Preparation and properties optimization of CeO2-Y2O3 Co-stabilized zirconia via vat photopolymerization

被引:4
|
作者
Zhang, Ren-Zhong [1 ,2 ,3 ]
Huang, Yu-Xuan [4 ]
Li, Wei-Kang [1 ,2 ]
Pan, Ming-Zhu [1 ,2 ]
Liu, Zi-Mo [1 ,2 ]
Wu, Jia-Min [1 ,2 ,3 ]
Zhang, Xiao-Yan [5 ]
Ye, Chun-Sheng [1 ,2 ]
Shi, Yu-Sheng [1 ,2 ]
机构
[1] Huazhong Univ Sci & Technol, Sch Mat Sci & Engn, State Key Lab Mat Proc & Die Mould Technol, Wuhan 430074, Peoples R China
[2] Minist Educ, Engn Res Ctr Ceram Mat Addit Mfg, Wuhan 430074, Peoples R China
[3] Huazhong Univ Sci & Technol, Wenzhou Adv Mfg Inst, Wenzhou 325035, Peoples R China
[4] Huazhong Univ Sci & Technol, Coll Life Sci & Technol, Wuhan 430074, Peoples R China
[5] Univ Sci & Technol Beijing, Inst Adv Mat & Technol, Beijing 100083, Peoples R China
基金
中国国家自然科学基金; 北京市自然科学基金;
关键词
Vat photopolymerization; Zirconia; Photopolymerization; Mechanical property; Low -temperature degradation; LOW-TEMPERATURE DEGRADATION; Y-TZP; MECHANICAL-PROPERTIES; DENTAL IMPLANTS; CERAMICS; TRANSFORMATION; ALUMINA; COMPOSITES;
D O I
10.1016/j.ceramint.2024.03.331
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Employed ubiquitously in oral restorations, zirconia-based bioceramics face challenges with low-temperature degradation (LTD) in the tetragonal phase (t-ZrO2) within oral environments. In order to improve the resistance of ZrO2 ceramics to LTD, this study utilized vat photopolymerization technology to prepare 7Ce3Y-ZrO2 (7 mol% CeO2 and 3 mol% Y2O3). By adjusting the dispersant content and photosensitive resin ratio enabled the attainment of a 63.5 mu m curing depth with a 400 mJ/cm2 exposure, meeting the requirements for vat photopolymerization printing. After sintering at 1550 degrees C, these ceramics shown a relative density of 97.84 % and an impressive flexural strength of 503.1 MPa. Accelerated LTD tests were conducted to assess LTD-resistance, revealing no degradation in mechanical properties or evidence of tetragonal to monoclinic phase transitions. This stability is credited to the cerium ions' efficacy in hindering oxygen vacancy formation and subsequent aging within the ZrO2. This study affirms that CeO2-Y2O3 co-stabilized ZrO2 ceramics prepared using vat photopolymerization technology exhibit outstanding properties and resistance to LTD, showcasing significant potential in the field of oral restoration.
引用
收藏
页码:22316 / 22326
页数:11
相关论文
共 50 条
  • [31] Preparation and conductivity of Yb2O3-Y2O3 and Gd2O3-Y2O3 co-doped zirconia ceramics
    Kan, Yanmei
    Li, Songli
    Wang, Peiling
    Zhang, Guo-Jun
    Van der Biest, Omer
    Vleugels, Jef
    SOLID STATE IONICS, 2008, 179 (27-32) : 1531 - 1534
  • [33] Mechanical properties of ZrO2 ceramic stabilized by Y2O3 and CeO2
    Yu, MQ
    Fan, SG
    Zhang, LM
    Sun, SZ
    JOURNAL OF WUHAN UNIVERSITY OF TECHNOLOGY-MATERIALS SCIENCE EDITION, 2002, 17 (02): : 14 - 18
  • [34] Mechanical properties of ZrO2 ceramic stabilized by Y2O3 and CeO2
    Res. Institute of Synthetic Crystals, Beijing 100018, China
    Journal Wuhan University of Technology, Materials Science Edition, 2002, 17 (02): : 14 - 18
  • [35] Mechanical properties of ZrO2 ceramic stabilized by Y2O3 and CeO2
    Ming-qing Y.
    Shi-gang F.
    Lian-meng Z.
    Shu-zhen S.
    Journal of Wuhan University of Technology-Mater. Sci. Ed., 2002, 17 (2): : 14 - 18
  • [36] ???????Study on thermal shock resistance of Sc2O3 and Y2O3 co-stabilized ZrO2 thermal barrier coatings
    Dong, Y. S.
    Yan, C. L.
    Li, J.
    Jiang, Z. C.
    Mo, W. L.
    Zhang, Q. J.
    CERAMICS INTERNATIONAL, 2023, 49 (12) : 20034 - 20040
  • [37] Effect of point defects on the thermal conductivity of Sc2O3-Y2O3 co-stabilized tetragonal ZrO2 ceramic materials
    Fan, W.
    Bai, Y.
    Wang, Z. Z.
    Che, J. W.
    Wang, Y.
    Tao, W. Z.
    Wang, R. J.
    Liang, G. Y.
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2019, 39 (07) : 2389 - 2396
  • [38] Catalytic combustion of toluene on Pt/Al2O3 and Pd/Al2O3 catalysts with CeO2, CeO2-Y2O3 and La2O3 as coatings
    Zhou, Bing
    Ke, Quanli
    Wen, Meijun
    Ying, Tianbiao
    Cui, Guokai
    Zhou, Ying
    Gu, Zhenyu
    Lu, Hanfeng
    JOURNAL OF RARE EARTHS, 2023, 41 (08) : 1171 - 1178
  • [39] Study on Thermal Shock Resistance of Nano-CeO2-Y2O3 Co-Stabilized ZrO2 (CYSZ) Ceramic Powders Thermal Barrier Coating of Aircraft Engine
    Lyu, Yang
    Shao, Xuan
    Wang, Wen-Xue
    Tang, Hui
    JOURNAL OF NANOELECTRONICS AND OPTOELECTRONICS, 2019, 14 (11) : 1597 - 1605
  • [40] Phase stability, thermal shock behavior and CMAS corrosion resistance of Yb2O3-Y2O3 co-stabilized zirconia thermal barrier coatings prepared by atmospheric plasma spraying
    Fang, Huanjie
    Wang, Weize
    Yang, Zining
    Yang, Ting
    Wang, Yihao
    Huang, Jibo
    Ye, Dongdong
    SURFACE & COATINGS TECHNOLOGY, 2021, 427