Effect of process parameter on the flowability of nanocrystalline CoNiCrAlY powder synthesized by mechanical milling

被引:0
|
作者
Dash, Annadaa Shankara [1 ]
Manna, Indranil [2 ,3 ]
Devapal, Deepa [4 ]
Sharma, Sharad Chandra [4 ]
Majumdar, Jyotsna Dutta [3 ]
机构
[1] IIT Kharagpur, Sch Nanosci & Technol, Kharagpur, West Bengal, India
[2] BIT Mesra, Ranchi, Jharkhand, India
[3] IIT Kharagpur, Dept Met & Mat Engn, Kharagpur, West Bengal, India
[4] Vikram Sarabhai Space Ctr, Thiruvananthapuram, Kerala, India
来源
PARTICUOLOGY | 2024年 / 92卷
关键词
Mechanical milling; Microstructure; Process control agent (PCA); CoNiCrAlY; Toluene; Stearic acid; Flowability; ISOTHERMAL OXIDATION BEHAVIOR; BETA-PHASE DEPLETION; PARTICLE-SIZE; BOND COATS; COATINGS; TEMPERATURE; HVOF; TRANSFORMATION; OPTIMIZATION; RESISTANCE;
D O I
10.1016/j.partic.2024.05.006
中图分类号
TQ [化学工业];
学科分类号
0817 ;
摘要
The present study concerns understanding the effect of process parameters on the characteristics and flowability of nanocrystalline CoNiCrAlY powder synthesized by mechanical milling. Mechanical milling has been conducted in a planetary ball mill with tungsten carbide (WC) ball, with ball to powder ratio of 10:1 at 300 rpm speed, using 1% stearic acid and toluene as process control agent (PCA) with time varying from 10 h to 36 h. The synthesized nanocrystalline powder were characterized by Scanning Electron Microscopy, X-ray Diffraction technique, X-ray Photoelectron Spectroscopy, and Differential Scanning Calorimetry. Subsequently, flowability in terms of Hausner ratio was assessed by Tap Density Tester. Average particle size of the powder was found to decrease from 33 mu m to 22 mu m after 10 h of milling and further increases to 43 mu m and 38 mu m after 25 and 36 h of milling, respectively, in stearic acid medium. However, in toluene medium particle size continuously decreases from 33 mu m to 9.7 mu m with increasing milling time. The particle morphology changes from spherical to platelet shape at low milling hours in both of the media. After 25 h of milling, the shape of the particles is nearly spherical for stearic acid and irregular for toluene used as a PCA. Crystallize size was found to decrease with increasing milling time from 147 nm to 7.7 nm and to 6.4 nm in stearic acid and toluene media, respectively. There was presence of y, y', 13, hcp-Co, Al2O3 and AlOOH phases on the powder particles milled in both the medium. The measured Hausner ratio of the powders was found to vary from 1.18 to 1.32 in stearic acid medium, and was found to increase with increasing milling time. On the other hand, in toluene media flowability decreases (Hausner ratio increases from 1.33 to 1.44) with increasing milling time. (c) 2024 Published by Elsevier B.V. on behalf of Chinese Society of Particuology and Institute of Process Engineering, Chinese Academy of Sciences.
引用
收藏
页码:210 / 223
页数:14
相关论文
共 50 条
  • [1] Mechanical milling process modeling and making WC nanocrystalline powder
    A. I. Gusev
    A. S. Kurlov
    Inorganic Materials, 2009, 45 : 35 - 42
  • [2] Mechanical milling process modeling and making WC nanocrystalline powder
    Gusev, A. I.
    Kurlov, A. S.
    INORGANIC MATERIALS, 2009, 45 (01) : 35 - 42
  • [3] Thermal stability of nanocrystalline WC–Co powder synthesized by using mechanical milling at low temperature
    Jianhong He
    Leoanardo Ajdelsztajn
    Enrique J. Lavernia
    Journal of Materials Research, 2001, 16 : 478 - 488
  • [4] Raman Scattering of Nanocrystalline δ-TiNx Synthesized by Mechanical Milling
    DING Zhan-hui 1
    2. key Laboratory of Superhard Materials
    3. key Laboratory of Excited State Process
    Chemical Research in Chinese Universities, 2005, (04) : 489 - 491
  • [5] Raman scattering of nanocrystalline δ-TiNx synthesized by mechanical milling
    Ding, ZH
    Yao, B
    Ma, HA
    Jia, XP
    Qiu, LX
    Su, WH
    CHEMICAL RESEARCH IN CHINESE UNIVERSITIES, 2005, 21 (04) : 489 - 491
  • [7] Thermal stability of nanocrystalline WC-Co powder synthesized by using mechanical milling at low temperature
    He, JH
    Ajdelsztajn, L
    Lavernia, EJ
    JOURNAL OF MATERIALS RESEARCH, 2001, 16 (02) : 478 - 488
  • [8] The Effect of Powder Flowability in the Selective Laser Sintering Process
    Tan, Yuan-qiang
    Zheng, Jun-hui
    Gao, Wei
    Jiang, Sheng-qiang
    Feng, Yuntian
    PROCEEDINGS OF THE 7TH INTERNATIONAL CONFERENCE ON DISCRETE ELEMENT METHODS, 2017, 188 : 629 - 636
  • [9] Nanocrystalline/nanoparticle ZnO synthesized by high energy ball milling process
    Amirkhanlou, Sajjad
    Ketabchi, Mostafa
    Parvin, Nader
    MATERIALS LETTERS, 2012, 86 : 122 - 124
  • [10] Synthesized by ball milling Al-Pb-Si-Sn-Cu nanocrystalline powder
    Ran, G
    Zhou, JE
    Li, PL
    Xi, SQ
    Zhang, ZW
    RARE METAL MATERIALS AND ENGINEERING, 2004, 33 (12) : 1312 - 1316