Revealing the oxidation growth mechanism and crack evolution law of novel Si-HfO 2 /Yb 2 Si 2 O 7 /Yb 2 SiO 5 environmental barrier coatings during thermal cycling

被引:2
|
作者
Liu, Ruixiang [1 ,2 ]
Liang, Wenping [1 ]
Miao, Qiang [1 ]
Zhao, Hui [1 ,2 ]
Zhang, Xiaofeng [3 ]
Zhang, Meng [1 ]
Yan, Rongxue [1 ]
Ramasubramanian, Brindha [2 ]
Ramakrishna, Seeram [2 ]
机构
[1] Nanjing Univ Aeronaut & Astronaut, Coll Mat Sci & Technol, Nanjing 210016, Peoples R China
[2] Natl Univ Singapore, Dept Mech Engn, Singapore City 117575, Singapore
[3] Guangdong Acad Sci, Inst New Mat, Natl Engn Lab Modern Mat Surface Engn Technol, Guangzhou 510651, Peoples R China
来源
JOURNAL OF ADVANCED CERAMICS | 2024年 / 13卷 / 10期
基金
中国国家自然科学基金;
关键词
environmental barrier coatings (EBCs); thermal cycling; oxidation; crack propagation; defects; CMAS; PVD; MICROSTRUCTURE; RESISTANCE; DESIGN; OXYGEN; VAPOR;
D O I
10.26599/JAC.2024.9220969
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The development of Si-HfO 2 /Yb 2 Si 2 O 7 /Yb 2 SiO 5 environmental barrier coatings (EBCs) aims to improve the operational temperature and longevity of ceramic matrix composites (CMCs) in turbine environments. Nevertheless, several critical questions remain unanswered, including the oxidation mechanism of Si-HfO2 bond coating, the compatibility of its mixed thermally grown oxide (m-TGO) with adjacent layers during thermal cycling, and the evolution pattern of vertical mud- cracks that impact the overall performance in service. Using plasma spraying physical vapor deposition (PS-PVD), we fabricated these EBCs on a CMC substrate, and thermal cycling tests at 1400, 1450, and 1500 degrees C revealed that their durability reached 200 h. m-TGO growth followed a parabolic model, with the oxygen diffusion activation energy being 133.69 kJ/mol between 1400 and 1450 degrees C and 101.47 kJ/mol from 1450 to 1500 degrees C, emphasizing that the transport of molecular oxygen is key to controlling the oxidation of m-TGO in this EBC system. Although residual stresses and stored elastic strain energy build up between m-TGO and adjacent layers, especially around the cristobalite phase transition temperature, causing interlaminar crack formation in later thermal cycles, the stored elastic strain energy remains lower than that of the silicon oxide-thermally grown oxide (SiO2-TGO) formed in Si bond coating system. In addition to [110] dislocations, (001) twinning and interaction zones between twinning and dislocations were discovered for the first time, driving the bifurcation of mud cracks. Notably, controlling the mud-crack density is vital for protection of Yb2SiO5 layer, as bifurcated mud-crack tips may converge with adjacent mud-cracks.
引用
收藏
页码:1677 / 1696
页数:20
相关论文
共 50 条
  • [41] Interface evolution of Si/Mullite/Yb2SiO5 PS-PVD environmental barrier coatings under high temperature
    Zhang, Xiaofeng
    Song, Jinbing
    Deng, Ziqian
    Wang, Chao
    Niu, Shaopeng
    Liu, Guo
    Deng, Chunming
    Deng, Changguang
    Liu, Min
    Zhou, Kesong
    Lu, Jian
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2020, 40 (04) : 1478 - 1487
  • [42] Crystal structures and thermal expansion of Yb2Si2O7-Gd2Si2O7 solid solutions
    Stokes, Jamesa L.
    Harder, Bryan J.
    Wiesner, Valerie L.
    Wolfe, Douglas E.
    JOURNAL OF SOLID STATE CHEMISTRY, 2022, 312
  • [43] Constrained sintering and thermal ageing behaviour of electrophoretically deposited Yb2Si2O7 environmental barrier coating
    Yilmaz, Esma
    Paksoy, Ahmet Hilmi
    Gibson, Grant
    Xiao, Ping
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2023, 43 (14) : 6427 - 6439
  • [44] Crystal growth behavior and sintering-resistance property of nano-sized β-Yb2Si2O7 for environmental barrier coatings
    Wang, Chunjie
    Wang, Yue
    CERAMICS INTERNATIONAL, 2020, 46 (11) : 19514 - 19518
  • [45] Study of water vapor corrosion at 1300°C of Si/3Al2O3·2SiO2 +BSAS/Yb2SiO5 environmental barrier coatings
    He, Shi-Mei
    Mu, Ren-De
    Xu, Zhen-Hua
    He, Li-Min
    Huang, Guang-Hong
    Cailiao Gongcheng/Journal of Materials Engineering, 2011, (07): : 34 - 38
  • [46] Hot corrosion behaviour of Yb2Si2O7 environmental barrier coatings in molten NaVO3 salt
    Zhang, Yongqiu
    Zou, Binglin
    Chen, Xiaolong
    Cai, Xiaolong
    Wang, Ying
    Huang, Pai
    Yu, Ge
    Gu, Zhengwei
    CERAMICS INTERNATIONAL, 2021, 47 (21) : 30598 - 30609
  • [47] Density functional study of the phase stability and Raman spectra of Yb2O3, Yb2SiO5 and Yb2Si2O7 under pressure
    Ogawa, Takafumi
    Otani, Noriko
    Yokoi, Taishi
    Fisher, Craig A. J.
    Kuwabara, Akihide
    Moriwake, Hiroki
    Yoshiya, Masato
    Kitaoka, Satoshi
    Takata, Masasuke
    PHYSICAL CHEMISTRY CHEMICAL PHYSICS, 2018, 20 (24) : 16518 - 16527
  • [48] High-temperature oxidation behavior and mechanical properties of PS-PVD sprayed Yb2Si2O7 environmental barrier coatings
    Ma, Rong
    Qian, Jiachen
    Gao, Xiaolong
    Li, Weihai
    Zhou, Ziyang
    Jin, Xiaochao
    Fan, Xueling
    SURFACE & COATINGS TECHNOLOGY, 2024, 494
  • [49] Oxidation mechanism of the Si-X (X=HfO2, Yb2O3 or HfO2+Yb2O3) composite systems in air and water vapor at 1300 °C
    Huang, Panxin
    Peng, Kexue
    Han, Guifang
    Li, Jianzhang
    Xiao, Shikang
    Cao, Xinxin
    Zhang, Jingde
    JOURNAL OF ALLOYS AND COMPOUNDS, 2024, 1005
  • [50] High-temperature oxidation resistance of SiC f /SiC composites annealed and cladded with LaMgAl 11 O 19 /Yb 2 Si 2 O 7 thermal/environmental barrier coatings
    Lu, Kaiyue
    Huang, Yan
    Zhao, Kuangyi
    Chen, Tingyang
    Deng, Tengfei
    Luo, Chunxi
    Deng, Longhui
    Dong, Shujuan
    Jiang, Jianing
    Cao, Xueqiang
    CORROSION SCIENCE, 2024, 231