Electromagnetic wave absorbing properties and oxidation resistance of CNTs/SiC composite bonded with CNTs@calcium aluminate cement

被引:0
|
作者
Lei, Changkun [1 ,2 ]
Ding, Donghai [1 ]
Xiao, Guoqing [1 ]
Hou, Xinmei [2 ,3 ]
Wang, Enhui [2 ,3 ]
Zhou, Renbiao [1 ]
Feng, Chunzhuo [1 ]
机构
[1] Xian Univ Architecture & Technol, Coll Mat Sci & Engn, Xian 710055, Peoples R China
[2] Univ Sci & Technol Beijing, Inst Carbon Neutral, Beijing 100083, Peoples R China
[3] Liaoning Acad Mat, Shenyang 110000, Liaoning, Peoples R China
基金
中国国家自然科学基金;
关键词
EMW absorption property; Castable CNTs/SiC composites; CNTs@CAC; Flexural strength; Oxidation resistance; MICROWAVE-ABSORPTION PROPERTIES; THERMAL-SHOCK RESISTANCE; CARBON; CERAMICS; REFRACTORIES; INTEGRATION;
D O I
10.1016/j.ceramint.2024.06.309
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
To achieve homogeneous dispersion of CNTs in the SiC-based composites, calcium aluminate cement encased carbon nanotubes agglomerate (CNTs@CAC) was synthesized and used as a binder for castable CNTs/SiC composite. The EMW absorption, physical and mechanical properties of CNTs/SiC composite bonded with CNTs@CAC were investigated. SiC nanowires were in-situ generated in CNTs/SiC composite using CNTs from CNTs@CAC as the template. The uniform conductive network of SiC nanowires and CNTs and multiple heterogeneous interfaces promoted the dissipation of the incident EMW by conductance loss and polarization loss. As a result, the CNTs/SiC composite bonded with CNTs@CAC achieved a maximum EAB of 4.0 GHz in the X-band (8.2-12.4 GHz) at a thickness of 2.4 mm. Even after oxidation at 1000 degrees C for 8 h, the EAB covered the entire Xband. Moreover, RCS simulations were carried out via CST. The RCS values of CNTs@CAC bonded CNTs/SiC composites were all lower than those of mechanically mixed Secar71 and CNTs bonded CNTs/SiC composites under different incident angles of EMW, indicating that CNTs/CAC bonded CNTs/SiC composites can attenuate more electromagnetic energy. The bulk density of CNTs/SiC composite bonded with CNTs@CAC was 1.85 g/cm3, 3 , and flexure strength was 22.8 MPa.
引用
收藏
页码:35007 / 35018
页数:12
相关论文
共 22 条
  • [21] Single-source-precursor derived multicomponent CNTs/Fe3Si/Fe/SiOCN ceramic nanocomposites: microstructural evolution and excellent electromagnetic wave absorbing properties
    Yu, Zhaoju
    Zhu, Qikun
    Li, Fen
    Chen, Ting
    Du, Hanzi
    JOURNAL OF MATERIALS CHEMISTRY C, 2022, 10 (16) : 6252 - 6262
  • [22] The Electromagnetic Wave Absorption Performance and Mechanical Properties of Cement-Based Composite Material Mixed with Functional Aggregates with High Fe2O3 and SiC
    Zhang, Zuoqun
    Yang, Chaoshan
    Cheng, Hua
    Huang, Xiaohan
    Zhu, Yuhao
    REVUE DES COMPOSITES ET DES MATERIAUX AVANCES-JOURNAL OF COMPOSITE AND ADVANCED MATERIALS, 2021, 31 (04): : 249 - 255