摘要
PurposeThis study aims to investigate the effect of incorporating cobalt (Co) into Sn-58Bi alloy on its phase composition, tensile properties, hardness and thermal aging performances. The fracture morphologies of tensile-tested solders are also investigated to correlate the microstructural changes with tensile properties of the solder alloys. Then, the thermal aging performances of the solder alloys are investigated in terms of their intermetallic compound (IMC) layer morphology and thickness.Design/methodology/approachThe Sn-58Bi and Sn-58Bi-xCo, where x = 1.0, 1.5 and 2.0 Wt.%, were prepared using the flux doping technique. X-ray diffraction (XRD) is used to study the phase composition of the solder alloys, whereas scanning electron microscopy (SEM) and energy-dispersive X-ray spectroscopy (EDX) are used to investigate the microstructure, fractography and compositions of the solders. Tensile properties such as ultimate tensile strength (UTS), Young's modulus and elongation are tested using the tensile test, whereas the microhardness value is gained from the micro-Vickers hardness test. The morphology and thickness of the IMC layer at the solder's joints are investigated by varying the thermally aging duration up to 56 days at 80 degrees C.FindingsXRD analysis shows the presence of Co3Sn2 phase and confirms that Co was successfully incorporated via the flux doping technique. The microstructure of all Sn-58Bi-xCo solders did not differ significantly from Sn-58Bi solders. Sn-58Bi-2.0Co solder exhibited optimum properties among all compositions, with the highest UTS (87.89 +/- 2.55 MPa) at 0.01 s-1 strain rate and the lowest IMC layer thickness at the interface after being thermally aged for 56 days (3.84 +/- 0.67 mu m).Originality/valueThe originality and value of this research lie in its novel exploration of the flux doping technique to introduce minor alloying of Co into Sn-58Bi solder alloys, providing new insights into enhancing the properties and performance of these solders. This new Sn-Bi-Co alloy has the potential to replace lead-containing solder alloy in low-temperature soldering.
引用
收藏
页码:285 / 295
页数:11
相关论文
共 50 条
  • [41] Microstructural Evolution and Mechanical Properties of Sn-58Bi Solder Alloys with Different Cooling
    Li, Xiaoping
    Shen, Jun
    Gong, Mengqi
    Li, Hao
    Luo, Dengjun
    Chen, Qin
    Su, Dezhi
    ADVANCED ENGINEERING MATERIALS, 2022, 24 (06)
  • [42] Developing a lead-free solder alloy Sn-Bi-Ag-Cu by mechanical alloying
    C. M. L. Wu
    M. L. Huang
    J. K. L. Lai
    Y. C. Chan
    Journal of Electronic Materials, 2000, 29 : 1015 - 1020
  • [43] Developing a lead-free solder alloy Sn-Bi-Ag-Cu by mechanical alloying
    Wu, CML
    Huang, ML
    Lai, JKL
    Chan, YC
    JOURNAL OF ELECTRONIC MATERIALS, 2000, 29 (08) : 1015 - 1020
  • [44] Effect of cobalt nanoparticles on mechanical properties of Sn-58Bi solder joint (vol 33, pg 22573, 2022)
    Bashir, M. Nasir
    Saad, Hafiz Muhammad
    Rizwan, Muhammad
    Bingol, Sedat
    Channa, Iftikhar Ahmed
    Gul, Mustabshirha
    Haseeb, A. S. M. A.
    Naher, Sumsun
    JOURNAL OF MATERIALS SCIENCE-MATERIALS IN ELECTRONICS, 2022, 33 (36) : 27171 - 27172
  • [45] Microstucture and mechanical properties of semi-solid Sn-58Bi Alloy
    Hu, Yongjun
    Zhong, Binqiang
    Li, Feng
    Cheng, Xiaoling
    Xiao, Xiaoting
    Lin, Yong
    He, Jiannan
    He, Yuanchuan
    Zheng, Chuchun
    Zheng, Yu Chuan
    Wu, Yuchi
    MATERIALS ENGINEERING FOR ADVANCED TECHNOLOGIES, PTS 1 AND 2, 2011, 480-481 : 687 - 690
  • [46] Mechanical Property of Sn-58Bi Solder Paste Strengthened by Resin
    Liu, Lu
    Xue, Songbai
    Liu, Siyi
    APPLIED SCIENCES-BASEL, 2018, 8 (11):
  • [47] Effects of Zn addition on mechanical properties of eutectic Sn-58Bi solder during liquid-state aging
    Ma, Dong-liang
    Wu, Ping
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2015, 25 (04) : 1225 - 1233
  • [48] Effects of Sn-Ag-x layers on the solderability and mechanical properties of Sn-58Bi solder
    Zhang S.
    Liu Y.
    Zhang H.
    Zhou M.
    Xue Y.
    Zeng X.
    Cao R.
    Chen P.
    Welding International, 2021, 35 (1-3): : 16 - 23
  • [49] Effects of Minor Addition of Cu and Ni on the Microstructure, Thermal and Mechanical Properties, and Wettability of Sn-58Bi Solder Alloys
    Sungkhaphaitoon, Phairote
    Chantaramanee, Suchart
    JOURNAL OF ELECTRONIC MATERIALS, 2025, : 4154 - 4165
  • [50] Investigation of microstructures and tensile properties of a Sn-Cu lead-free solder alloy
    Zhu, FL
    Zhang, HH
    Guan, RF
    Liu, S
    JOURNAL OF MATERIALS SCIENCE-MATERIALS IN ELECTRONICS, 2006, 17 (05) : 379 - 384