Influence of cryogenic treatment time on the mechanical properties of AZ31 magnesium alloy sheets after cross-rolling

被引:2
|
作者
Shen, Tianyuan [1 ]
Liu, Huan [2 ]
Yang, Gongji [2 ]
Ma, Min [2 ]
Jiang, Bingchun [3 ]
Jing, Lei [4 ]
Wang, Xiaojun [5 ,6 ]
Tang, Lunyuan [6 ]
Lu, Liwei [1 ,2 ]
机构
[1] Hunan Univ Sci & Technol, Sch Mech Engn, Xiangtan 411201, Hunan, Peoples R China
[2] Hunan Univ Sci & Technol, Sch Mat Sci & Engn, Xiangtan 411201, Hunan, Peoples R China
[3] Guangdong Univ Sci & Technol, Sch Mech & Elect Engn, Dongguan 523083, Guangdong, Peoples R China
[4] Northwest Inst Nonferrous Met Res, Xian 710016, Shanxi, Peoples R China
[5] Harbin Inst Technol, Natl Key Lab Precis Hot Proc Met, Harbin 150001, Peoples R China
[6] Hunan Rongtuo New Mat Res Co Ltd, Xiangtan 411100, Hunan, Peoples R China
基金
中国国家自然科学基金;
关键词
AZ31 Magnesium alloy; Cross-rolling; Cryogenic treatment time; Mechanical properties; MICROSTRUCTURE; DEFORMATION; TEXTURE; RECRYSTALLIZATION; EVOLUTION; DUCTILITY; BEHAVIOR; DISLOCATION; PARTICLES;
D O I
10.1016/j.jallcom.2024.174096
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
To investigate the influence of cryogenic treatment time on the mechanical properties and the microstructure of the AZ31 Mg alloy sheets, the different times of cryogenic treatment after two -pass cross -rolling were carried out at air-cooling, 1 hour, 3 hours and 6 hours. The consequences of the tensile experiment illustrated that the crossrolling Mg alloy with 1 -hour cryogenic treatment showed the highest ultimate tensile strength (343 MPa), which was 9.6%, 9.6% and 11.7% higher than air-cooling, 3 -hour cryogenic and 6 -hour cryogenic samples. The primary reasons for this include fine-grained strengthening, twin strengthening, low -angle grain boundaries (LAGBs) strengthening, dislocation strengthening and precipitation strengthening. The internal grain of the magnesium alloy sheet after 1 hour of cryogenic treatment was refined to 5.2 mu m. The {10-11} contraction twin, {10-12} extension twin and {10-12}-{10-11} double twin were surveyed according to the electron backscatter diffraction (EBSD) results. On the <11-20> axis, all the four samples exhibited the {0001} basal texture. And the sample of 1 -hour cryogenic treatment exhibited the highest basal texture intensity. According to the microstructure observation, high -density dislocation and several precipitates were illustrated in the sample of 1hour cryogenic treatment.
引用
收藏
页数:13
相关论文
共 50 条
  • [41] Hot rolling of AZ31 magnesium alloy and its effects on microstructure and mechanical properties
    Chen, B
    Lin, DL
    Zeng, XQ
    Lu, C
    MAGNESIUM - SCIENCE, TECHNOLOGY AND APPLICATIONS, 2005, 488-489 : 619 - 622
  • [42] Mechanical properties and formability of AZ31 magnesium alloy processed by differential speed rolling
    Huang, Xinsheng
    Suzuki, Kazutaka
    Watazu, Akira
    Shigematsu, Ichinori
    Saito, Naobumi
    ECO-MATERIALS PROCESSING AND DESIGN VIII, 2007, 544-545 : 395 - +
  • [43] Influence of different deformation processing on the AZ31 magnesium alloy sheets
    Su-Qin Zhu
    Hong-Ge Yan
    Wei-Jun Xia
    Ji-Zi Liu
    Jun-Feng Jiang
    Journal of Materials Science, 2009, 44 : 3800 - 3806
  • [44] Influence of Microstructure and Mechanical Properties on Formability in High Strain Rate Rolled AZ31 Magnesium Alloy Sheets
    Liu, Fubao
    Liu, Xiao
    Zhu, Biwu
    Yang, Hui
    Xiao, Gang
    Hu, Mingyue
    METALS AND MATERIALS INTERNATIONAL, 2022, 28 (06) : 1361 - 1371
  • [45] Influence of different deformation processing on the AZ31 magnesium alloy sheets
    Zhu, Su-Qin
    Yan, Hong-Ge
    Xia, Wei-Jun
    Liu, Ji-Zi
    Jiang, Jun-Feng
    JOURNAL OF MATERIALS SCIENCE, 2009, 44 (14) : 3800 - 3806
  • [46] The influence of preheating temperature on the mechanical properties of AZ31 magnesium alloys after hot-rolling
    Janecek, M
    Supík, V
    Holländer, F
    Wendt, J
    KOVOVE MATERIALY-METALLIC MATERIALS, 2005, 43 (03): : 218 - 228
  • [47] Influence of Microstructure and Mechanical Properties on Formability in High Strain Rate Rolled AZ31 Magnesium Alloy Sheets
    Fubao Liu
    Xiao Liu
    Biwu Zhu
    Hui Yang
    Gang Xiao
    Mingyue Hu
    Metals and Materials International, 2022, 28 : 1361 - 1371
  • [48] Influence of hot extrusion on microstructure and mechanical properties of AZ31 magnesium alloy
    Wang Ling
    Tian Su-gui
    Meng Fan-lai
    Du Hong-qiang
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2006, 16 : S1770 - S1773
  • [49] Influence of homogenizing on mechanical properties of as-cast AZ31 magnesium alloy
    张宝红
    张治民
    Transactions of Nonferrous Metals Society of China, 2010, 20 (S2) : 439 - 443
  • [50] Influence of homogenizing on mechanical properties of as-cast AZ31 magnesium alloy
    Zhang B.-H.
    Zhang Z.-M.
    Transactions of Nonferrous Metals Society of China (English Edition), 2010, 20 (SUPPL. 2): : s439 - s443