Cracking resistance and impact wear of thin and thick hard coatings under cyclic loading

被引:0
|
作者
Kulu, Priit [1 ]
Saarna, Mart [1 ]
Sergejev, Fjodor [1 ]
Surzenkov, Andrei [1 ]
Sivitski, Alina [2 ]
机构
[1] Dept. of Materials Engineering, Tallinn Univ. of Technology, Tallinn, 19086, Estonia
[2] Dept. of Mechatronics, Tallinn Univ. of Technology, Tallinn, 19086, Estonia
来源
Journal of ASTM International | 2012年 / 9卷 / 02期
关键词
Wear resistance - Hardness - Multilayers - Titanium nitride - Hard coatings - Aluminum compounds - Fuels - Tool steel - Adhesion - Cracks;
D O I
10.1520/JAI104108
中图分类号
学科分类号
摘要
Among wear resistant coatings and deposition techniques physical vapour deposition of hard thin coatings and high-velocity oxy-fuel spraying of thick WC-Co-based powder coating have provided good wear protection against various types of wear including impact wear. Three different substrate and coating systems-hard metal-coating, cold work tool steel-coating and nitrided steel-coating-were studied. Monoand multilayer coatings as well as duplex coatings were selected for testing. For characterization of coating systems nanohardness and microhardness as well as Rockwell adhesion test and single point indentation methods were used. Wear resistance of coatings was determined considering impact wear. The best adhesion determined by indentation was demonstrated by monolayer coating (TiN) on a hard metal substrate; the same coating system has a higher impact wear resistance. The coatings with multilayer structure (TiAlN) demonstrate better cracking resistance. Resistance to cracking as well as to impact wear depends on coating E/H ratio (at lower loads) as well as on substrate material E/H ratio (at higher loads). For characterization of resistance to plastic deformation for substrate H s3 =Es2 ratio was used. The obtained data enable a comparison of cracking and impact wear resistance of a coated system and selection of an optimal coating for metal forming tools applications. Copyright © 2012 by ASTM International.
引用
收藏
相关论文
共 50 条
  • [31] Comparative study on performance of UHTCC and RPC thick panels under hard projectile impact loading
    Xu, Shilang
    Zhou, Fei
    Li, Qinghua
    Chen, Bokun
    Jiang, Xiao
    Yin, Xing
    Wu, Ping
    CEMENT & CONCRETE COMPOSITES, 2021, 122
  • [32] Deformation-wear transition map of DLC coating under cyclic impact loading
    Bin Abdollah, Mohd Fadzli
    Yamaguchi, Yuto
    Akao, Tsuyoshi
    Inayoshi, Naruhiko
    Miyamoto, Nobuyuki
    Tokoroyama, Takayuki
    Umehara, Noritsugu
    WEAR, 2012, 274 : 435 - 441
  • [33] DYNAMIC IMPACT TESTER OF HARD THIN COATINGS
    Grossman, Jan
    Dupak, Libor
    Fort, Tomas
    Sobota, Jaroslav
    21ST INTERNATIONAL CONFERENCE ON METALLURGY AND MATERIALS (METAL 2012), 2012, : 1033 - 1036
  • [34] Simulating wear under cyclic loading by a minimization approach
    Peigney, M
    INTERNATIONAL JOURNAL OF SOLIDS AND STRUCTURES, 2004, 41 (24-25) : 6783 - 6799
  • [35] Crack propagation of a thin hard coating under cyclic loading: Irreversible cohesive zone model
    Feng, J.
    Qin, Y.
    Liskiewicz, T. W.
    Beake, B. D.
    Wang, S.
    SURFACE & COATINGS TECHNOLOGY, 2021, 426
  • [36] Hard coatings on elastomers for reduced permeability and increased wear resistance
    Cadambi, R. M.
    Ghassemieh, E.
    PLASTICS RUBBER AND COMPOSITES, 2012, 41 (4-5) : 169 - 174
  • [37] WEAR RESISTANCE OF HARD COATINGS IN POWDER INJECTION MOLDING (PIM)
    Panahi, Ali Keshavarz
    Khoshkish, Hossein
    Saraji, Mostafa Rezaee
    PROCEEDINGS OF THE ASME 10TH BIENNIAL CONFERENCE ON ENGINEERING SYSTEMS DESIGN AND ANALYSIS, 2010, VOL 1, 2010, : 485 - 488
  • [38] Ultradispersed diamond coatings enhancing wear resistance of hard alloys
    Adrianiova, TN
    Zakharov, AA
    Letunovskii, VV
    Demchenko, AN
    Sergienko, VP
    Gorshkov, AS
    Goryacheva, LV
    RUSSIAN JOURNAL OF APPLIED CHEMISTRY, 2000, 73 (03) : 384 - 386
  • [39] Interface cracking of FGM coatings under uniform thermal loading
    Yildirim, B
    Erdogan, F
    PROCEEDINGS OF THE EIGHTH JAPAN-U.S. CONFERENCE ON COMPOSITE MATERIALS, 1999, : 388 - 396
  • [40] Antiwear coatings for parts that operate under cyclic loading
    Yakovlev, M. G.
    Kurapov, P. A.
    JOURNAL OF FRICTION AND WEAR, 2014, 35 (01) : 12 - 15