Laser Powder Bed Fusion and Heat Treatment of the Martensitic Age-Hardenable Steel (1.2709)

被引:0
|
作者
Solanki, Keyur [1 ]
Shah, Chirag [1 ]
Zinn, Carolin [1 ]
Lehmhus, Dirk [2 ]
Gupta, Nikhil [3 ]
von Hehl, Axel [1 ]
机构
[1] Univ Siegen, Fac Sch Sci & Technol 4, Inst Mat Engn, Chair Mat Sci & Mat Testing LMW, Paul Bonatz Str 9-11, D-57076 Siegen, Germany
[2] Fraunhofer Inst Mfg Technol & Adv Mat IFAM, Dept Casting Technol & Lightweight Construction, D-28359 Bremen, Germany
[3] NYU, Tandon Sch Engn, Dept Mech & Aerosp Engn, New York, NY 11201 USA
关键词
aging behavior; laser powder bed fusion; maraging steel; parameter optimization; MECHANICAL-PROPERTIES; MARAGING-STEEL; PROCESS PARAMETERS; MELTING PROCESS; PERFORMANCE; MICROSTRUCTURE; PRECIPITATION; BEHAVIOR;
D O I
10.1002/srin.202400173
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
The primary objective of this study is to clarify the fundamental question of whether, in principle, it is possible to dispense with a prior solution annealing process in favor of a direct aging heat treatment for specimens of maraging stainless steel grade X3NiCoMoTi18-9-5 (1.2709) produced by laser powder bed fusion (LPBF). The waiver of a solution annealing process would significantly increase the process efficiency and thus support a sustainable and resource-friendly production of such components. Therefore, the hardness, microstructure, and the present phases of specimens in as-built + aged condition (AB + A) and solution-annealed + aged (SOL + A) are examined during this study. Initially, an extended parameter study is performed using a Renishaw AM 250 LPBF system equipped with a pulsed mode laser system to achieve the highest possible apparent density. As test specimens, small cubes are produced for parameter study and are analyzed for porosity by means of optical microscopy. To investigate the relationship between microstructure and hardness in different material states, one series of specimens is aged directly after LPBF processing in the as-built state (AB + A). For comparison, the other series was solution annealed at 820 degrees C for 60 min, quenched in water and then aged (SOL + A). A maximum hardness value of 614 HV1.0 is achieved for specimen aged at 490 degrees C for 120 min in as built condition (AB + A), while 624 HV1.0 was measured for specimen aged at 490 degrees C for 180 min in conventionally solution annealed + aged (SOL + A) condition. Significant austenite reversion is not observed at aging temperature of 490 degrees C in both cases. Aging of specimens at temperatures of 540 and 600 degrees C resulted in reduction of specimen hardness due to higher percentage of austenite reversion. No significant difference between the hardness values of AB + A and SOL + A specimens is observed. It can therefore be concluded that, in principle, conventional solution annealing and ageing can be dispensed with in favor of direct aging. However, as the results are based on small sized specimens, further investigations into the scalability are needed. The rapid solidification and intrinsic cyclic reheating during laser powder bed fusion (LPBF) result in precipitation during the LPBF process which, in the cast steels, is expected after solution annealing followed by quenching and aging. The waiver of solution annealing for maraging steel specimens produced via LPBF manufacturing can increase the process efficiency and thus support a sustainable and resource-friendly production of such components.image (c) 2024 WILEY-VCH GmbH
引用
收藏
页数:11
相关论文
共 50 条
  • [31] Heat treatment of aluminium alloys produced by laser powder bed fusion: A review
    Fiocchi, J.
    Tuissi, A.
    Biffi, C. A.
    MATERIALS & DESIGN, 2021, 204
  • [32] The Effect of Laser Post-Heat Treatment of Laser Powder Bed Fusion High Nitrogen Steel on the Microstructure and Mechanical Properties
    Fu, Jiazhe
    Liu, Jie
    Zhong, Sheng
    Li, Tiannan
    Zhang, Peng
    Xing, Ying
    Liang, Yanwen
    Guo, Shun
    Wang, Kehong
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2025,
  • [33] Unveiling the cellular microstructure-property relations in martensitic stainless steel via laser powder bed fusion
    Wu, Lingzhi
    Zhang, Cong
    Khan, Dil Faraz
    Zhang, Ruijie
    Wang, Yongwei
    Jiang, Xue
    Yin, Haiqing
    Qu, Xuanhui
    Liu, Geng
    Su, Jie
    INTERNATIONAL JOURNAL OF MINERALS METALLURGY AND MATERIALS, 2024, 31 (11) : 2476 - 2487
  • [34] Crystallographic aspects of 17-4 PH martensitic steel produced by laser-powder bed fusion
    Vysotskiy, Igor
    Malopheyev, Sergey
    Zuiko, Ivan
    Mironov, Sergey
    Kaibyshev, Rustam
    MATERIALS CHARACTERIZATION, 2022, 194
  • [35] Crystallographic Aspects of 17-4 PH Martensitic Steel Produced by Laser-Powder Bed Fusion
    Mironov, Sergey
    Malopheyev, Sergey
    Zuiko, Ivan
    Kaibyshev, Rustam
    Vysotskiy, Igor
    SSRN, 2022,
  • [36] Crystallographic Aspects of 17-4 Ph Martensitic Steel Produced by Laser-Powder Bed Fusion
    Belgorod National Research University, Pobeda 85, Belgorod
    308015, Russia
    1600,
  • [37] IN-787 - AGE-HARDENABLE STEEL FOR LINE PIPE AND GENERAL STRUCTURAL USES
    HYDREAN, PP
    SHELTON, CH
    CHARD, JE
    CANADIAN MINING AND METALLURGICAL BULLETIN, 1972, 65 (724): : 20 - &
  • [38] ON IMPROVEMENT IN NOTCH TOUGHNESS OF COPPER-NICKEL-ALUMINUM AGE-HARDENABLE STEEL
    ASADA, C
    WATANABE, T
    TRANSACTIONS OF THE JAPAN INSTITUTE OF METALS, 1968, S 9 : 387 - &
  • [39] Heat Treatment Effect on the Corrosion Resistance of 316L Stainless Steel Produced by Laser Powder Bed Fusion
    Sangoi, Kevin
    Nadimi, Mahdi
    Song, Jie
    Fu, Yao
    METALS, 2025, 15 (01)
  • [40] Effect of heat treatment on the corrosion resistance of 316L stainless steel manufactured by laser powder bed fusion
    Liu, Wei
    Liu, Chengsong
    Wang, Yong
    Zhang, Hua
    Ni, Hongwei
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2024, 32 : 3896 - 3912