
  • [9] Effect of sintering temperature on the microstructure and mechanical properties of ZrO2-3 mol%Y2O3 sol-gel films
    Diaz-Parralejo, A.
    Ortiz, A. L.
    Caruso, R.
    CERAMICS INTERNATIONAL, 2010, 36 (08) : 2281 - 2286
  • [10] Investigation on addition of ZrO2-3 mol% Y2O3 powder on sintering behavior and mechanical properties of B4C
    H. R. Baharvandi
    A. M. Hadian
    A. Abdizadeh
    N. Ehsani
    Journal of Materials Science, 2006, 41 : 5269 - 5272