Effect of Boron Concentration in the Fe-Cr-Mo-(B,C) Hardfacing Alloys on the Microstructure and Mechanical Properties

被引:0
|
作者
Gol, Yusuf [1 ]
Kilinc, Bulent [2 ]
机构
[1] Sakarya Univ Appl Sci, Grad Educ Inst, Dept Mfg Engn, TR-54187 Serdivan, Sakarya, Turkiye
[2] Sakarya Univ Appl Sci, Vocat Sch Arifiye, Machine & Met Program, TR-54580 Arifiye, Sakarya, Turkiye
关键词
hardfacing; hardness; microstructure; Mo2FeB2; wear; WEAR-RESISTANCE; BEHAVIOR; EVOLUTION; MOLYBDENUM; TOUGHNESS; STEEL;
D O I
10.1007/s11665-024-10123-3
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
This study presents the production of Fe-Cr-Mo-(B,C)-based hardfacing coatings containing a Mo2FeB2 phase on low-carbon DIN St37 steel using a gas tungsten arc (GTA) welding process. The effects of the B content on the phase distribution, microstructure, microhardness and wear rate of the coatings were systematically studied. An x-ray analysis showed that the coating microstructures consisted of Mo2FeB2, alpha-(Fe-Cr), M6C, M-2,M-3(B,C), M-23(C,B)(6), martensite and M-7(C,B)(3) (M=Fe,Cr,Mo) phases. Microstructural examination revealed a hypoeutectic microstructure in the boron-free and 10% boron-containing coatings. For the coatings with 20 and 30% boron contents, the microstructure completely changed and became hypereutectic. The hardness values of the coatings significantly increased with increasing boron content. The measured row hardness values of the coating layers were 754.67 +/- 28.80-1811 +/- 25 HV0.3. The measured macrohardness values from the surface were 834.53 +/- 22.84-1215.72 +/- 51.13 HV1. Increasing the amount of added boron decreased the wear rate of the coatings. The S3 (Fe7Cr3Mo3B6C) sample had the best wear performance among the produced coating layers and the highest boron content for all wear loads.
引用
收藏
页数:12
相关论文
共 50 条
  • [31] Improvement of Mechanical Properties of Fe-Cr-Mo-[Cu-Ni]-C Sintered Sintered Steels by Sinter Hardening
    Dudrova, Eva
    Grande, Marco Actis
    Rosso, Mario
    Kabatova, Margita
    Bidulsky, Robert
    Hryha, Eduard
    RESEARCHES IN POWDER METALLURGY, 2011, 672 : 31 - +
  • [32] Effect of heat input on ultrahard Fe-Cr-B-C-W-Mo-Nb hardfacing
    Gramajo, J.
    Gualco, A.
    Svoboda, H.
    PROCEEDINGS OF THE INSTITUTION OF MECHANICAL ENGINEERS PART J-JOURNAL OF ENGINEERING TRIBOLOGY, 2024,
  • [33] Effects of High Carbon Ferrochrome Additions on the Microstructure and Properties of Fe-C-Cr-Nb Hardfacing Alloys
    Huang, Fei
    Li, Renwei
    Ren, Zhen'an
    Liu, Wumu
    MATERIALS SCIENCE-MEDZIAGOTYRA, 2021, 27 (02): : 161 - 166
  • [34] EFFECT OF IRON ADDITIONS ON MICROSTRUCTURE AND MECHANICAL-PROPERTIES OF NI-CR-MO-SI HARDFACING ALLOY
    MASON, SE
    RAWLINGS, RD
    MATERIALS SCIENCE AND TECHNOLOGY, 1994, 10 (10) : 924 - 928
  • [35] Microstructures and wear resistance of Fe-Cr-B-C hardfacing alloys
    Wang, Zhi-Hui
    Wan, Guo-Li
    He, Ding-Yong
    Jiang, Jian-Min
    Cui, Li
    Cailiao Gongcheng/Journal of Materials Engineering, 2014, (09): : 57 - 62
  • [36] Characterization of Fe–C–Cr Based Hardfacing Alloys
    Vineet Shibe
    Vikas Chawla
    Transactions of the Indian Institute of Metals, 2018, 71 : 2211 - 2220
  • [37] Dilution effects on microstructure and wear resistance of a Fe-C-Cr-Mo hardfacing alloy
    Effetti della diluizione sulla microstruttura e comportamento ad usura di una lega Fe-C-B-Cr-Mo
    2015, Associazione Italiana di Metallurgia (107):
  • [38] Effect of Cu on microstructure, crystallography and mechanical properties in Fe-B-C-Cu alloys
    Yi, Yanliang
    Xing, Jiandong
    Wan, Mingjia
    Yu, Langlang
    Lu, Yafang
    Jian, Yongxin
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2017, 708 : 274 - 284
  • [39] The Influence of Boron and Carbon Addition on the Glass Formation and Mechanical Properties of High Entropy (Fe, Co, Ni, Cr, Mo)-(B, C) Glassy Alloys
    Kong, Fanli
    Inoue, Akihisa
    Wang, Fang
    Chang, Chuntao
    COATINGS, 2024, 14 (01)
  • [40] Effects of boron on microstructures and wear resistance of Fe-Cr-C system hardfacing alloys
    Zhang, Yanchao
    Cui, Li
    He, Dingyong
    Zhou, Zheng
    Hanjie Xuebao/Transactions of the China Welding Institution, 2014, 35 (03): : 89 - 92