摘要
In this research, the reduction of iron ore sinter in a blast furnace (BF) simulator in CO-CO2-N2-reducing gas, simulating conditions at the BF center and wall, is investigated. Measurements from an operating BF guide the study, ensuring realistic reduction parameters. Reduction rate and extent, along with physical properties, are assessed under a temperature range of 700-1100 degrees C. In isothermal reduction experiments, the BF center exhibits superior conditions, particularly at 900 degrees C, achieving an 83.78% reduction degree compared to 27.17% at the wall for the same temperature. In this study, it is highlighted that basic iron ore sinter demonstrates higher reduction efficiency compared to acid iron ore pellets under identical BF center reducing conditions. Specific surface area and porosity measurements unveil a contrasting trend in specific surface area and porosity evolution between the BF wall and center. Surface morphology analysis reveals that the reduction in specific surface area and porosity of sinter samples at the BF center conditions at 1000-1100 degrees C is attributed to the sintering of the formed metallic iron. Carbon analysis confirms no carbon deposition took place during reduction. Mineralogical and physical property analyses provide detailed insights into the evolving phase composition during sinter reduction. In this study, iron ore sinter reduction in a simulated blast furnace environment is investigated. In the results, superior reduction at the blast furnace center, with basic iron ore sinter exhibiting higher efficiency compared to acid pellets, is shown. Temperature variations influence specific surface area and porosity evolution. No carbon deposition occurs during reduction.image (c) 2024 WILEY-VCH GmbH
引用
下载
收藏
页数:14
相关论文
共 50 条
  • [31] Hydrogen-based direct reduction of iron oxide at 700°C: Heterogeneity at pellet and microstructure scales
    Yan Ma
    Isnaldi R.Souza Filho
    Xue Zhang
    Supriya Nandy
    Pere Barriobero-Vila
    Guillermo Requena
    Dirk Vogel
    Michael Rohwerder
    Dirk Ponge
    Hauke Springer
    Dierk Raabe
    International Journal of Minerals,Metallurgy and Materials, 2022, 29 (10) : 1901 - 1907
  • [32] Effect of the Boudouard Reaction on the Reduction of Hematite and a Lorraine Iron Ore Sinter and on the Morphology of the Solids During Reduction.
    Gaballah, I.
    Jeannot, F.
    Gleitzer, Ch.
    Memoires Scientifiques de la Revue de Metallurgie, 1972, 69 (7-8): : 513 - 521
  • [33] Optimization of chemical composition and microstructure of iron ore sinter for low-temperature drip of molten iron with high permeability
    Higuchi, K
    Naito, M
    Nakano, M
    Takamoto, Y
    ISIJ INTERNATIONAL, 2004, 44 (12) : 2057 - 2066
  • [34] Characterisation of iron ore sinter and its behaviour during non-isothermal reduction conditions
    Hessien, M. M.
    Kashiwaya, Y.
    Ishii, K.
    Nasr, M. I.
    El-Geassy, A. A.
    IRONMAKING & STEELMAKING, 2008, 35 (03) : 183 - 190
  • [35] EFFECT OF SINTER-CAKE LOAD REDUCTION BY MAGNETIC FORCE ON IRON-ORE SINTERING
    INAZUMI, T
    FUJIMOTO, M
    SATO, S
    SATO, K
    ISIJ INTERNATIONAL, 1995, 35 (04) : 372 - 379
  • [36] IMPROVEMENT OF PRODUCTIVITY AND REDUCTION DISINTEGRATION OF IRON-ORE SINTER BY INCREASING SIZE OF LIMESTONE PARTICLES
    SHIGAKI, I
    SAWADA, M
    YOSHIOKA, K
    TAKAHASHI, T
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1985, 71 (16): : 1880 - 1887
  • [37] Effects of Compound Silicate Gangue on Mineral Composition and Microstructure of Sinter Produced by Baiyunebo Iron Ore Concentrates
    Luo, Guoping
    Wu, Shengli
    Wang, Yici
    Zhang, Guangjie
    Hao, Zhizhong
    Wu, Hulin
    ADVANCED ENGINEERING MATERIALS, PTS 1-3, 2011, 194-196 : 201 - +
  • [38] Experimental determination of the reaction:: Magnesite+enstatite=forsterite+CO2 in the ranges 6-25kbar and 700-1100°C
    Koziol, AM
    Newton, RC
    AMERICAN MINERALOGIST, 1998, 83 (3-4) : 213 - 219
  • [39] Effect of FeO concentration in sinter iron ore on reduction behavior in a hydrogen-enriched blast furnace
    Ko-ichiro Ohno
    Takayuki Maeda
    Kazuya Kunitomo
    Masashi Hara
    International Journal of Minerals,Metallurgy and Materials, 2022, (10) : 1820 - 1829
  • [40] Effect of FeO concentration in sinter iron ore on reduction behavior in a hydrogen-enriched blast furnace
    Ohno, Ko-ichiro
    Maeda, Takayuki
    Kunitomo, Kazuya
    Hara, Masashi
    INTERNATIONAL JOURNAL OF MINERALS METALLURGY AND MATERIALS, 2022, 29 (10) : 1820 - 1829