Simultaneously improving high-temperature strength and ductility of as-cast (TiB + TiC)/Ti-6Al-4Sn-7Zr-1Nb-1Mo-1W-0.2Si via triplex heat treatment

被引:0
|
作者
Wu, Jing-Xi [1 ]
Du, Zhi-Ming [1 ]
Chen, Yu-Yong [1 ]
Xie, Hua-Sheng [2 ,3 ]
Peng, Qing-Jun [4 ]
Liu, Shi-Bing [2 ,3 ]
Zhang, Shu-Zhi [5 ]
Li, Ke-Feng [4 ]
Zhang, Yu [1 ]
机构
[1] Harbin Inst Technol, Sch Mat Sci & Engn, Harbin 150001, Peoples R China
[2] Natl Key Lab Adv Casting Technol, Shenyang 110022, Peoples R China
[3] Shenyang Res Inst Foundry Co Ltd, CAM, Shenyang 110022, Peoples R China
[4] China North Ind Grp Corp Ltd, Harbin Machinery Grp Corp 1, Harbin 150001, Peoples R China
[5] Yanshan Univ, Sch Mat Sci & Engn, Qinhuangdao 066000, Peoples R China
来源
RARE METALS | 2024年
基金
国家重点研发计划; 中国国家自然科学基金; 黑龙江省自然科学基金;
关键词
ALPHA-TITANIUM-ALLOY; TENSILE PROPERTIES; HEAT-TREATMENT; FRACTURE-BEHAVIOR; MECHANICAL-PROPERTIES; POWDER-METALLURGY; THERMAL-STABILITY; MATRIX COMPOSITES; MICROSTRUCTURE; EVOLUTION;
D O I
10.1007/s12598-024-02944-x
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
引用
下载
收藏
页码:652 / 661
页数:10
相关论文
共 36 条
  • [21] The dynamic softening identification and constitutive equation establishment of Ti-6.5Al-2Sn-4Zr-4Mo-1W-0.2Si alloy with initial lamellar microstructure
    Yang, Xuemei
    Zhao, Jinhui
    Yan, Xuewei
    Shi, Xiaonan
    Guo, Hongzhen
    HIGH TEMPERATURE MATERIALS AND PROCESSES, 2022, 41 (01) : 669 - 682
  • [22] Dynamic Softening Behavior of Ti-6.5Al-2Sn-4Zr-4Mo-1W-0.2Si Alloy with Lamellar Starting Microstructure during Hot Deformation
    Yang, Xuemei
    Shi, Xiaonan
    Yan, Xuewei
    Guo, Hongzhen
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2023, 32 (08) : 3729 - 3738
  • [23] Tuning the number density of αs precipitates in Ti-6Al-2Sn-2Zr-3Mo-1Cr-2Nb-0.1Si alloys for achieving high strength
    Wang, Shu
    Liang, Yilong
    Sun, Hao
    Feng, Xin
    Huang, Chaowen
    JOURNAL OF ALLOYS AND COMPOUNDS, 2021, 882
  • [24] Achieving high strength and ductility in Ti-6.8Mo-3.9Al-2.8Cr-2Nb-1.2V-1Zr-1Sn alloy by rapid optimizing microstructure through gradient heat treatment梯度热处理快速优化Ti-6.8Mo-3.9Al-2.8Cr-2Nb-1.2V-1Zr-1Sn合金获得 高强高韧性能的微观组织
    Chang Wang
    Wei Zhou
    Si-yun Li
    Xiao-yong Zhang
    Hui-qun Liu
    Journal of Central South University, 2023, 30 : 387 - 399
  • [25] Fatigue crack initiation in Ti-5Al-4Sn-2Zr-1Mo-0.7Nd-0.25Si high temperature titanium alloy
    Lei, J.F.
    Wang, Z.G.
    Li, D.
    Hu, Z.Q.
    International Journal of Fatigue, 1997, 19 (Suppl 1):
  • [26] Effect of Rare-earth Element Addition on Structure of Heat-resistant Ti-6.5Al-4Zr-2.5Sn-2.4V-1Nb-0.5Mo-0.2Si Titanium Alloy
    Skvortsova, Svetlana
    Grushin, Ivan
    Umarova, Oksana
    Speranskiy, Konstantin
    2017 INTERNATIONAL CONFERENCE ON MECHANICAL, MATERIAL AND AEROSPACE ENGINEERING (2MAE 2017), 2017, 114
  • [27] INTERACTION BETWEEN ND-RICH PHASE PARTICLES AND LIQUID-SOLID INTERFACE IN AS-CAST TI-5AL-4SN-2ZR-1MO-0.25SI-1ND TITANIUM-ALLOY
    LI, GP
    LI, D
    LIU, YY
    HU, ZQ
    SCRIPTA METALLURGICA ET MATERIALIA, 1995, 33 (04): : 547 - 551
  • [28] EFFECT OF HIGH TEMPERATURE DEFORMATlON ON MORPHOLOGY OF Nd-RICH PHASE PARTICLES IN Ti-5Al-4Sn-2Zr-1MO-0.25Si-1Nd ALLOY
    LI Geping
    GUAN Shaoxuan
    WANG Qingjiang
    LIU Yuyin
    LI Dong
    HU Zhuangqi (Institute of Metal Researeh
    Chinese Academy of Sciences
    Shenyang
    China)
    Acta Metallurgica Sinica(English Letters), 1995, (01)
  • [29] Martensite decomposition under thermal-mechanical coupling conditions to fabricate an ultrafine-grained Ti6Al4Mo4Zr1W0.2Si alloy
    Zhou, Taoyu
    Yang, Jiuxu
    Li, Nan
    Sun, Hao
    Zhang, Bohua
    Zhao, Zibo
    Wang, Qingjiang
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2024, 168 : 157 - 168
  • [30] Influence of Isothermal Forging Temperature on Microstructure and Mechanical Properties of Ti-6Al-2Sn-2Zr-3Mo-1Cr-2Nb-Si Titanium Alloy
    Shi Zhifeng
    Guo Hongzhen
    Peng Xiaona
    Wang Tao
    Yao Zekun
    TI-2011: PROCEEDINGS OF THE 12TH WORLD CONFERENCE ON TITANIUM, VOL I, 2012, : 252 - 255