Effect of High-Energy Ball-Milling Duration on Densification, Microstructure, and Mechanical Properties of Cr2AlC-Dispersed 90W-6Ni-2Fe-2Co Heavy Alloys

被引:0
|
作者
Adhikari, Deepak [1 ,2 ]
Sengupta, Pradyut [2 ]
Panigrahi, Ajit [1 ,2 ]
Bajpai, Shubhra [1 ,2 ]
Gupta, Surojit [3 ]
Debata, Mayadhar [1 ,2 ]
机构
[1] Acad Sci & Innovat Res AcSIR, Ghaziabad 201002, India
[2] CSIR Inst Minerals & Mat Technol, Adv Mat Technol Dept, Bhubaneswar 751013, India
[3] Univ North Dakota, Dept Mech Engn, Adv Mat Res Grp, 243 Centennial Dr, Grand Forks, ND 58202 USA
关键词
ball milling; grain size refinement; MAX phases; mechanical properties; DYNAMIC DEFORMATION-BEHAVIOR; HALL-PETCH RELATION; MICROHARDNESS MEASUREMENTS; MAX PHASES; NI; TEMPERATURE; CR2ALC; SUBSTITUTION; PERFORMANCE; DISTORTION;
D O I
10.1002/adem.202400852
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
This study focuses on the role of Cr2AlC-MAX phase incorporation on the density, phase composition, microstructure, and mechanical properties of 90W-6Ni-2Fe-2Co heavy alloy. The blended powders are ball milled in a high-energy ball mill up to 40 h, compacted, and sintered at 1500 degrees C. The mechanical alloying results in a refined microstructure with uniform distribution of W, matrix, and dispersoids. The minimum grain size of W (14.7 +/- 5.6 mu m) is obtained in 2 wt% Cr2AlC-containing tungsten alloy prepared from 40 h-milled powders. Among the investigated alloys, 1 wt% Cr2AlC-incorporated samples exhibit maximum compressive stress (2026 MPa). The incorporation of fine Cr2AlC as dispersoids is found to be beneficial in improving the strength as well as ductility of WHAs. The best combination of yield strength (553.4 MPa), ultimate tensile strength (1011.2 MPa), ductility (11.4%), and product of strength and elongation (11.5 GPa%) is found in alloy prepared from 40 h milled 90W-4.8Ni-1.6Fe-1.6Co-2Cr(2)AlC. The improved tensile strength in Cr2AlC-incorporated WHAs may be attributed to the combined effect of grain size refinement and dispersion strengthening. Overall, the combination of ball milling and Cr2AlC incorporation in tungsten-heavy alloys is found to be effective in developing a novel W-based alloy system for strategic applications.
引用
收藏
页数:14
相关论文
共 45 条
  • [41] Effect of Ti additions on the mechanical properties and thermal expansion properties of Ni9Cr9Co9Fe9Tix (x=1, 2, 3) high entropy alloy
    Zhang, Jiachen
    Yang, Zhong
    Yang, Xigang
    Yang, Mingnian
    Cao, Xu
    [J]. MATERIALS TODAY COMMUNICATIONS, 2024, 39
  • [42] Microstructures and mechanical properties of body-centered-cubic (Al, Ti)0.7(Ni,Co,Fe,Cr)5 high entropy alloys with coherent B2/L21 nanoprecipitation
    Li, Chunling
    Ma, Yue
    Hao, Jiamiao
    Yan, Yu
    Wang, Qing
    Dong, Chuang
    Liaw, Peter K.
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2018, 737 : 286 - 296
  • [43] Tuning of the mechanical properties of a laser powder bed fused eutectic high entropy alloy Ni30Co30Cr10Fe10Al18W2 through heat treatment
    Yu, Yiwei
    Zhao, Yakai
    Feng, Kai
    Chen, Rong
    Han, Bolun
    Ji, Kaifeng
    Qin, Meng
    Li, Zhuguo
    Ramamurty, Upadrasta
    [J]. Materials Science and Engineering: A, 2024, 918
  • [44] Electric and ferroelectric properties of high-energy ball milling-assisted (1 − x) Sr0.2Ba0.8TiO3 + (x) Ni0.1Cu0.2Zn0.15Mg0.55Fe2O4 composite
    B. I. Salem
    O. M. Hemeda
    M. Mostafa
    A. M. A. Henaish
    [J]. Journal of Materials Science: Materials in Electronics, 2020, 31 : 18673 - 18682
  • [45] Electric and ferroelectric properties of high-energy ball milling-assisted (1-x) Sr0.2Ba0.8TiO3 + (x) Ni0.1Cu0.2Zn0.15Mg0.55Fe2O4composite
    Salem, B. I.
    Hemeda, O. M.
    Mostafa, M.
    Henaish, A. M. A.
    [J]. JOURNAL OF MATERIALS SCIENCE-MATERIALS IN ELECTRONICS, 2020, 31 (21) : 18673 - 18682