Effect of process parameter on the flowability of nanocrystalline CoNiCrAlY powder synthesized by mechanical milling

被引:0
|
作者
Dash, Annadaa Shankara [1 ]
Manna, Indranil [2 ,3 ]
Devapal, Deepa [4 ]
Sharma, Sharad Chandra [4 ]
Majumdar, Jyotsna Dutta [3 ]
机构
[1] IIT Kharagpur, Sch Nanosci & Technol, Kharagpur, West Bengal, India
[2] BIT Mesra, Ranchi, Jharkhand, India
[3] IIT Kharagpur, Dept Met & Mat Engn, Kharagpur, West Bengal, India
[4] Vikram Sarabhai Space Ctr, Thiruvananthapuram, Kerala, India
来源
PARTICUOLOGY | 2024年 / 92卷
关键词
Mechanical milling; Microstructure; Process control agent (PCA); CoNiCrAlY; Toluene; Stearic acid; Flowability; ISOTHERMAL OXIDATION BEHAVIOR; BETA-PHASE DEPLETION; PARTICLE-SIZE; BOND COATS; COATINGS; TEMPERATURE; HVOF; TRANSFORMATION; OPTIMIZATION; RESISTANCE;
D O I
10.1016/j.partic.2024.05.006
中图分类号
TQ [化学工业];
学科分类号
0817 ;
摘要
The present study concerns understanding the effect of process parameters on the characteristics and flowability of nanocrystalline CoNiCrAlY powder synthesized by mechanical milling. Mechanical milling has been conducted in a planetary ball mill with tungsten carbide (WC) ball, with ball to powder ratio of 10:1 at 300 rpm speed, using 1% stearic acid and toluene as process control agent (PCA) with time varying from 10 h to 36 h. The synthesized nanocrystalline powder were characterized by Scanning Electron Microscopy, X-ray Diffraction technique, X-ray Photoelectron Spectroscopy, and Differential Scanning Calorimetry. Subsequently, flowability in terms of Hausner ratio was assessed by Tap Density Tester. Average particle size of the powder was found to decrease from 33 mu m to 22 mu m after 10 h of milling and further increases to 43 mu m and 38 mu m after 25 and 36 h of milling, respectively, in stearic acid medium. However, in toluene medium particle size continuously decreases from 33 mu m to 9.7 mu m with increasing milling time. The particle morphology changes from spherical to platelet shape at low milling hours in both of the media. After 25 h of milling, the shape of the particles is nearly spherical for stearic acid and irregular for toluene used as a PCA. Crystallize size was found to decrease with increasing milling time from 147 nm to 7.7 nm and to 6.4 nm in stearic acid and toluene media, respectively. There was presence of y, y', 13, hcp-Co, Al2O3 and AlOOH phases on the powder particles milled in both the medium. The measured Hausner ratio of the powders was found to vary from 1.18 to 1.32 in stearic acid medium, and was found to increase with increasing milling time. On the other hand, in toluene media flowability decreases (Hausner ratio increases from 1.33 to 1.44) with increasing milling time. (c) 2024 Published by Elsevier B.V. on behalf of Chinese Society of Particuology and Institute of Process Engineering, Chinese Academy of Sciences.
引用
收藏
页码:210 / 223
页数:14
相关论文
共 50 条
  • [21] Effect of particle surface roughness on the flowability and spreadability of Haynes 230 powder during laser powder bed fusion process
    Zhang, Peng
    Bi, Zhongnan
    Yu, Hongyao
    Wang, Rui
    Sun, Guangbao
    Zhang, Shaoming
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2023, 26 : 4444 - 4454
  • [22] Optimized nanocrystalline strontium hexaferrite prepared by applying a methane GTR process on a conventionally synthesized powder
    Dehghan, R.
    Ebrahimi, S. A. Seyyed
    JOURNAL OF MAGNETISM AND MAGNETIC MATERIALS, 2014, 368 : 234 - 239
  • [23] Synthesis of the nanocrystalline/nanosized NiFe2O4 powder by ceramic method and mechanical milling
    Tarta, V. F.
    Chicinas, I.
    Marinca, T. F.
    Neamtu, B. V.
    Popa, F.
    Prica, C. V.
    ADVANCED MATERIALS AND STRUCTURES IV, 2012, 188 : 27 - 30
  • [24] Effect of Process Parameters on the Characteristics of Nanocrystalline Alumina Particles Synthesized by Solution Combustion Process
    Bobu Manuel Jolly
    Sai Kishore Ravi
    Stephen Ipe
    S. S. Bhattacharya
    Transactions of the Indian Institute of Metals, 2015, 68 : 147 - 151
  • [25] Effect of Process Parameters on the Characteristics of Nanocrystalline Alumina Particles Synthesized by Solution Combustion Process
    Jolly, Bobu Manuel
    Ravi, Sai Kishore
    Ipe, Stephen
    Bhattacharya, S. S.
    TRANSACTIONS OF THE INDIAN INSTITUTE OF METALS, 2015, 68 : S147 - S151
  • [26] Prenucleation effect on characterisations of synthesised nanocrystalline tungsten carbide via mechanical milling
    Razavi, M.
    Rahimipour, M. R.
    Rajabi, A.
    MATERIALS TECHNOLOGY, 2013, 28 (03) : 145 - 154
  • [27] Effect of mechanical milling of fly ash powder on compressive strength of geopolymer
    Debnath, Krishna
    Das, Dipankar
    Rout, Prasanta Kumar
    MATERIALS TODAY-PROCEEDINGS, 2022, 68 : 242 - 249
  • [28] Magnetic behavior of nickel ferrite-polyethylene nanocomposites synthesized by mechanical milling process
    Nathani, H
    Gubbala, S
    Misra, RDK
    MATERIALS SCIENCE AND ENGINEERING B-SOLID STATE MATERIALS FOR ADVANCED TECHNOLOGY, 2004, 111 (2-3): : 95 - 100
  • [29] Effect of the ball milling process on surface hydration behavior of ceramic powder
    Xu, Yuping
    Shimizu, Wakako
    Xin, Yunzi
    Kato, Kunihiko
    Shirai, Takashi
    CERAMICS INTERNATIONAL, 2024, 50 (11) : 20790 - 20795
  • [30] An Investigation on Hydrogen Storage Kinetics of the Nanocrystalline and Amorphous LaMg12-type Alloys Synthesized by Mechanical Milling
    张羊换
    WANG Jinglong
    ZHANG Peilong
    ZHU Yongguo
    HOU Zhonghui
    SHANG Hongwei
    Journal of Wuhan University of Technology(Materials Science), 2018, 33 (02) : 278 - 287