Effect of the application of surface treatments before and after sintering on the flexural strength, phase transformation and surface topography of zirconia

被引:23
|
作者
Kurtulmus-Yilmaz, Sevcan [1 ]
Aktore, Huseyin [1 ]
机构
[1] Near East Univ, Fac Dent, Dept Prosthodont, Mersin10, Lefkosa, Turkey
关键词
Er; Cr:YSGG laser; Airborne-particle abrasion; Pre-sintered zirconia; XRD analysis; FE-SEM analysis; SHEAR BOND STRENGTH; Y-TZP ZIRCONIA; PARTIALLY-STABILIZED ZIRCONIA; AIRBORNE-PARTICLE ABRASION; MECHANICAL-PROPERTIES; HEAT-TREATMENT; CERAMICS; LASER; CORE; ROUGHNESS;
D O I
10.1016/j.jdent.2018.02.006
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Objectives: To evaluate the effects of airborne-particle abrasion (APA) and Er, Cr:YSGG laser irradiation on 4-point-flexural strength, phase transformation and morphologic changes of zirconia ceramics treated at pre-sintered or post-sintered stage. Methods: Three hundred and forty-two bar shaped zirconia specimens were milled with different sizes according to the flexural strength test (n = 10), X-ray diffraction (XRD) (n = 4) and field emission scanning electron microscope (FE-SEM) (n = 4) analyses. For each test protocol, specimens were divided into 4 main groups whether the surface treatments applied before or after sintering and whether the specimens received heat treatment or not as pre-sintered, post-sintered no-heat and post-sintered heat-treated groups, and a group was served as control. Main groups were further divided into 6 equal subgroups according to surface treatment method applied (2 W-, 3 W-, 4 W-, 5 W-, 6 W- laser irradiations and APA). Surface treatments were applied to pre-sintered groups before sintering and to post-sintered groups after sintering. Post-sintered heat-treated groups were subjected to veneer ceramic firing simulation after surface treatments. Flexural strength and flexural modulus values were statistically analysed and monoclinic phase content was calculated. Weibull analysis was used to evaluate strength reliability and fractographic analysis was conducted. Results: Highest flexural strength values were detected at post-sintered no-heat APA and 4W-laser groups (P < 0.05). Pre-sintered groups showed statistically lower flexural strength values. Heat treatment decreased the strength of the specimens. Monoclinic phase content was only detected at post-sintered no-heat groups and the highest amount was detected at APA group. Rougher surfaces and deeper irregularities were detected at FE-SEM images pre-sintered groups. Conclusions: Application of surface treatments at pre-sintered stage may be detrimental for zirconia ceramics in terms of flexural strength. Clinical significance: Treating the surface of zirconia ceramic before sintering process is not recommended due to significant decrease in flexural strength values. 2 W-4 W Er, Cr: YSGG laser irradiations can be regarded as alternative surface treatment methods when zirconia restoration would be subjected to veneer ceramic firing procedures.
引用
收藏
页码:29 / 38
页数:10
相关论文
共 50 条
  • [21] Effect of thickness and surface modifications on flexural strength of monolithic zirconia
    Ozer, Fusun
    Naden, Andrew
    Turp, Volkan
    Mante, Francis
    Sen, Deniz
    Blatz, Markus B.
    JOURNAL OF PROSTHETIC DENTISTRY, 2018, 119 (06): : 987 - 993
  • [22] Influence of surface treatment before glazing on wear and flexural strength of translucent zirconia
    Wenger, Manon
    Zitzmann, Nicola U.
    Rohr, Nadja
    DENTAL MATERIALS, 2025, 41 (04) : 464 - 472
  • [23] Effect of different zirconia surface pretreatments on the flexural strength of veneered Y-TZP ceramic before and after in vitro aging
    Siarampi, Eleni
    Sarafidou, Katia
    Papadopoulou, Lambrini
    Kantiranis, Nikolaos
    Kontonasaki, Eleana
    Koidis, Petros
    JOURNAL OF PROSTHODONTIC RESEARCH, 2022, 66 (03) : 491 - 501
  • [24] Surface Microhardness and Flexural Strength of Colored Zirconia
    Liu Qi
    Shao Longquan
    Wen Ning
    Deng Bin
    CHINESE CERAMICS COMMUNICATIONS, 2010, 105-106 : 49 - +
  • [25] Effect of surface treatments on the flexural strength of dental ceramics.
    Kim, CW
    Chung, SH
    Lim, BS
    JOURNAL OF DENTAL RESEARCH, 1996, 75 : 380 - 380
  • [26] Effect of Surface Treatments and Aging in Water on Bond Strength to Zirconia
    Lindgren, J.
    Smeds, J.
    Sjogren, G.
    OPERATIVE DENTISTRY, 2008, 33 (06) : 675 - 681
  • [27] Effect of surface treatments on bonding strength of zirconia to dental cements
    Hashiguchi, M.
    Sato, H.
    Nishi, Y.
    Ban, S.
    Krnel, K.
    Kocjan, A.
    Kosmac, T.
    BIOCERAMICS 21, 2009, 396-398 : 575 - 578
  • [28] Effect of zirconia surface treatments on the shear strength of zirconia/veneering ceramic composites
    Fischer, Jens
    Grohmann, Philipp
    Stawarczyk, Bogna
    DENTAL MATERIALS JOURNAL, 2008, 27 (03) : 448 - 454
  • [29] Effect of surface treatments on the bond strength of veneering ceramic to zirconia
    Korkmaz, Fatih Mehmet
    Bagis, Bora
    Turgut, Sedanur
    Ates, Sabit Melih
    Ayaz, Elif Aydogan
    JOURNAL OF APPLIED BIOMATERIALS & FUNCTIONAL MATERIALS, 2015, 13 (01): : 17 - 27
  • [30] The Effect of Translucency and Surface Treatment on the Flexural Strength of Aged Monolithic Zirconia
    Giti, Rashin
    Abbasi, Benika
    INTERNATIONAL JOURNAL OF DENTISTRY, 2021, 2021