Replacing Phenol and Formaldehyde for Green Adhesive Synthesis by Lignin and Furfural

被引:2
|
作者
Tao, Yehan [1 ]
Zhou, Siying [1 ]
Luo, Qi [1 ,2 ]
Song, Fei [1 ,2 ]
Gong, Xiaoyu [1 ]
Wang, Zhicheng [1 ]
Wang, Haisong [1 ]
Li, Changzhi [2 ]
机构
[1] Dalian Polytech Univ, Coll Light Ind & Chem Engn, Liaoning Collaborat Innovat Ctr Lignocellulos Bior, Liaoning Key Lab Lignocellulose Chem & Biomat, Dalian 116034, Peoples R China
[2] Chinese Acad Sci, Dalian Inst Chem Phys, CAS Key Lab Sci & Technol Appl Catalysis, Dalian 116023, Peoples R China
来源
ACS APPLIED POLYMER MATERIALS | 2024年 / 6卷 / 12期
基金
中国国家自然科学基金;
关键词
lignin; furfural; green adhesive; phenol-formaldehyde; biomass; THERMAL-PROPERTIES; RESIN; DEPOLYMERIZATION; BIOMASS;
D O I
10.1021/acsapm.3c03087
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Traditional phenol-formaldehyde resin involves the use of petrochemical-based phenol and formaldehyde as feedstocks, raising environmental and health concerns. Herein, renewable biobased substances, i.e., lignin and furfural, were employed to partially replace petroleum-based phenol and formaldehyde for developing greener adhesives by batch copolymerization method. The substitution rates of phenol by acetonitrile-extracted lignin and formaldehyde by furfural can reach 80 and 15%, respectively. The application of these greener raw materials can effectively decrease the emission of toxic content, increasing the viscosity and thermal stability without any sacrifice in the binding performance. The resin with 40% phenol substitution rate and 15% formaldehyde substitution rate displayed superior trade-off between bonding strength (a wet tensile strength of 1.68 MPa) and free formaldehyde content (0.21%) among all biobased resins, much superior to those of commercial adhesive (0.7 MPa and 5%) and those prepared with industrial lignin (0.66 MPa and 0.38%). By using two major biomass-derived feedstocks, this work provides a sustainable strategy to develop a green adhesive featuring superior adhesive properties, enhanced environmental compatibility, and improved thermal stability that shows a broader application potential in the adhesive field.
引用
收藏
页码:6897 / 6905
页数:9
相关论文
共 50 条
  • [31] Thermal degradation of lignin-phenol-formaldehyde and phenol-formaldehyde resol resins
    Alonso, M. V.
    Oliet, M.
    Dominguez, J. C.
    Rojo, E.
    Rodriguez, F.
    JOURNAL OF THERMAL ANALYSIS AND CALORIMETRY, 2011, 105 (01) : 349 - 356
  • [32] Replacing formaldehyde by furfural in urea formaldehyde resin: effect on formaldehyde emission and physical–mechanical properties of particleboards
    Robab Ghafari
    Kazem DoostHosseini
    Ali Abdulkhani
    Sayed Ahmad Mirshokraie
    European Journal of Wood and Wood Products, 2016, 74 : 609 - 616
  • [33] Kraft lignin in phenol formaldehyde resin. Part 1. Partial replacement of phenol by kraft lignin in phenol formaldehyde adhesives for plywood
    Danielson, B
    Simonson, R
    JOURNAL OF ADHESION SCIENCE AND TECHNOLOGY, 1998, 12 (09) : 923 - 939
  • [34] PHENOL-LIGNIN-FORMALDEHYDE ADHESIVES FOR PLYWOOD
    GUPTA, RC
    SINGH, SP
    JOLLY, S
    HOLZFORSCHUNG UND HOLZVERWERTUNG, 1978, 30 (06): : 109 - 112
  • [35] Effect of the Adhesive System on the Properties of Fiberboard Panels Bonded with Hydrolysis Lignin and Phenol-Formaldehyde Resin
    Savov, Viktor
    Valchev, Ivo
    Antov, Petar
    Yordanov, Ivaylo
    Popski, Zlatomir
    POLYMERS, 2022, 14 (09)
  • [36] Graphitization of Lignin-Phenol-Formaldehyde Resins
    Talabi, Segue Isaac
    da Luz, Ana Paula
    Pandolfelli, Victor Carlos
    Lima, Vitor Hugo
    Botaro, Vaguer Roberto
    Lucas, Alessandra de Almeida
    MATERIALS RESEARCH-IBERO-AMERICAN JOURNAL OF MATERIALS, 2020, 23 (02):
  • [37] Lignin-phenol-formaldehyde aerogels and cryogels
    Grishechko, L. I.
    Amaral-Labat, G.
    Szczurek, A.
    Fierro, V.
    Kuznetsov, B. N.
    Celzard, A.
    MICROPOROUS AND MESOPOROUS MATERIALS, 2013, 168 : 19 - 29
  • [38] Synthesis and characterization of phenol-formaldehyde resin using enzymatic hydrolysis lignin
    Qiao, Wei
    Li, Shujun
    Guo, Guowan
    Han, Shiyan
    Ren, Shixue
    Ma, Yanli
    JOURNAL OF INDUSTRIAL AND ENGINEERING CHEMISTRY, 2015, 21 : 1417 - 1422
  • [39] Replacing formaldehyde by furfural in urea formaldehyde resin: effect on formaldehyde emission and physical-mechanical properties of particleboards
    Ghafari, Robab
    DoostHosseini, Kazem
    Abdulkhani, Ali
    Mirshokraie, Sayed Ahmad
    EUROPEAN JOURNAL OF WOOD AND WOOD PRODUCTS, 2016, 74 (04) : 609 - 616
  • [40] THERMAL AND ADHESIVE CHARACTERISTICS OF ACETONE-FORMALDEHYDE-PHENOL-FORMALDEHYDE RESINS
    STEINER, PR
    FOREST PRODUCTS JOURNAL, 1977, 27 (09) : 38 - 43