Microstructure and Room Temperature Deformation Behavior of Mg-9.5Li-2.56Al-2.58Zn Alloy

被引:0
|
作者
Zhang, Jinlong [1 ]
Lu, Enhao [1 ]
Zhu, Jun [1 ]
Zhang, Ying [1 ]
Jiang, Hang [1 ]
Yin, Chen [1 ]
Zhang, Qiming [1 ]
机构
[1] School of Materials Engineering, Xi'an Aeronautical University, Xi'an,710077, China
关键词
Binary alloys - Constitutive equations - Zinc alloys - Grain boundaries - Lithium alloys - Strain rate - Microstructure - Aluminum alloys - Deformation - Stress-strain curves - Magnesium alloys;
D O I
暂无
中图分类号
学科分类号
摘要
The microstructure and phase composition of Mg-9.5Li-2.56Al-2.58Zn alloy were studied. At the same time, the UTM5305 electronic universal testing machine was used to carry out the room temperature compression experiments with different strain rates and different deformations, to obtain the true stress-strain curve, and to construct the room temperature deformation constitutive equation of the alloy. The microstructure and compression properties of the alloy before and after compression were studied. The results show that Mg-9.5Li-2.56Al-2.58Zn alloy consists of five phases: α-Mg, β-Li, Al12Mg17, AlLi and MgLiAl2. β-Li is the matrix phase, α-Mg phase is strip or block, fibrous Al12Mg17 phase is in the interior of α-Mg phase, granular MgLiAl2 phase is distributed on the grain boundary, and intragranular AlLi phase is granular. After solution treatment, the number of precipitates in the alloy structure decreases obviously, and the strength of the alloy increases. According to the true stress-strain curve of Mg-9.5Li-2.56Al-2.58Zn alloy, the effect of strain rate on the flow stress was analyzed. There are peak stress and softening phenomenon after peak value in the compression of extruded and solid solution alloy at room temperature, which is conducive to room temperature forming. The constitutive equation constants n and lnA-(Q/RT) in different states were obtained by linear regression, and the constitutive equation based on Arrhenius model was constructed. With the increase of compression deformation, the microstructure of the alloy is gradually flattened and elongated, and the AlLi phase increases. © 2021, Science Press. All right reserved.
引用
收藏
页码:1359 / 1364
相关论文
共 50 条
  • [21] Effect of Al addition on the elevated temperature deformation behavior of Mg-Zn-Y alloy
    Kim, Do Hyung
    Lee, Ju Yeon
    Lim, Hyun Kyu
    Kim, Won Tae
    Kim, Do Hyang
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2008, 487 (1-2): : 481 - 487
  • [22] Microstructure and Deformation Behavior of a Mg-RE-Zn-Al Alloy Reinforced with the Network of a Mg-RE Phase
    Shin, Beom Soo
    Kwon, Jin Wook
    Bae, Dong Hyun
    METALS AND MATERIALS INTERNATIONAL, 2009, 15 (02) : 203 - 207
  • [23] Microstructure and deformation behavior of a Mg-RE-Zn-Al alloy reinforced with the network of a Mg-RE phase
    Beom Soo Shin
    Jin Wook Kwon
    Dong Hyun Bae
    Metals and Materials International, 2009, 15 : 203 - 207
  • [24] The hot deformation behavior, microstructure and texture evolution of homogenized Mg-9Li-1Zn alloy
    Yang, Yaqin
    Liu, Yunfang
    Guo, Xintao
    Yin, Caihong
    Yu, Jianmin
    Zhang, Zhimin
    Huang, Huagui
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2023, 25 : 2602 - 2618
  • [25] Deformation Behavior of Mg-Nd Alloy at Room Temperature and Cryogenic Temperature
    Chen, Hao
    Peng, Lili
    Li, Jiandong
    Zhang, Jing
    RARE METAL MATERIALS AND ENGINEERING, 2024, 53 (07) : 1944 - 1952
  • [26] Hot deformation behavior of an extruded Mg-Li-Zn-RE alloy
    Chen, Zhaoyun
    Li, Zhiqiang
    Yu, Chun
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2011, 528 (03): : 961 - 966
  • [27] Deformation mechanism transition with strain rate in Mg-3Al-1Zn alloy at room temperature
    Matsunaga, T.
    Somekawa, H.
    Hongo, H.
    Tabuchi, M.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2015, 647 : 212 - 215
  • [28] Influence of neodymium on microstructure and corrosion behavior of Mg-8Li-3Al-2Zn alloy
    Gu, M. Y.
    Wei, G. L.
    Liu, W. C.
    Wu, G. H.
    MATERIALS AND CORROSION-WERKSTOFFE UND KORROSION, 2017, 68 (04): : 436 - 443
  • [29] Effect of strain rate on deformation behaviour of a Mg-8.5Li-1Zn alloy sheet at room temperature
    Takada, H
    Kikuchi, S
    Tsukada, T
    Kubota, K
    Hatta, N
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1999, 271 (1-2): : 251 - 256
  • [30] Microstructure, Mechanical Properties and Deformation Behavior of Mg-Gd-Zn Alloy
    Li, K.
    Injeti, V. S. Y.
    Trivedi, P.
    Misra, R. D. K.
    MAGNESIUM TECHNOLOGY 2018, 2018, : 187 - 191