Effect of heat treatment on microstructure and high-temperature wear performance of additive manufactured IN718

被引:0
|
作者
Samuel, S. Calvin [1 ,8 ]
Prabhu, T. Ram [2 ]
Moganraj, Arivarasu [3 ]
Samuel, Melvin S. [4 ,5 ]
Praveenkumar, K. [6 ]
Bobby, S. Solomon [1 ,7 ]
Prakasam, Anand [7 ]
机构
[1] Additive 3D, Bangalore 560040, Karnataka, India
[2] CEMILAC, Def R&D Org, Bangalore 560075, Karnataka, India
[3] Vellore Inst Technol, Ctr Innovat Mfg Res, Vellore 632014, India
[4] Marquette Univ, Dept Civil Construct & Environm Engn, Milwaukee, WI 53233 USA
[5] Saveetha Inst Med & Tech, Saveetha Sch Engn, Dept Bioengn, Chennai 602105, India
[6] Indian Inst Sci, Dept Mat Engn, Bangalore 560012, India
[7] EOS Electro Opt Syst, Chennai 600099, India
[8] Indian Inst Sci, Dept Design & Mfg, Bangalore 560012, India
关键词
Additive manufacturing; High temperature wear; Laser powder bed fusion; Delamination wear; Solution double aging heat treatment; Tribology; MECHANICAL-PROPERTIES; DELTA-PHASE; LASER; EVOLUTION; BEHAVIOR;
D O I
10.1016/j.jmapro.2024.08.017
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The additive manufactured IN718 under Laser Powder Bed Fused (LPBF) was evaluated for its microstructure, microhardness, and wear behavior in both as-printed and precipitation heat-treated condition. The microstructure of as-print IN718 shows slender columnar dendrites oriented directionally along build direction and coarse cellular structure in the remelt zone that formed between the laser-deposited tracks. After solution double aging heat treatment (AMS 5662), reinforcing precipitates (gamma ' and gamma '') were observed in the gamma-matrix and delta-phase precipitation at grain boundaries. Microhardness analysis indicates that the alloy's hardness was improved and stabilized in all direction after the heat treatment. The alloy's tribological behavior was examined at temperatures of 28 degrees C, 400 degrees C, 500 degrees C, and 600 degrees C in a pin on disc setup. SEM and XRD analyses were used to examine the worn-out surface and wear debris. Surface examination of the worn-out sample reveals abrasion wear at 28 degrees C and delamination wear at 400 degrees C, 500 degrees C and 600 degrees C. The topography study highlights that abrasion and delamination wear are considerably reduced after heat-treatment. The friction coefficient and wear loss increase with the test temperature indicates that delamination plays a crucial role in affecting both friction and wear loss. XRD analysis on the worn-out surface detected nickel oxide (NO) formation in all high temperature tested samples and the NiO is ineffective in reducing friction and wear loss. The sectional analysis of worn-out surface shows noticeable variations in delamination intensity as the test temperature rises. A thorough examination of the wear debris reveals delamination marks on the front surface and micro-cracks developing on the back surface. The microstructure examination carried out near the worn-out surface of both as-printed and heat-treated sample tested at 600 degrees C. The analysis confirmed excess delta-phase formation at the grain boundary of as-printed sample aggravates crack propagation and wear loss due to delamination.
引用
收藏
页码:683 / 697
页数:15
相关论文
共 50 条
  • [41] Experimental Characterization of an Additively Manufactured Inconel 718 Heat Exchanger for High-Temperature Applications
    Battaglia, Fabio
    Arie, Martinus
    Zhang, Xiang
    Ohadi, Michael
    Shooshtari, Amir
    ENERGIES, 2023, 16 (10)
  • [42] Effect of high-temperature heat treatment duration on the purity and microstructure of MWCNTs
    Srikanth, I.
    Padmavathi, N.
    Prasad, P. S. R.
    Ghosal, P.
    Jain, R. K.
    Subrahmanyam, Ch
    BULLETIN OF MATERIALS SCIENCE, 2016, 39 (01) : 41 - 46
  • [43] Effect of high-temperature heat treatment duration on the purity and microstructure of MWCNTs
    I SRIKANTH
    N PADMAVATHI
    P S R PRASAD
    P GHOSAL
    R K JAIN
    CH SUBRAHMANYAM
    Bulletin of Materials Science, 2016, 39 : 41 - 46
  • [44] Effect of Solution Treatment on the Microstructure and Mechanical Properties of IN718 Alloy
    Du Jinhui
    Lv Xudong
    Deng Qun
    Luo Ying
    RARE METAL MATERIALS AND ENGINEERING, 2017, 46 (09) : 2359 - 2365
  • [45] Microstructure and High-Temperature Deformation Behavior of Dissimilar Superalloy Welded Joint of DD407/IN718
    Liu Yang
    Wang Lei
    Song Xiu
    Liang Taosha
    ACTA METALLURGICA SINICA, 2019, 55 (09) : 1221 - 1230
  • [46] Influence of heat-treatment and cryo-treatment on high temperature wear performance of LPBF Inconel 718
    Joshy, Jino
    Kuriachen, Basil
    WEAR, 2023, 522
  • [47] STUDY THE MICROHARDNESS AND SURFACE ROUGHNESS OF AS-BUILT AND HEAT-TREATED ADDITIVE MANUFACTURED IN718 ALLOY
    Maurya, Ajay Kumar
    Kumar, Amit
    UPB Scientific Bulletin, Series D: Mechanical Engineering, 2022, 84 (01): : 211 - 224
  • [48] Comparative study on microstructure, mechanical and high temperature oxidation resistant behaviors of SLM IN718 superalloy before and after heat treatment
    Chen, Bingqing
    Zhuo, Longchao
    Xie, Yixing
    Huang, Shuai
    Wang, Tianyuan
    Yan, Taiqi
    Gong, Xiufang
    Wang, Yanlin
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2024, 31 : 1535 - 1546
  • [49] Effects of Specimen Orientation and Heat Treatment on Microstructure and Crack Propagation Path of the IN718 Alloy Built by the Additive Manufacturing Process
    Kim, Chanmi
    Park, Junho
    Joo, Yunkon
    Kong, Byeongook
    Hong, Hyun-Uk
    Shin, Jong-Ho
    Lee, Jehyun
    METALS AND MATERIALS INTERNATIONAL, 2023, 29 (06) : 1786 - 1795
  • [50] Effects of Specimen Orientation and Heat Treatment on Microstructure and Crack Propagation Path of the IN718 Alloy Built by the Additive Manufacturing Process
    Chanmi Kim
    Junho Park
    Yunkon Joo
    Byeongook Kong
    Hyun-Uk Hong
    Jong-Ho Shin
    Jehyun Lee
    Metals and Materials International, 2023, 29 : 1786 - 1795