Alumina-based ceramic coatings obtained by the SHS process for high temperature corrosion and wear protection of steel tubulars

被引:0
|
作者
Medvedovski, Eugene [1 ]
Mendoza, Gerardo Leal [2 ]
机构
[1] Endurance Technol Inc, 39-C Stonehaven Dr, Ottawa, ON K2M 1E3, Canada
[2] Endurance Technol Inc, 71-4511 Glenmore Dr, Calgary, AB T2C 2R9, Canada
关键词
Coatings; Alumina ceramics; Corrosion; Wear; SHS; LINED COMPOSITE PIPES; MECHANICAL-PROPERTIES; CENTRIFUGAL-SHS; COMBUSTION SYNTHESIS; MOLTEN-SALT; MICROSTRUCTURE; OXIDATION; GLASS; RESISTANCE; BEHAVIOR;
D O I
10.1016/j.ceramint.2024.07.055
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Ceramic coatings have much potential for steel tubulars' protection against high temperature corrosion of gases and liquids, often containing abrasive solid particles, and to enhance their integrity in severe power generation, mineral and oil & gas production environments. Combining self-propagating high-temperature synthesis (SHS) with high-speed centrifugal process, alumina-based coatings were produced onto the inner surface of tubulars for these applications. According to the developed SHS batch formulation and the designed centrifugal device and process, well-consolidated composite ceramic layers with a thickness of 1.5-3 mm have been obtained. The developed SHS process does not create hazardous gases, and it takes similar to 30 s for the ceramic phase formation. A high-level compaction due to centrifugal forces and a liquid phase sintering approach provided a dense gradient ceramic structure formed by oxide grains cemented by a glassy phase and bonded with a steel substrate through a thin iron layer. The coatings were successfully produced onto the inner surface of carbon and stainless steels' tubes of up to 12 ft-lengths and standard dimensions from 2 to 3/8 '' to 7.5" OD. The coatings were tested, for the first time, in wear and high-temperature corrosive environments, e.g., in steam-H2S-CO2 gases and molten salts, with encouraging results due to high contents of Al2O3 and some other oxides and consolidated ceramic structure. They can be recommended for applications in high-temperature (900 degrees C and greater) corrosive environments and erosive flows.
引用
收藏
页码:36666 / 36690
页数:25
相关论文
共 50 条
  • [31] Chlorine-induced high temperature corrosion of HVAF-sprayed Ni-based alumina and chromia forming coatings
    Sadeghimeresht, Esmaeil
    Reddy, Liam
    Hussain, Tanvir
    Markocsan, Nicolaie
    Joshi, Shrikant
    CORROSION SCIENCE, 2018, 132 : 170 - 184
  • [32] Achieving high anti-wear and corrosion protection performance of phenoxy-resin coatings based on reinforcing with functional graphene oxide
    Wu, Daiqiong
    Su, Qiong
    Chen, Lei
    Cui, Haixia
    Zhao, Zhicheng
    Wu, Yanping
    Zhou, Huidi
    Chen, Jianmin
    APPLIED SURFACE SCIENCE, 2022, 601
  • [33] A Review on the Wear, Corrosion and High-Temperature Resistant Properties of Wire Arc-Sprayed Fe-Based Coatings
    Ndumia, Joseph Ndiithi
    Kang, Min
    Gbenontin, Bertrand Vigninou
    Lin, Jinran
    Nyambura, Samuel Mbugua
    NANOMATERIALS, 2021, 11 (10)
  • [34] Development of oxide-based High temperature environmental barrier coatings for ceramic matrix composites via the slurry process
    Lee, Kang N.
    Waters, Deborah L.
    Puleo, Bernadette J.
    Garg, Anita
    Jennings, Wayne D.
    Costa, Gustavo
    Sacksteder, Dagny E.
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2021, 41 (02) : 1639 - 1653
  • [35] High Velocity Oxy-Fuel Thermally Sprayed rGO Reinforced Alumina-Based Coatings on 17-4 PH Steel: Exploring the Effect of Flame Heat Treatment
    Pattnayak, Abhijit
    Kumar, Deepak
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2024, 34 (6) : 5402 - 5415
  • [36] Protection of carbon steel against molten aluminum attack and high temperature corrosion using high velocity oxygen-fuel WC-Co coatings
    Lopez, A. J.
    Rams, J.
    SURFACE & COATINGS TECHNOLOGY, 2015, 262 : 123 - 133
  • [37] Graphene modified phosphate-based metal/ceramic composite coating for corrosion protection in the high-temperature marine environment
    Chen, Zhiyu
    Xu, Xiaomei
    Liu, Hongyi
    Han, Fei
    Liu, Shuan
    CERAMICS INTERNATIONAL, 2022, 48 (18) : 25858 - 25871
  • [38] Glass-alumina composite coatings for high temperature corrosion protection. Part I: Effect of crystallization and interfacial reaction on the thermo-physical properties
    Chen, Minghui
    Shen, Mingli
    Zhu, Shenglong
    Wang, Fuhui
    Niu, Yan
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2011, 528 (7-8): : 3186 - 3192
  • [39] High temperature wear and corrosion resistance of Co-free Ni-based alloy coatings on nuclear valve sealing surfaces
    Liu, Xiu-Bo
    Fu, Ge-Yan
    Liu, Shuang
    Shi, Shi-Hong
    He, Xiang-Ming
    Wang, Ming-Di
    NUCLEAR ENGINEERING AND DESIGN, 2011, 241 (12) : 4924 - 4928
  • [40] Investigation of HVOF-sprayed WC- and NiCr-based coatings to improve corrosion and wear performance of high-strength steel
    Herman Jacobus Cornelis Voorwald
    Luiz Fábio dos Santos Vieira
    Verônica Mara de Oliveira Velloso
    Martin Ferreira Fernandes
    Maria Odila Hilário Cioffi
    Journal of the Brazilian Society of Mechanical Sciences and Engineering, 2022, 44