Investigation of Basicity on Compressive Strength and Oxidation Induration Mechanism of Vanadium-Titanium Magnetite Pellets

被引:0
|
作者
Zhang, Song [1 ,2 ]
Zong, Yanbing [1 ]
Huang, Yun [3 ]
Gui, Xiangyou [4 ]
Lei, Dian [3 ]
Zhang, Jianliang [1 ,5 ]
Gan, Xian [3 ]
Wang, Zhenyang [1 ]
Zhang, Shushi [1 ]
Lu, Peiyuan [1 ]
机构
[1] Univ Sci & Technol Beijing, Sch Met & Ecol Engn, Beijing 100083, Peoples R China
[2] Bijie Big Data Ind Dev Ctr, Bijie 551700, Guizhou, Peoples R China
[3] Pangang Grp Xichang Steel&Vanadium Co Ltd, Xichang 615032, Sichuan, Peoples R China
[4] Bijie Vocat & Tech Coll, Bijie 551700, Guizhou, Peoples R China
[5] Univ Queensland, Sch Chem Engn, St Lucia, Qld 4072, Australia
基金
中国国家自然科学基金;
关键词
iron and steel industries; oxidation induration; pellets; vanadium-titanium magnetites; HIGH-CHROMIUM VANADIUM; CONSOLIDATION MECHANISM; BEHAVIORS;
D O I
10.1002/srin.202400461
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
Currently, the typical charge structure for blast furnace smelting of vanadium-titanium magnetite (VTM) is the addition of acidic pellets, high-basicity sinters, and lumps. To increase the percentage of pellets entering the blast furnace, it is necessary to transfer the basicity burden to the pellets. In this study, the effect of basicity on the phase transition and oxidation hardening mechanism of VTM pellets is investigated. In the results, it is indicated that when the preheating temperature is 950 degrees C, the preheating time is 15 min, the roasting temperature is 1260 degrees C, and the roasting time is 15 min, with the basicity (CaO/SiO2) increasing from 0.08 to 1.3, the compressive strength of pellets shows a trend of "increasing first and then decreasing," with the highest value reaching 3159 N pellet-1 at basicity of 0.5. As the basicity increases, calcium ferrate can be generated by CaO in the liquid phase with Fe2O3 in addition to silicate with SiO2, which will increase the amount of the liquid phase. With the increase of basicity, the oxide-bonded induration is gradually weakened, and the slag-bonded induration is gradually enhanced. A moderate amount of liquid phase can play the role of bonding and filling, thereby improving compressive strength. With the increase of basicity, the content of recrystallized hematite decreases, and the oxide-bonded induration is gradually weakened; while with the larger amount of CaO added, it will generate low-melting-point silicate and calcium ferrate with SiO2 and Fe2O3 and transform into the liquid phase at high temperature, and the slag-bonded induration is gradually enhanced.image (c) 2024 WILEY-VCH GmbH
引用
收藏
页数:11
相关论文
共 50 条
  • [1] Phase Evolution Behavior and Oxidation Induration Mechanism of High-Chromium Vanadium-Titanium Magnetite Flux Pellets
    Chen, Bojian
    Wen, Jing
    Jiang, Tao
    Li, Lin
    Yang, Guangdong
    Zhao, Tao
    METALLURGICAL AND MATERIALS TRANSACTIONS B-PROCESS METALLURGY AND MATERIALS PROCESSING SCIENCE, 2022, 53 (01): : 178 - 189
  • [2] Preparation, Sintering Behavior and Consolidation Mechanism of Vanadium-Titanium Magnetite Pellets
    Chen, Weibin
    Dong, Zhaoqi
    Jiao, Yang
    Liu, Lili
    Wang, Xidong
    CRYSTALS, 2021, 11 (02): : 1 - 11
  • [3] Oxidation induration process and kinetics of Hongge vanadium titanium-bearing magnetite pellets
    Li, W.
    Fu, G. -Q.
    Chu, M. -S.
    Zhu, M. -Y.
    IRONMAKING & STEELMAKING, 2017, 44 (04) : 294 - 303
  • [4] Phase Evolution Behavior and Oxidation Induration Mechanism of High-Chromium Vanadium–Titanium Magnetite Flux Pellets
    Bojian Chen
    Jing Wen
    Tao Jiang
    Lin Li
    Guangdong Yang
    Tao Zhao
    Metallurgical and Materials Transactions B, 2022, 53 : 178 - 189
  • [5] Softening-melting Properties of High-chromium Vanadium-titanium Magnetite Pellets with Different Basicity
    Chen, Bojian
    Wen, Jing
    Jiang, Tao
    Li, Lin
    Yu, Tangxia
    Tang, Wenbo
    Hu, Peng
    ISIJ INTERNATIONAL, 2023, 63 (10) : 1607 - 1618
  • [6] Effect of diboron trioxide on the crushing strength and smelting mechanism of high-chromium vanadium-titanium magnetite pellets
    Cheng, Gong-jin
    Gao, Zi-xian
    Yang, He
    Xue, Xiang-xin
    INTERNATIONAL JOURNAL OF MINERALS METALLURGY AND MATERIALS, 2017, 24 (11) : 1228 - 1240
  • [7] ROASTING CHARACTERISTICS OF OXIDIZED PELLETS OF VANADIUM-TITANIUM MAGNETITE CONCENTRATES
    Chen, Xuling
    Huang, Yunsong
    Gan, Min
    Fan, Xiaohui
    Yuan, Lishun
    Lv, Wei
    5TH INTERNATIONAL SYMPOSIUM ON HIGH-TEMPERATURE METALLURGICAL PROCESSING, 2014, : 279 - 286
  • [8] Preparation of oxidized pellets with high chromium vanadium-titanium magnetite
    Tang, Jue
    Zhang, Yong
    Chu, Man-Sheng
    Xue, Xiang-Xin
    Dongbei Daxue Xuebao/Journal of Northeastern University, 2013, 34 (04): : 545 - 550
  • [9] Carbothermic Reduction Mechanism of Vanadium-titanium Magnetite
    Shuang-yin CHEN
    Xiao-jiao FU
    Man-sheng CHU
    Xi-zhe LI
    Zheng-gen LIU
    Jue TANG
    Journal of Iron and Steel Research(International), 2016, 23 (05) : 409 - 414
  • [10] Carbothermic Reduction Mechanism of Vanadium-titanium Magnetite
    Chen, Shuang-yin
    Fu, Xiao-jiao
    Chu, Man-sheng
    Li, Xi-zhe
    Liu, Zheng-gen
    Tang, Jue
    JOURNAL OF IRON AND STEEL RESEARCH INTERNATIONAL, 2016, 23 (05) : 409 - 414