Influence of Schistosity Orientation on Failure Mode and Indirect Tensile Strength of Mica Schist

被引:0
|
作者
Hudyma, Nick [1 ]
Avar, B. Burcin [2 ]
Chittoori, Bhaskar [1 ]
机构
[1] Boise State Univ, Dept Civil Engn, Boise, ID 83725 USA
[2] Tony Gee & Partners LLP, Ashford TN23 1HU, England
来源
GEOTECHNICS | 2023年 / 3卷 / 03期
关键词
indirect tension test; schistosity; failure mode; Levene's Test; t-tests; ANISOTROPY; ROCK;
D O I
10.3390/geotechnics3030050
中图分类号
P5 [地质学];
学科分类号
0709 ; 081803 ;
摘要
The indirect tension test is an important laboratory test for rock characterization. The presence of rock fabric, such as schistosity, complicates the assessment of test results. One hundred and forty-five indirect tension tests were conducted on mica schist specimens to investigate the effect of schistosity orientation on failure mode and tensile strength. Tensile strength results did not provide a clear relationship between schistosity orientation and tensile strength, so the failure patterns were investigated. A new naming scheme for failure modes was developed, incorporating fracture patterns observed in the specimen faces and edges. The Single Mode failure group specimens had only one failure pattern that appeared on both specimen faces, either axial failure (seventy-three specimens), schistosity failure (six specimens), or out-of-plane failure (seven specimens). The Mixed Mode failure group had thirty-two specimens that exhibited one failure pattern on one face and another on the other. The Hybrid Mode failure group had twenty-seven specimens with multiple failure patterns on both specimen faces. It was noted that Mixed Mode and Hybrid Mode specimens with components of axial failure had higher indirect tensile strengths than specimens without elements of axial failures. Statistical analyses of the tensile strength data using Levene's Test for equal variances and two-sample t-tests showed no statistical difference between the Mixed Mode and Hybrid Mode failure groups. However, there was a statistical difference between the tensile strengths of the Single Mode axial failure specimens and the combined Mixed Mode and Hybrid Mode failure groups. These results clearly emphasize that indirect tensile strength should be assessed using schistosity orientation and failure mode.
引用
收藏
页码:937 / 954
页数:18
相关论文
共 50 条
  • [21] Printing orientation influence on tensile strength of PA12 specimens obtained by SLS
    Jevtic, Ivana
    Golubovic, Zorana
    Mladenovic, Goran
    Berto, Filippo
    Sedmak, Aleksandar
    Milovanovic, Aleksa
    Milosevic, Milos
    JOURNAL OF MECHANICAL SCIENCE AND TECHNOLOGY, 2023, 37 (11) : 5549 - 5554
  • [22] Printing orientation influence on tensile strength of PA12 specimens obtained by SLS
    Ivana Jevtić
    Zorana Golubović
    Goran Mladenović
    Filippo Berto
    Aleksandar Sedmak
    Aleksa Milovanović
    Miloš Milošević
    Journal of Mechanical Science and Technology, 2023, 37 : 5549 - 5554
  • [23] INFLUENCE OF IMMUNE SYNOVITIS ON FAILURE MODE AND STRENGTH OF ANTERIOR CRUCIATE
    GOLDBERG, VM
    BURSTEIN, A
    DAWSON, M
    JOURNAL OF BONE AND JOINT SURGERY-AMERICAN VOLUME, 1975, A 57 (04): : 580 - 580
  • [24] Influence of yield-to-tensile strength ratio on failure assessment of corroded pipelines
    Zhu, XK
    Leis, BN
    JOURNAL OF PRESSURE VESSEL TECHNOLOGY-TRANSACTIONS OF THE ASME, 2005, 127 (04): : 436 - 442
  • [25] Influence of fiber orientation and volume fraction on tensile strength and fatigue life of CARALL hybrid composite
    Yoon, Han-Ki
    PROGRESSES IN FRACTURE AND STRENGTH OF MATERIALS AND STRUCTURES, 1-4, 2007, 353-358 : 1455 - 1458
  • [26] Influence of activation mode, fatigue, and ceramic interposition on resin cements' diametral tensile strength
    Guimaraes Paes, Paula Nunes
    de Miranda, Mauro Sayao
    Sampaio-Filho, Helio Rodrigues
    Correr-Sobrinho, Lourenco
    BRAZILIAN ORAL RESEARCH, 2019, 33
  • [27] Effect of isothermal heat treatment on crystallinity, tensile strength and failure mode of CF/PPS laminate
    Liu, Yankuan
    Zhou, Xuelin
    Wang, Zhiping
    HIGH PERFORMANCE POLYMERS, 2021, 33 (05) : 497 - 508
  • [28] Mechanism and Failure Mode of Tensile Strength Deterioration of Shikuosi Sandstone under Dry and Wet Cycling
    Chen Z.
    Lan H.
    Liu S.
    Du K.
    Diqiu Kexue - Zhongguo Dizhi Daxue Xuebao/Earth Science - Journal of China University of Geosciences, 2024, 49 (02): : 612 - 624
  • [29] Three-dimensional discrete element modelling of influence factors of indirect tensile strength of asphalt mixtures
    Peng, Yong
    Wan, Lei
    Sun, Li-Jun
    INTERNATIONAL JOURNAL OF PAVEMENT ENGINEERING, 2019, 20 (06) : 724 - 733
  • [30] A New Fatigue Failure Criterion Based on Crack Width of Asphalt Concrete Under Indirect Tensile Mode of Loading
    Manh Tuan Nguyen
    Lee, Hyun Jong
    Baek, Jongeun
    Moon, Joon-Shik
    JOURNAL OF TESTING AND EVALUATION, 2016, 44 (01) : 55 - 66