Effects of heating temperature and atmosphere on element distribution and microstructure in high-Mn/Al austenitic low-density steel

被引:1
|
作者
Zhang, Qi [1 ,2 ]
Chen, Guanghui [1 ,2 ,3 ]
Zhu, Yuemeng [1 ,2 ]
Xue, Zhengliang [1 ,2 ]
Xu, Guang [1 ,2 ]
机构
[1] Wuhan Univ Sci & Technol, State Key Lab Refractories & Met, Wuhan 430081, Peoples R China
[2] Wuhan Univ Sci & Technol, Key Lab Ferrous Met & Resources Utilizat, Minist Educ, Wuhan 430081, Peoples R China
[3] Zhejiang Red Eagle Grp Co Ltd, Huzhou 313000, Peoples R China
基金
中国国家自然科学基金; 中国博士后科学基金;
关键词
low-density steel; oxidation; microstructure; element distribution; compound scale; C STEELS; OXIDATION; DECARBURIZATION; BEHAVIOR; FATIGUE; ALLOY; SI;
D O I
10.1007/s12613-024-2867-y
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The elemental distribution and microstructure near the surface of high-Mn/Al austenitic low-density steel were investigated after isothermal holding at temperatures of 900-1200 degrees C in different atmospheres, including air, N2, and N2 + CO2. No ferrite was formed near the surface of the experimental steel during isothermal holding at 900 and 1000 degrees C in air, while ferrite was formed near the steel surface at holding temperatures of 1100 and 1200 degrees C. The ferrite fraction was larger at 1200 degrees C because more C and Mn diffused to the surface, exuded from the steel, and then reacted with N and O to form oxidation products. The thickness of the compound scale increased owing to the higher diffusion rate at higher temperatures. In addition, after isothermal holding at 1100 degrees C in N2, the Al content near the surface slightly decreased, while the C and Mn contents did not change. Therefore, no ferrite was formed near the surface. However, the near-surface C and Al contents decreased after holding at 1100 degrees C in the N2 + CO2 mixed atmosphere, resulting in the formation of a small amount of ferrite. The compound scale was thickest in N2, followed by the N2 + CO2 mixed atmosphere, and thinnest in air. Overall, the element loss and ferrite fraction were largest after holding in air at the same temperature. The differences in element loss and ferrite fraction between in N2 and N2 + CO2 atmospheres were small, but the compound scale formed in N2 was significantly thicker. According to these results, N2 + CO2 is the ideal heating atmosphere for the industrial production of high-Mn/Al austenitic low-density steel.
引用
收藏
页码:2670 / 2680
页数:11
相关论文
共 50 条
  • [21] Research on the high-temperature oxidation properties of high-Mn and low-Ni austenitic stainless steel containing an aluminizing layer
    Deng, Yongjie
    Qin, Feipeng
    Zhao, Yanjun
    Yu, Jinyu
    Wei, Xiangxin
    Wei, Feng
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2024, 33 : 8746 - 8757
  • [22] Effect of deformation temperature on strain localization phenomena in an austenitic Fe-30Mn-6.5Al-0.3C low-density steel
    Gutierrez-Urrutia, Ivan
    Shibata, Akinobu
    ACTA MATERIALIA, 2024, 264
  • [23] Dynamic recrystallization behavior and microstructure evolution of low-density high-strength Fe-Mn-Al-C steel
    Wan, Peng
    Kang, Tao
    Li, Feng
    Gao, Pengfei
    Zhang, Lei
    Zhao, Zhengzhi
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2021, 15 : 1059 - 1068
  • [24] Effects of Nitrogen on the Microstructure and Mechanical Properties of Fe-28Mn-10Al-0.8C Low-Density Steel
    Guo, Shuai
    Zhu, Hangyu
    Zhao, Jixuan
    Song, Mingming
    Li, Jianli
    Xue, Zhengliang
    STEEL RESEARCH INTERNATIONAL, 2022, 93 (08)
  • [25] Microstructure and Mechanical Properties of Al-Added High Mn Austenitic Steel
    Jin, Jae-Eun
    Lee, Young -Kook
    ADVANCED STEELS: THE RECENT SCENARIO IN STEEL SCIENCE AND TECHNOLOGY, 2011, : 259 - 264
  • [26] Effect of annealing temperature on the microstructure and tensile properties of Fe-10Mn-10Al-0.7C low-density steel
    Zhao, Chao
    Song, Renbo
    Zhang, Leifeng
    Yang, Fuqiang
    Kang, Tai
    MATERIALS & DESIGN, 2016, 91 : 348 - 360
  • [27] Impact toughness of Fe–Mn-Al-C austenitic low-density steel solution treated at different temperatures
    Zhiqi Xie
    Weijun Hui
    Saiyihan Bai
    Yongjian Zhang
    Xiaoli Zhao
    Journal of Materials Science, 2023, 58 : 1415 - 1435
  • [28] Impact toughness of Fe-Mn-Al-C austenitic low-density steel solution treated at different temperatures
    Xie, Zhiqi
    Hui, Weijun
    Bai, Saiyihan
    Zhang, Yongjian
    Zhao, Xiaoli
    JOURNAL OF MATERIALS SCIENCE, 2023, 58 (03) : 1415 - 1435
  • [29] Influence of prior cold rolling reduction on microstructure and mechanical properties of a reversion annealed high-Mn austenitic steel
    Behjati, P.
    Kermanpur, A.
    Karjalainen, L. P.
    Jarvenpaa, A.
    Jaskari, M.
    Baghbadorani, H. Samaei
    Najafizadeh, A.
    Hamada, A.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2016, 650 : 119 - 128
  • [30] Effect of early stage of κ-carbides precipitation on tensile properties and deformation mechanism in high Mn-Al-C austenitic low-density steel
    Ren, P.
    Chen, X. P.
    Yang, M. J.
    Liu, S. M.
    Cao, W. Q.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2022, 857