Enhanced interfacial and cycle stability of 4.6 V LiCoO2 cathode achieved by surface modification of KAlF4

被引:0
|
作者
Meng, Zihao [1 ]
Wang, Hao [1 ]
Wang, Yujie [1 ]
Zhang, Huanhuan [1 ]
Xiang, Qing [1 ]
Zheng, Yilong [1 ]
Yuan, Huibo [1 ]
Huang, Jintao [1 ]
Fan, Tianju [1 ,2 ]
Min, Yonggang [1 ,3 ]
机构
[1] Guangdong Univ Technol, Sch Mat & Energy, Guangzhou 510006, Peoples R China
[2] BYD Automobile Ind Co Ltd, Automot Engn Res Inst, Shenzhen 518000, Peoples R China
[3] Guangzhou Liangyue Mat Technol Co Ltd, Guangzhou 510663, Peoples R China
关键词
Lithium cobalt oxides; High voltage cathodes; Surface modification; Passivation layer; Cycle stability; CATHODE; ELECTRODE; DEGRADATION; PERFORMANCE; MECHANISMS; PARTICLE; STATE; OXIDE;
D O I
10.1016/j.jallcom.2024.176087
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Lithium cobalt oxide is one of the most popular cathode materials for lithium-ion batteries. Due to its relatively low capacity, increasing the output voltage is often necessary to release more capacity. However, subjecting cathode materials to high charging potentials inevitably induces surface-side reactions, compromising the integrity of the crystal structure and accelerating capacity degradation. Therefore, the stability of cathode materials at high voltage becomes crucial for lithium-ion batteries. In this study, we employed the ternary compound KAlF4 4 (KAF) as a surface modification coating for LiCoO2 2 (LCO). With the optimized ratio (1 wt%) of KAF, coated LCO cathodes exhibited enhanced capacity retention, excellent cycling, and rate stability. In the high voltage range of 3.0-4.6 V, the specific capacity of the initial discharge at a rate of 0.5 C reached 198.30 mA h g- 1 . Remarkably, the coated LCO retained 91.56 % of its initial capacity after 200 cycles at 0.5 C. Even at a high rate of 5 C, the coated sample retained a discharge capacity of 120.87 mA h g- 1 , significantly higher than that of bare LCO (80.24 mA h g-- 1 ). After a thorough investigation into the structure changes before and after cycling, we elucidated the mechanism of KAF coating in improving the stability of high-voltage LCO cathodes. The results indicated that KAF forms a stable passivation layer on the surface of LCO, which suppresses cracking and corrosion during charging and discharging, eventually stabilizes the crystal structure, and enhances the cycling stability of LCO.
引用
收藏
页数:11
相关论文
共 50 条
  • [21] Phosphate-Rich Interface for a Highly Stable and Safe 4.6 V LiCoO2 Cathode
    Yang, Chao
    Liao, Xiaobin
    Zhou, Xing
    Sun, Congli
    Qu, Rui
    Han, Jin
    Zhao, Yan
    Wang, Liguang
    You, Ya
    Lu, Jun
    ADVANCED MATERIALS, 2023, 35 (14)
  • [22] Tailoring Electrolyte Dehydrogenation with Trace Additives: Stabilizing the LiCoO2 Cathode beyond 4.6 V
    Yan, Yawen
    Weng, Suting
    Fu, Ang
    Zhang, Haitang
    Chen, Jianken
    Zheng, Qizheng
    Zhang, Baodan
    Zhou, Shiyuan
    Yan, Hao
    Wang, Chuan-Wei
    Tang, Yonglin
    Luo, Haiyan
    Mao, Bing-Wei
    Zheng, Jianming
    Wang, Xuefeng
    Qiao, Yu
    Yang, Yong
    Sun, Shi-Gang
    ACS ENERGY LETTERS, 2022, 7 (08) : 2677 - 2684
  • [23] A surface modification layer with cobalt aluminate inhibits 4.6 V high-voltage phase transition of LiCoO2
    Li, Zhi-Wei
    Jiang, Yun-Shan
    Xia, Yang
    Deng, Liang
    Sun, Mei-Yan
    Shao, Guang-Jie
    Zhao, Lei
    Yu, Fu-Da
    Wang, Zhen-Bo
    ELECTROCHIMICA ACTA, 2022, 428
  • [24] Stabilizing the Anionic Redox in 4.6 V LiCoO2 Cathode through Adjusting Oxygen Magnetic Moment
    Kong, Weijin
    Wong, Deniz
    An, Ke
    Zhang, Jicheng
    Chen, Zhenhua
    Schulz, Christian
    Xu, Zijian
    Liu, Xiangfeng
    ADVANCED FUNCTIONAL MATERIALS, 2022, 32 (31)
  • [25] Enhanced electrochemical and thermal stability of surface-modified LiCoO2 cathode by CeO2 coating
    Ha, HW
    Yun, NJ
    Kim, MH
    Woo, MH
    Kim, K
    ELECTROCHIMICA ACTA, 2006, 51 (16) : 3297 - 3302
  • [26] Eliminate voltage decay of LiCoO2 at 4.6 V through a combined bulk and surface reconfiguration
    Xue, Xu
    Zhao, Yaru
    Wang, Zhi
    Zhang, Yufei
    Li, Chenchen
    ELECTROCHIMICA ACTA, 2025, 512
  • [27] Tuning surface chemistry to reduce the step-like degradation of LiCoO2 at 4.6 V
    Wang, Xiaohu
    Ren, Hengyu
    Du, Yuhao
    Li, Zijian
    Zhao, Wenguang
    Ji, Haocheng
    Yi, Haocong
    Pan, Qingrui
    Liu, Jiajie
    Lou, Zirui
    Zhou, Lin
    Pan, Feng
    Zhao, Qinghe
    NANO ENERGY, 2024, 125
  • [28] Lattice-Engineering modulated band structure facilitates enhanced stability of high-voltage LiCoO2 at 4.6 V
    Zhang, Zhi
    Wu, Guang-Xin
    Tan, Zhou-Liang
    Chen, He-Zhang
    Yu, Zhen
    Yu, Zhen-Rong
    Huang, Xiao-Bing
    Yang, Wen-Jie
    Huang, Ying-De
    Chemical Engineering Journal, 2024, 502
  • [29] Surface engineering of LiCoO2 by a multifunctional nanoshell for stable 4.6V electrochemical performance
    Zhang, Si-Dong
    Qi, Mu-Yao
    Guo, Sijie
    Sun, Yong-Gang
    Wu, Ting-Ting
    Zhang, Hong-Shen
    Lu, Si-Qi
    Meng, Fanqi
    Zhang, Qinghua
    Gu, Lin
    Zhao, Zhiwei
    Peng, Zhangquan
    Jin, Hongchang
    Ji, Hengxing
    Lu, Ying-Rui
    Chan, Ting-Shan
    Duan, Ran
    Cao, An-Min
    ENERGY STORAGE MATERIALS, 2023, 57 : 289 - 298
  • [30] Lattice-Engineering modulated band structure facilitates enhanced stability of high-voltage LiCoO2 at 4.6 V
    Zhang, Zhi
    Wu, Guang-Xin
    Tan, Zhou-Liang
    Chen, He-Zhang
    Yu, Zhen
    Yu, Zhen-Rong
    Huang, Xiao-Bing
    Yang, Wen-Jie
    Huang, Ying-De
    CHEMICAL ENGINEERING JOURNAL, 2024, 502