Comparative investigation of structural, morphological, mechanical, tribological and electrochemical properties of TiO2 films formed on Cp-Ti, Ti6Al4V and Ti45Nb alloys

被引:1
|
作者
Kovaci, H. [1 ]
Senel, K. [1 ]
Acar, M. T. [2 ]
Bozkurt, Y. B. [1 ]
Celik, A. [1 ]
机构
[1] Ataturk Univ, Fac Engn, Dept Mech Engn, Erzurum, Turkiye
[2] Erzincan Binali Yildirim Univ, Fac Engn & Architecture, Dept Mech Engn, Erzincan, Turkiye
来源
关键词
Titanium; Friction; Wear; Corrosion; TiO2; TITANIUM-ALLOYS; SURFACE MODIFICATION; NANOTUBES;
D O I
10.1016/j.surfcoat.2024.131024
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
This study focuses on the comparison of structural, morphological, mechanical, tribological and electrochemical properties of TiO2 films fabricated on Cp-Ti, Ti6Al4V and Ti45Nb alloys, which are widely used in different industries. For this purpose, TiO2 films were grown on Cp-Ti, Ti6Al4V and Ti45Nb materials by anodization method. Structural, morphological and mechanical properties of the samples were determined using XRD, SEM, Micro Raman, contact angle, surface roughness and micro hardness devices. Afterwards, the samples were subjected to wear and corrosion tests using a pin-on-disc wear device and a corrosion device, respectively. Wear tests were carried out in both dry and liquid environments. In electrochemical corrosion tests, Ringer's solution was used and open circuit potential (OCP) and electrochemical polarization analyzes were performed. According to the results of XRD and Raman analyses, it was determined that TiO2 films were successfully grown on the surface of the samples. Additionally, it was observed that these films were in Rutile and Anatase phases and their peak intensities increased with increasing anodization time. While the thickest films were obtained from Ti45Nb samples, the thinnest films were obtained from Cp-Ti samples. As a result of the increase in surface roughness with anodization, surface wettability increased in all samples. It was seen that electrical resistance of the materials was highly effective on the film thickness, surface roughness and surface structures. Wear coefficients decreased in all samples for both dry and liquid wear conditions due to the increased surface hardness and anodic film thickness and the lowest wear coefficients were obtained from the Ti45Nb sample. Corrosion performance of the samples increased with anodization because TiO2 films acted as protective layers on surface of materials.
引用
收藏
页数:14
相关论文
共 50 条
  • [1] Comparison of the structural properties, surface wettability and corrosion resistance of TiO2 nanotubes fabricated on Cp-Ti, Ti6Al4V and Ti45Nb
    Acar, M. T.
    Kovaci, H.
    Celik, A.
    MATERIALS TODAY COMMUNICATIONS, 2022, 33
  • [2] Structural, Morphological, and Electrochemical Corrosion Properties of TiO2 Formed on Ti6Al4V Alloys by Anodization
    Atmani, Djamila
    Saoula, Nadia
    Abdi, Abderrezak
    Azzaz, Mohamed
    Wang, Youling
    Mohamedi, Mohamed
    CRYSTAL RESEARCH AND TECHNOLOGY, 2018, 53 (12)
  • [3] The comparison of wear performances of CP-Ti, Ti6Al4V, Ti45Nb alloys oxidized by anodic oxidation under ambient air and vacuum conditions
    Asl, Hojjat Ghahramanzadeh
    Sert, Yasar
    Kucukomeroglu, Tevfik
    Bayrak, Ozgu
    MATERIALS TODAY COMMUNICATIONS, 2023, 34
  • [4] Tribological behaviour of plasma electrolytic oxide coatings on Ti6Al4V and cp-Ti alloys
    Tekin, K. C.
    Malayoglu, U.
    Shrestha, S.
    SURFACE ENGINEERING, 2016, 32 (06) : 435 - 442
  • [5] Liquid Boriding of Cp-Ti and Ti6Al4V Alloy: Characterization of Boride Layers and Tribological Properties
    M. Keddam
    N. Makuch
    B. Boumaali
    A. Piasecki
    A. Miklaszewski
    M. Kulka
    Surface Engineering and Applied Electrochemistry, 2020, 56 : 348 - 357
  • [6] Liquid Boriding of Cp-Ti and Ti6Al4V Alloy: Characterization of Boride Layers and Tribological Properties
    Keddam, M.
    Makuch, N.
    Boumaali, B.
    Piasecki, A.
    Miklaszewski, A.
    Kulka, M.
    SURFACE ENGINEERING AND APPLIED ELECTROCHEMISTRY, 2020, 56 (03) : 348 - 357
  • [7] Effect of Manufacturing Process on Electrochemical Properties of CP-Ti and Ti-6Al-4V Alloys
    Kim, K. T.
    Cho, H. W.
    Chang, H. Y.
    Kim, Y. S.
    CORROSION SCIENCE AND TECHNOLOGY-KOREA, 2018, 17 (01): : 20 - 29
  • [8] Improving structural, tribological and electrochemical properties of Ti6Al4V alloy with B-doped TiO2 thin films
    Celik, A.
    Acar, M. T.
    Yetim, T.
    Kovaci, H.
    Yetim, A. F.
    TRIBOLOGY INTERNATIONAL, 2020, 146 (146)
  • [9] Surface characterisation of cp Ti, Ti6Al7Nb and Ti6Al4V
    Sittig, C
    Wieland, M
    Marti, A
    Hauert, R
    Vallotton, PH
    Textor, M
    Spencer, ND
    ECASIA 97: 7TH EUROPEAN CONFERENCE ON APPLICATIONS OF SURFACE AND INTERFACE ANALYSIS, 1997, : 147 - 150
  • [10] Comparative Evaluation on the In Vitro Biological Performance of Ti45Al8.5Nb Intermetallic with Ti6Al4V and Ti6Al7Nb Alloys
    Li, Huafang
    Zheng, Yufeng
    Lin, Junpin
    ADVANCED ENGINEERING MATERIALS, 2011, 13 (05) : B187 - B193