Low cost paints reinforced with an Al2O3/Y2O3/graphene nanocomposite for fire-resistant wood coating applications

被引:2
|
作者
El-Tantawy, Ahmed [1 ]
Hassan, Ibrahim M. [1 ]
El-kady, Omayma A. [2 ]
Ali, Ahmed. I. [3 ,4 ,5 ]
Son, Jong Yeog [4 ,5 ]
Ayoub, Nasser. M. [1 ]
机构
[1] Helwan Univ, Fac Technol & Educ, Dept Prod Technol, El Sawah St, Cairo 11281, Egypt
[2] Cent Met Res & Dev Inst CMRDI, Powder Technol Dept, POB 87, Cairo, Egypt
[3] Helwan Univ, Fac Technol & Educ, Basic Sci Dept, El Sawah St, Cairo 11281, Egypt
[4] Kyung Hee Univ, Coll Appl Sci, Dept Appl Phys, Suwon 446701, South Korea
[5] Kyung Hee Univ, Inst Nat Sci, Coll Appl Sci, Suwon 446701, South Korea
来源
MATERIALS ADVANCES | 2024年 / 5卷 / 18期
关键词
AL2O3-Y2O3;
D O I
10.1039/d4ma00552j
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Low-cost eco-friendly 10wt%Al2O3/5wt%Y2O3/graphene (graphene nanosheets (GNSs): 0.5, 1.0, 1.5, 2.0, 2.5wt%) nanocomposite powders were fabricated using a powder metallurgy technique. X-ray diffraction and FE-SEM confirmed that the phase and morphology of the surface are homogenous and crack-free with nanoscale particles. Thermal analysis (TGA/DSC) confirmed the decomposition sequence as a function of temperature. Furthermore, X-ray photoelectron spectroscopy (XPS) was investigated in a comparison between samples of two compositions of oxygen, aluminum, and yttrium atoms at 75 eV, 158 eV and 158 eV at the equivalent of 1200 cps, 4200 cps, and 4600 cps, respectively. The results for fire resistance confirmed the impact of GNS percentage on fire resistance and fire endurance, and in a rising temperature test. In addition, compared with the period in previous experiments (35 s), the sample with paint with 10wt%Al2O3/5wt%Y2O3/2.5wt%GNSs (2.5 g of graphene) had a fire resistance time of 887 s at T = 190 degrees C. Thus, the present work demonstrated that low-cost and easily fabricated Al2O3/Y2O3/GNSs nanocomposite powders enhanced the properties of the wood-paint to be a good candidate in fire resistance applications.
引用
收藏
页码:7377 / 7386
页数:10
相关论文
共 50 条
  • [31] THERMODYNAMICS OF REDUCTION OF AL2O3, Y2O3, AND SC2O3 IN LI VAPOR
    YUDIN, BF
    LAPSHIN, SA
    POLONSKII, YA
    MOGILENSKII, VI
    INORGANIC MATERIALS, 1976, 12 (11) : 1629 - 1633
  • [32] Effect of Nb2O5 addition on Al2O3 - Y2O3 sintering
    Cabral, R. F.
    Louro, L. H. L.
    Campos, J. B.
    Lima, E. S.
    MATERIA-RIO DE JANEIRO, 2014, 19 (02): : 125 - 131
  • [33] Nano/Micro-Laminated (ZrO2–Y2O3)/(Al2O3–Y2O3) Composite Coatings and Their Oxidation Resistance
    Mingming Yao
    Yedong He
    Deren Wang
    Wei Gao
    Oxidation of Metals, 2007, 68 : 1 - 8
  • [34] Regulation of Y2O3 addition on structure and properties of Al2O3/ZrO2(Y2O3) directionally solidified eutectic ceramic
    Zhai, Shuoyan
    Pan, Wei
    Liu, Juncheng
    CERAMICS INTERNATIONAL, 2023, 49 (18) : 30240 - 30247
  • [35] Ceramics Based on Cubic ZrO2 (Y2O3) with Addition of a Fused Al2O3 – ZrO2 (Y2O3) Eutectic
    S. S. Ordan'yan
    P. S. Gudovskikh
    D. N. Pigunova
    Refractories and Industrial Ceramics, 2004, 45 : 1 - 2
  • [36] PRESSURELESS SINTERING OF SI3N4 WITH Y2O3 AND AL2O3
    HAYASHI, T
    MUNAKATA, H
    SUZUKI, H
    SAITO, H
    JOURNAL OF MATERIALS SCIENCE, 1986, 21 (10) : 3501 - 3508
  • [37] Properties of SiC Ceramics Sintered via Liquid Phase Using Al2O3 + Y2O3, Al2O3 + Yb2O3 and Al2O3 + Dy2O3 as Additives: a Comparative Study
    Ribeiro, Sebastiao
    Ribeiro, Giseli Cristina
    de Oliveira, Marcela Rego
    MATERIALS RESEARCH-IBERO-AMERICAN JOURNAL OF MATERIALS, 2015, 18 (03): : 525 - 529
  • [38] Dispersion of SiC in aqueous media with Al2O3 and Y2O3 as sintering additives
    Zhang, JX
    Iwasa, M
    Jiang, DL
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2005, 88 (04) : 1013 - 1016
  • [39] Effect of toughening with Y2O3 and YAG on the tribological properties of Al2O3 coatings
    Ma, Wenqiang
    Sun, Chufeng
    Zhao, Xiaoqin
    Bu, Zhenyu
    Xue, Yun
    Lu, Lina
    An, Yulong
    Zhou, Huidi
    Chen, Jianmin
    TRIBOLOGY INTERNATIONAL, 2024, 199
  • [40] Effects of Y2O3 addition on microwave dielectric characteristics of Al2O3 ceramics
    Song, K. X.
    Wu, S. Y.
    Chen, X. M.
    MATERIALS LETTERS, 2007, 61 (16) : 3357 - 3360