Highly Asymmetric Lamellar Structure in Blends of Polystyrene-b-Poly(acrylic acid) Block Copolymers and Poly(4-vinylpyridine) Homopolymers Facilitated by Polyelectrolyte Complexation
被引:2
|作者:
Ding, Shi-Peng
[1
]
Qian, Kun
[1
]
Ye, Ze
[1
]
Xia, Ding-Li
[1
]
Xu, Jun-Ting
[1
]
机构:
[1] Zhejiang Univ, Dept Polymer Sci & Engn, State Key Lab Biobased Transportat Fuel Technol, Hangzhou 310027, Peoples R China
基金:
中国国家自然科学基金;
关键词:
COACERVATE CORE MICELLES;
PS-B-PAA;
CORONA COMPOSITION;
PHASE-BEHAVIOR;
CRYSTALLIZATION;
MORPHOLOGY;
MIXTURES;
NANOSTRUCTURES;
STABILITY;
D O I:
10.1021/acs.macromol.4c01435
中图分类号:
O63 [高分子化学(高聚物)];
学科分类号:
070305 ;
080501 ;
081704 ;
摘要:
Highly asymmetric lamellar (A-LAM) structures, in which the thickness of one layer is several times larger than that of the other, have potential applications in block copolymer (BCP) nanolithography. In this work, A-LAM structures were constructed via blending polystyrene-b-poly(acrylic acid) (PS-b-PAA) BCPs with poly(4-vinylpyridine) (P4VP) homopolymers, in which the PAA block and P4VP homopolymers could form polyelectrolyte complexes (PECs). The A-LAM structure with the thickness ratio (l(PS):l(PAA/P4VP)) of as high as 4.95:1 was achieved when the blending ratio of functional groups (n(AA):n(4VP)) was only 1:0.1 and the volume fraction of polystyrene (PS) (f(PS)) was 0.832. The molecular weight of P4VP homopolymers has little effect on the formation of the A-LAM structure. However, when the molecular weight of PS-b-PAA BCPs is too low or too high, A-LAM structures cannot be formed at such a high f(PS). We proposed that the competition between chain stretching of PS chains and the electrostatic cross-linking within PAA/P4VP phase is the determining factor for the formation of A-LAM structures.