Features of the use of tool electrodes manufactured by additive technologies in electrical discharge machining of products

被引:0
|
作者
Ablyaz, Timur [1 ]
Blokhin, Vladimir [1 ]
Shlykov, Evgeniy [1 ]
Muratov, Karim [1 ]
Osinnikov, Ilya [1 ]
机构
[1] Perm Natl Res Polytech Univ, 29 Komsomolsky Prospekt, Perm 614990, Russia
来源
OBRABOTKA METALLOV-METAL WORKING AND MATERIAL SCIENCE | 2024年 / 26卷 / 03期
基金
俄罗斯科学基金会;
关键词
Additive technologies; Selective laser melting; Copy-piercing electrical discharge; machining; Current; Voltage; Pulse on time; Surface roughness; Tool electrode wear; EDM ELECTRODES; LASER; DEFECT;
D O I
10.17212/1994-6309-2024-26.3-135-148
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
Introduction. The paper presents the results of a study of the application of a tool electrode (TE) manufactured by selective laser melting from MS1 maraging steel powder for copy-piercing electrical discharge machining (KPEDM). The purpose of the work: an experimental study of the features of using additively manufactured TEs in KPEDM of critical products. Research methods. The samples were manufactured using a ReaLizer SLM 50 installation. Spherical MS1 powder with an average particle size of 30 mu m was used as the starting material. To test the modes and select the TE sample with the least amount of surface defects, four manufacturing modes were tested, and the best sample was selected for further study. KPEDM was carried out on EMT Smart CNC equipment in a transformer oil environment. The samples were mounted in a clamp with direct polarity and used as TEs, while a 12X18N10T plate served as an electrode-part. The study was conducted using a factorial experiment (type 2 (3) ) with the center of the plan. The input data of the factorial experiment were current I , A, voltage U , W, pulse on time T (on) , mu s. The output parameters were the roughness parameter by Ra and gamma - wear of the EI. The roughness parameter by Ra was measured using the Mahr Perthometer S2 installation. Results and discussion. The SLS method was used to produce EI samples from MS1 powder; the highest quality sample No. 4 was selected for the KPEEM. Empirical equations were obtained that describe the relationship between the surface quality parameter - roughness by Ra and gamma - wear of the EI made of maraging steel MS1, depending on the KPEEM modes. In the minimum mode, with a current of I = 4 A and a voltage of U = 50 V, the wear of the EI is gamma = 0.0063875 g. The maximum wear of the EI is gamma = 0.13938 g with a current of I = 8 A and a voltage of U = 50 V. It was found that with a constant pulse on time of T (on) = 75 mu s, the lowest roughness Ra = 2.83 mu m was obtained with a current of I = 4 A and a voltage of U = 100 V, and the maximum roughness was Ra = 4.1568 mu m with I = 8 A and U = 100 V.
引用
收藏
页数:10
相关论文
共 50 条
  • [41] A laser ultrasonic technique for studying the properties of products manufactured by additive technologies
    A. A. Popovich
    D. V. Masaylo
    V. Sh. Sufiiarov
    E. V. Borisov
    I. A. Polozov
    V. A. Bychenok
    I. Yu. Kinzhagulov
    I. V. Berkutov
    D. S. Ashikhin
    A. V. Il’inskii
    Russian Journal of Nondestructive Testing, 2016, 52 : 303 - 309
  • [42] A laser ultrasonic technique for studying the properties of products manufactured by additive technologies
    Popovich, A. A.
    Masaylo, D. V.
    Sufiiarov, V. Sh
    Borisov, E. V.
    Polozov, I. A.
    Bychenok, V. A.
    Kinzhagulov, I. Yu.
    Berkutov, I. V.
    Ashikhin, D. S.
    Il'inskii, A. V.
    RUSSIAN JOURNAL OF NONDESTRUCTIVE TESTING, 2016, 52 (06) : 303 - 309
  • [43] Investigation of machining parameters of super hardened tool in micro electrical discharge machining
    Raja, D. Elil
    Gnanasekaran, K.
    Ramesh, K.
    Singh, S. Prathap
    Jagadeesh, S.
    MATERIALS TODAY-PROCEEDINGS, 2021, 47 : 6965 - 6970
  • [44] The influence of tool quality on the machining of additive manufactured and powder metallurgy titanium alloys
    Ma, Junhui
    Tran, Tanny
    Gali, Olufisayo A.
    Riahi, Reza A.
    PROCEEDINGS OF THE INSTITUTION OF MECHANICAL ENGINEERS PART B-JOURNAL OF ENGINEERING MANUFACTURE, 2022, 236 (13) : 1716 - 1725
  • [45] Manufacturing of tool electrodes with optimized configuration for copy-piercing electrical discharge machining by rapid prototyping method
    Ablyaz, Timur
    Blokhin, Vladimir
    Shlykov, Evgeniy
    Muratov, Karim
    Osinnikov, Ilya
    OBRABOTKA METALLOV-METAL WORKING AND MATERIAL SCIENCE, 2024, 26 (04):
  • [46] Study on the Movement Rule of Discharge Products in Large Area Titanium Alloy Machining by Electrical Discharge Machining
    Li D.
    Liu Z.
    Wang Y.
    Hong J.
    Lu B.
    Liu, Zhigang (mezgliu@xjtu.edu.cn), 1600, Chinese Mechanical Engineering Society (53): : 200 - 208
  • [47] On surface integrity of miniature spur gears manufactured by wire electrical discharge machining
    Jain, N.K. (nkjain@iiti.ac.in), 1735, Springer London (72): : 9 - 12
  • [48] On surface integrity of miniature spur gears manufactured by wire electrical discharge machining
    Kapil Gupta
    Neelesh Kumar Jain
    The International Journal of Advanced Manufacturing Technology, 2014, 72 : 1735 - 1745
  • [49] On surface integrity of miniature spur gears manufactured by wire electrical discharge machining
    Gupta, Kapil
    Jain, Neelesh Kumar
    INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2014, 72 (9-12): : 1735 - 1745
  • [50] Neutron resonance spin flippers: Static coils manufactured by electrical discharge machining
    Martin, N.
    Wagner, J. N.
    Dogu, M.
    Fuchs, C.
    Kredler, L.
    Boeni, P.
    Haeussler, W.
    REVIEW OF SCIENTIFIC INSTRUMENTS, 2014, 85 (07):