Effect of fast charging on degradation and safety characteristics of lithium-ion batteries with LiNi x Co y Mn z Al 1- x- y- z O 2 cathodes

被引:3
|
作者
Zhou, Hanwei [1 ]
Alujjage, Anuththara S. [1 ]
Terese, Maria [1 ]
Fear, Conner [1 ]
Joshi, Tapesh [2 ]
Rikka, Vallabha Rao [2 ]
Jeevarajan, Judith A. [2 ]
Mukherjee, Partha P. [1 ]
机构
[1] Purdue Univ, Sch Mech Engn, W Lafayette, IN 47907 USA
[2] UL Res Inst, Electrochem Safety Res Inst, Houston, TX 77204 USA
关键词
Lithium -ion battery; Fast charging; NCMA cathode; Degradation mechanisms; Accelerating rate calorimeter; Thermal stability; Battery safety; DIFFERENTIAL VOLTAGE ANALYSIS; IMPEDANCE SPECTROSCOPY; CYCLE LIFE; CELLS; CHALLENGES; OPPORTUNITIES; OPTIMIZATION; INSIGHTS; ANODE; RICH;
D O I
10.1016/j.cej.2024.152181
中图分类号
X [环境科学、安全科学];
学科分类号
08 ; 0830 ;
摘要
Fast charging compatibility is an important technical aspect required of advanced lithium-ion (Li-ion) batteries to lead the revolution and increase the adoption of electric vehicles. Although substantial material-level innovations have greatly promoted the widespread employment of fast charging rates for Li-ion batteries, the unfavorable rapid degradation and cell-level thermal instability are still bottlenecks for commercial success. In this study, fast-charging induced aging mechanisms and thermal safety characteristics of Li-ion batteries with quaternary energy-dense LiNixCoyMnzAl1-x-y-zO2 (NCMA) cathodes are comprehensively investigated. Promising fast-charge strategies under different thermal environments are applied to reveal their specific adverse side effects on electrochemical performances and cell lifetime. Post-mortem analysis is conducted to understand the distributions, microstructures, and chemical states of electrodepositions on cell components. Cell-level thermal safety evaluations are carried out based on accelerating rate calorimeter tests to determine evolutions of thermal safety hazards as a result of imposed fast charging conditions. This research highlights the significant role of lithium plating and aluminum dissolution in accelerating the thermo-electrochemical failure of the chosen NCMA-based Li-ion chemistry, providing new insights on degradation-safety interactions and effective mitigation strategies under fast charging conditions.
引用
收藏
页数:15
相关论文
共 50 条
  • [41] Characteristics of LiCoO2, LiMn2O4 and LiNi0.45Co0.1Mn0.45O2 as cathodes of lithium ion batteries
    Hua-jun Guo
    Xin-hai Li
    Xin-ming Zhang
    Su-ming Zeng
    Zhi-xing Wang
    Wen-jie Peng
    Journal of Central South University of Technology, 2005, 12 : 44 - 49
  • [42] Degradation mechanism and performance enhancement strategies of LiNixCoyAl1-x-yO2 (x ≥ 0.8) cathodes for rechargeable lithium-ion batteries: a review
    Fang, Rui
    Miao, Chang
    Nie, Yan
    Wang, Ding
    Xiao, Wei
    Xu, Mingbiao
    Wang, Changjun
    IONICS, 2020, 26 (07) : 3199 - 3214
  • [43] A novel layered material of LiNi0.32Mn0.33Co0.33Al0.01O2 for advanced lithium-ion batteries
    Wu, Feng
    Wang, Meng
    Su, Yuefeng
    Bao, Liying
    Chen, Shi
    JOURNAL OF POWER SOURCES, 2010, 195 (09) : 2900 - 2904
  • [44] Dual-Functional Tungsten Boosted Lithium-Ion Diffusion and Structural Integrity of LiNi0.8Co0.1Mn0.1O2 Cathodes for High Performance Lithium-Ion Batteries
    Zhu, Zhenhua
    Gao, Aimei
    Liang, Yansheng
    Yi, Fenyun
    Meng, Tao
    Ling, Jingzhou
    Hao, Junnan
    Shu, Dong
    ACS SUSTAINABLE CHEMISTRY & ENGINEERING, 2022, 10 (01) : 50 - 60
  • [45] Probing depth-dependent inhomogeneous lithium concentration in thick LiNi0.88Co0.09Al0.03O2 cathodes for lithium-ion batteries
    Choi, Soyoung
    Toaran, Weerawat
    Kim, Seong Heon
    Song, Young Jae
    Kim, Young -Jun
    JOURNAL OF ALLOYS AND COMPOUNDS, 2023, 943
  • [46] Capacity fade of LiNi(1-x-y)CoxAlyO2 cathode for lithium-ion batteries during accelerated calendar and cycle life test. I. Comparison analysis between LiNi(1-x-y)CoxAlyO2 and Li CoO2 cathodes in cylindrical lithium-ion cells during long term storage test
    Watanabe, Shoichiro
    Kinoshita, Masahiro
    Nakura, Kensuke
    JOURNAL OF POWER SOURCES, 2014, 247 : 412 - 422
  • [47] Single-crystal LiNi0.5Co0.2Mn0.3O2: a high thermal and cycling stable cathodes for lithium-ion batteries
    Zeqin Zhong
    Lingzhen Chen
    Shaozhen Huang
    Weili Shang
    Lingyong Kong
    Ming Sun
    Lei Chen
    Wangbao Ren
    Journal of Materials Science, 2020, 55 : 2913 - 2922
  • [48] Single-crystal LiNi0.5Co0.2Mn0.3O2: a high thermal and cycling stable cathodes for lithium-ion batteries
    Zhong, Zeqin
    Chen, Lingzhen
    Huang, Shaozhen
    Shang, Weili
    Kong, Lingyong
    Sun, Ming
    Chen, Lei
    Ren, Wangbao
    JOURNAL OF MATERIALS SCIENCE, 2020, 55 (07) : 2913 - 2922
  • [49] Atomic-scale constituting stable interface for improved LiNi0.6Mn0.2Co0.2O2 cathodes of lithium-ion batteries
    Wang, Xin
    Cai, Jiyu
    Liu, Yongqiang
    Han, Xiaoxiao
    Ren, Yang
    Li, Jianlin
    Liu, Yuzi
    Meng, Xiangbo
    NANOTECHNOLOGY, 2021, 32 (11)
  • [50] The Electrolyte Additive Effects on Commercialized Ni-Rich LiNixCoyMnzO2 (x plus y plus z=1) Based Lithium-Ion Pouch Batteries at High Temperature
    Wang, Chengyun
    Hu, Qianqian
    Hao, Junnan
    Xu, Xijun
    Ouyang, Liuzhang
    Fan, Weizhen
    Ye, Jianshan
    Liu, Jiangwen
    Li, Jin
    Mei, Ao
    Zhu, Min
    ACS APPLIED ENERGY MATERIALS, 2021, 4 (03) : 2292 - 2299